Multilevel microstructure control of cast Al–7.0Si–4.0Cu alloy with high strength–toughness synergy via micro-alloying combined with manipulation by in-situ nano-ceramics
Source abstract
Abstract
Incident Ti–Si poisoning when applying traditional agents of microstructure manipulation in Al–Si alloys is always adverse to realize multilevel microstructure control. This work combined the manipulation by physically formed in-situ nano-ceramics from Fe79.58B11.26Si9.26 amorphous alloy and the micro-alloying to comprehensively improve the microstructure configuration of Al–7.0Si–4.0Cu alloy. It was suggested that micro-alloying of Mg and Sb prominently refined α-Al dendrites and eutectic silicon. Micro-alloying with Mg increased the nucleating temperature of α-Al, meanwhile Mg atoms can hinder the growth of α-Al and eutectic silicon. Sb atoms can also be adsorbed to the growth interfaces of eutectic silicon hindering the growth process. On this basis, trace Fe79.58B11.26Si9.26 amorphous alloy brought further optimization on α-Al dendrites and eutectic silicon, especially Al2Cu and Mg2Si, realizing the multilevel microstructure control. In-situ Fe2B and Fe3Si nano-ceramics were confirmed to have low lattice misfits with α-Al and silicon, serving as efficient nucleation sites and growth retardants. After combined micro-alloying and manipulation, the mean sizes of α-Al and eutectic silicon were significantly refined by 72.7% and 79.9%, respectively, meanwhile, the ultimate tensile strength (UTS) and plastic strain (δ) were improved to 480 MPa and 9.4%, corresponding to 30.1% and 77.4% improvement, respectively. This work provides new mentality to realize multilevel microstructure control and improvement of strength–toughness synergy in Al–Si alloys.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (52)
Show source-provided references
1. High cycle fatigue analysis and modelling of cast Al–Si alloys extracted from cylinder heads considering microstructure characteristics10.1016/j.jmrt.2022.05.186 ↗
2. Understanding the influencing mechanism of sub-micron sized TiB2p on the microstructures and properties of rheological squeeze casting hypereutectic Al–Si alloys10.1016/j.jmrt.2021.06.048 ↗
3. Additive manufacturing of metallic lattice structures: unconstrained design, accurate fabrication, fascinated performances, and challenges10.1016/j.mser.2021.100648 ↗
4. Synergistic optimization in solidification microstructure and mechanical performance of novel (TiCxNy−TiB2)p/Al nanocomposites: design, tuning and mechanism10.1016/j.compositesa.2022.106843 ↗
5. Enhancing strength-ductility synergy and mechanisms of Al-based composites by size-tunable in-situ TiB2 particles with specific spatial distribution10.1016/j.compositesb.2021.108912 ↗
6. Insight into solidification microstructure control by trace TiCN–TiB2 particles for yielding fine-tuned nanoprecipitates in a hypoeutectic Al–Si–Mg alloy10.1016/j.msea.2021.142093 ↗
7. EBSD, XRD and SRS characterization of a casting Al–7wt%Si alloy processed by equal channel angular extrusion: dislocation density evaluation10.1016/j.matchar.2019.04.044 ↗
8. Si phase modification on the elevated temperature mechanical properties of Al–Si hypereutectic alloys10.1016/j.msea.2019.01.119 ↗
9. Concurrent enhancement of strength and ductility for Al–Si binary alloy by refining Si phase to nanoscale10.1016/j.msea.2019.02.081 ↗
10. Role of trace nanoparticles in establishing fully optimized microstructure configuration of cold-rolled Al alloy10.1016/j.matdes.2021.109743 ↗
11. Interface formation and bonding control in high-volume-fraction (TiC+TiB2)/Al composites and their roles in enhancing properties10.1016/j.compositesb.2021.108605 ↗
12. Unprecedented enhancement in strength-plasticity synergy of (TiC+Al6MoTi+Mo)/Al cermet by multiple length-scale microstructure stimulated synergistic deformation10.1016/j.compositesb.2021.109265 ↗
13. Strengthening of dislocation and precipitation for high strength and toughness casting Al–Zn–Mg–Cu alloy via trace TiB2+TiC particles10.1016/j.msea.2022.144107 ↗
14. Versatility of trace nano-TiC–TiB2 in collaborative control of solidification-rolling-welding microstructural evolution in Al–Mg–Si alloy for enhanced properties10.1016/j.msea.2022.143661 ↗
15. Investigation on the elevated-temperature tribological behaviors and mechanism of Al-Cu-Mg composites reinforced by in-situ size-tunable TiB2-TiC particles10.1016/j.triboint.2022.107943 ↗
16. Corrosion behavior and characteristics of passive films of laser powder bed fusion produced Ti–6Al–4V in dynamic Hank's solution10.1016/j.matdes.2021.109907 ↗
17. Metastable pitting corrosion behavior of laser powder bed fusion produced Ti–6Al–4V in Hank's solution10.1016/j.corsci.2022.110333 ↗
18. Effect of large thickness-reduction on microstructure evolution and tensile properties of Mg–9Al–1Zn alloy processed by hard-plate rolling10.1016/j.jmst.2021.01.050 ↗
