Reaction between molten steel and CaO–SiO2–MgO–Al2O3-FetO slag under varying amounts of converter carryover slag
Source abstract
Abstract
Converter carryover slag during tapping has been a trouble for improvement of steel quality. In order to give an insight into the action mechanism of carryover slag on steel during tapping, a serious of molten steel-slag reaction experiments was conducted to elucidate the reaction mechanism between 3% Al steel and CaO–SiO2–MgO–Al2O3-FetO type slag at 1600 °C as well as its resulting effect on cleanliness under varying amount of converter carryover slag was investigated in laboratory. Composition evolutions in molten steel and slag during the reaction and microstructure on the steel-slag interface were investigated by employing different experimental techniques. 2[Al] + (Fe2O3) = 2[Fe] + (Al2O3) and 4[Al] + 3(SiO2) = 3[Si] + 2(Al2O3) were confirmed as a major reaction in the system. The initial (Fe2O3) content in experiments increased from 3% to 15%. The results indicated the metal-slag reaction tended to stable after about 10 min, the mass transfer of [Al] in molten steel was the rate-controlling step [Als] was more prone to react with (SiO2) for slags with initial (Fe2O3) less than 4.07%, but it reacted with both (Fe2O3) and (SiO2) when (Fe2O3) content was more. It was therefore suitable addition of Al alloy should take (SiO2) into consideration in addition to (Fe2O3) and dissolved [O]. Increase of carryover slag amount represented by increase of initial (Fe2O3) decreased the sulfur distribution but promoted the formation of MgO·Al2O3 inclusion. The sulfur distribution ratio decreased from roughly 5000 to 2000 but the number density of inclusion increased from 22.125/mm2 to 45.875/mm2 with increase of initial (Fe2O3) from 3% to 15%.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metallurgical Processes and Thermodynamics · Materials Engineering and Processing · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Slag entraining vortexing funnel formation during ladle teeming: similarity criteria and scale-up relationships10.1179/030192302225003486 ↗
2. Mattias · 2013
3. Fruehan · 2005
4. The role of process control on the steel cleanliness10.1080/03019233.2016.1245917 ↗
5. Doostmohammadi · 2009
6. Reduction of tundish skull and yield improvement in steel plants through physical modeling of steelmaking tundish systems10.1007/s12666-011-0067-8 ↗
7. A dynamic mixed-control model for BOF metal-slag-gas reactions10.1007/s11663-021-02094-w ↗
8. Purchase · 2003
9. Effects of Al addition on the reaction between high manganese steel and CaO-SiO2-Al2O3-MgO slag10.1002/srin.202000143 ↗
10. A reaction between high Mn-high Al steel and CaO-SiO2-type molten mold flux: Part I. Composition evolution in molten mold flux10.1007/s11663-012-9770-z ↗
11. A reaction between high Mn-high Al steel and CaO-SiO2-type molten mold flux: Part II. Reaction mechanism, interface morphology, and Al2O3 accumulation in molten mold flux10.1007/s11663-012-9769-5 ↗
12. Oxidation rate of aluminum in molten iron by CaO-SiO2-Al2O3-FeO-MnO slag10.2355/isijinternational.36.Suppl_S34 ↗
13. Hidden phenomena during transient reaction trajectories in liquid metals processing10.1007/s11663-020-01880-2 ↗
14. Reaction between high Mn-high Al steel and CaO-SiO2-type molten mold flux: retardation of Al2O3 accumulation at high Al content ([pct Al]0≥5) in steel and low MgO content (pct MgO0≤ 1.8) in flux10.1007/s11663-020-01972-z ↗
15. Deo · 1993
16. Kinetics of metal/slag reactions during spontaneous emulsification10.1007/s11663-005-0023-2 ↗
17. Reoxidation of Al-killed ultra-low C steel by FetO in RH slag: experiment, reaction rate model development, and mechanism analysis10.1007/s11663-021-02220-8 ↗
18. Kinetics of chromium oxide reduction from a basic steelmaking slag by silicon dissolved in liquid iron10.1007/BF02644316 ↗
19. Progress of thermodynamic modeling for sulfide dissolution in molten oxide slags: sulfide capacity and phase diagram10.1007/s11663-021-02224-4 ↗
20. Interfacial behaviour in Ferroalloys: the influence of sulfur in FeMn and SiMn systems10.1007/s11663-021-02323-2 ↗
21. A review of steel processing considerations for oxide cleanliness10.1007/s11663-020-01949-y ↗
22. Effect of silica in slag on inclusion compositions in 304 stainless steel: deoxidized with aluminum10.2355/isijinternational.44.1350 ↗
23. Formation and modification of MgO·Al2O3-based inclusions in alloy steels10.1007/s11663-012-9663-1 ↗
24. Steel/refractory/slag interfacial reaction and its effect on inclusions in high-Mn high-Al steel10.1016/j.ceramint.2021.09.194 ↗
25. Effect of slag composition on MgO·Al2O3 spinel-type inclusions in molten steel10.2355/isijinternational.ISIJINT-2017-174 ↗
26. Dissolution behavior of Al2O3 into tundish slag for high- Al steel10.1016/j.jmrt.2020.07.107 ↗