19. A new approach for improving the elevated-temperature strength and ductility of Al–Cu–Mg–Si alloys with minor amounts of dual-phased submicron/nanosized TiB2–TiC particles10.1016/j.msea.2019.138266 ↗
20. Microstructure and mechanical properties of Al–Mg–Si alloy fabricated by a short process based on sub-rapid solidification10.1016/j.jmst.2019.08.053 ↗
21. Influence of Ti addition on the microstructure and hardness properties of near-eutectic Al–Si alloys10.1016/j.jallcom.2006.10.131 ↗
22. Sb effect on micro structural and mechanical properties of rapidly solidified Al–12Si alloy10.1016/j.jallcom.2010.09.037 ↗
23. Effect of various melt and heat treatment conditions on impact toughness of A356 aluminum alloy10.1016/S1003-6326(16)64191-2 ↗
24. Insight into Si poisoning on grain refinement of Al–Si/Al–5Ti–B system10.1016/j.actamat.2020.01.039 ↗
25. Heat-treatment induced defect formation in α-Al matrix in Sr-modified eutectic Al–Si alloy10.1016/j.jallcom.2017.09.324 ↗
26. Cluster formation at the Si/liquid interface in Sr and Na modified Al–Si alloys10.1016/j.scriptamat.2016.02.018 ↗
27. Combining Sr and Na additions in hypoeutectic Al–Si foundry alloys10.1016/j.msea.2005.03.091 ↗
28. Comparison of in situ nanocrystals, Sr and nanocrystals+Sr manipulating microstructures and mechanical properties of eutectic Al–Si13.0–Cu5.0–(Ni2.0)–Mg0.6 alloy10.1016/j.jmrt.2020.05.061 ↗
29. Mutual poisoning effect between Sr and B in Al–Si casting alloys10.1016/S1359-6462(02)00648-6 ↗
30. Fractal dimension analysis of Mg2Si particles of Al–15%Mg2Si composite and its relationships to mechanical properties
31. Rapid crystallization of amorphous silicon nitride powder accelerated by liquid Si10.1016/j.ceramint.2012.03.001 ↗
32. Crystallization of hydroxyapatite during hydrothermal treatment on amorphous calcium phosphate layer coated by PEO technique10.1016/j.ceramint.2012.08.026 ↗
33. Multiscale design of α-Al, eutectic silicon and Mg2Si phases in Al-Si-Mg alloy manipulated by in situ nanosized crystals10.1016/j.msea.2020.140627 ↗
34. Design of a new Al-Cu alloy manipulated by in-situ nanocrystals with superior high temperature tensile properties and its constitutive equation10.1016/j.matdes.2019.107945 ↗
35. Simultaneously increasing strength and ductility of the Al–Cu alloys inoculated by Zr-based metallic glass10.1016/j.matchar.2014.12.016 ↗
36. Grain refinement behavior of Al–Cu alloys inoculated by various metallic glasses10.1016/j.matchemphys.2015.11.003 ↗
37. Investigation of the influences of ternary Mg addition on the solidification microstructure and mechanical properties of as-cast Al–10Si alloys10.1016/j.msea.2020.140247 ↗
38. The effects of neodymium addition on the intermetallic microstructure and mechanical properties of Al–7Si–0.3Mg–0.3Fe alloys10.1016/j.jallcom.2018.01.138 ↗
39. On the influences of Li on the microstructure and properties of hypoeutectic Al–7Si alloy10.1016/j.jallcom.2017.04.295 ↗
40. Optimizing strength and ductility of Al–7Si–0.4Mg foundry alloy: role of Cu and Sc addition10.1016/j.jallcom.2019.151944 ↗
41. Synergistic effects of Ce and Mg on the microstructure and tensile properties of Al–7Si–0.3Mg–0.2Fe alloy10.1016/j.jallcom.2019.05.049 ↗
42. Effect of trace yttrium addition on the microstructure and tensile properties of recycled Al–7Si–0.3Mg–1.0Fe casting alloys10.1016/j.msea.2016.04.036 ↗
43. Microstructure and mechanical properties of a bulk ultrafine grained Al–7Si–0.3Mg alloy produced by thermomechanical consolidation of a nanocrystalline powder10.1016/j.msea.2016.02.002 ↗
44. A novel modifier on the microstructure and mechanical properties of Al–7Si alloys10.1016/j.matlet.2019.05.050 ↗
45. Effect of Cd micro-addition on microstructure and mechanical properties in ternary Al–Si–Cu alloy10.1016/j.jallcom.2020.156739 ↗
46. The formation mechanism of the chill fine-grain layer with high supersaturation and its influence on the mechanical properties of die casting Al–7Si–0.5Mg alloy10.1016/j.msea.2021.142544 ↗
47. Tensile and wear behaviour of in situ Al–7Si/TiB2 particulate composites10.1016/j.wear.2007.09.007 ↗
48. Atomic structure and interface chemistry in a high-stiffness and high-strength Al–Si–Mg/TiB2 nanocomposite10.1016/j.msea.2019.138072 ↗
49. Effect of samarium (Sm) addition on the microstructures and mechanical properties of Al–7Si–0.7Mg alloys10.1016/j.jallcom.2013.03.050 ↗
50. Influence of grain refinement and modification on microstructure and mechanical properties of Al–7Si and Al–7Si–2.5Cu cast alloys10.1016/j.matchar.2007.01.011 ↗
51. Strong and ductile recycled Al–7Si–3Cu–1Fe alloy: controlling the morphology of quasicrystal approximant α-phase by Mn and V addition10.1016/j.jallcom.2021.161508 ↗
52. Microstructure design and strengthening of mechanical properties in Al–Si alloy through 0.05 wt % Ni-base amorphous alloy10.1016/j.vacuum.2021.110714 ↗