Abstract
In this paper, micro harmonic vibration was applied to the typical titanium alloys to clarify their damping performance at cryogenic temperatures. The effects of vibration modulus at different frequencies were elaborately analyzed, and the crack propagation mechanism was discussed. The increase of internal dislocations improves the damping performance and eventually leads to interface cracking, which is positively correlated with frequency. More importantly, dislocations of β phase aggregated at the interface, leading to interface cracks and transgranular fractures by stress concentration. Whereas, dislocations in the α phase are first activated and then glide toward the boundary to cause cracking, resulting in intergranular fracture. During harmonic vibration at 0∼−60 °C with 200 Hz, the crack propagation of α phase always has a hysteresis behavior compared with that of β phase. When ΔK = 0.137 MPa m1/2 (−60 °C, 200 Hz), the second crack tip of β phase is deflected in different directions, leading to higher harmonic vibration energy is consumption. As a result, the crack growth rate slows down and the damping performance reaches its peak. This contribution is expected to provide experimental data and theoretical support for the vibration damping behavior of typical titanium alloys at cryogenic temperature.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · High-Velocity Impact and Material Behavior · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Microstructure and tensile properties of a cost-affordable and ultrahigh-strength metastable β titanium alloy with a composition of Ti-6Al-1Mo-1Fe-6.9Cr10.1016/j.jallcom.2021.163476 ↗
2. High-strength titanium alloys for aerospace engineering applications: a review on melting-forging process10.1016/j.msea.2022.143260 ↗
3. Effect of deposition strategies on fatigue crack growth behaviour of wire + arc additive manufactured titanium alloy Ti–6Al–4V10.1016/j.msea.2021.141194 ↗
4. Microstructural and load hold effects on small fatigue crack growth in α + β dual phase Ti alloys
5. Effect of Ta addition on microstructures, mechanical and damping properties of Cu–Al–Mn–Ti alloy10.1016/j.jmrt.2021.10.031 ↗
6. Microstructure and mechanical properties of TiC/AlSi10Mg alloy fabricated by laser additive manufacturing under high-frequency micro-vibration10.1016/j.jallcom.2019.04.287 ↗
7. Mechanical behaviors and microstructure characteristics of W-tempered and peak-aged 7075 alloy sheets under low frequency vibration–assisted tension10.1016/j.msea.2021.142338 ↗
8. The effects of microstructure evolution on the fracture toughness of BT-25 titanium alloy during isothermal forging and subsequent heat treatment10.1016/j.msea.2018.12.062 ↗
9. Effect of shot peening and vibration finishing on the fatigue behavior of TC17 titanium alloy at room and high temperature10.1016/j.ijfatigue.2021.106391 ↗
10. Influence of dynamic angles and cutting strain on chip morphology and cutting forces during titanium alloy Ti-6Al-4 V vibration-assisted drilling10.1016/j.jmatprotec.2020.116898 ↗
11. Fatigue crack growth in residual stress fields of laser shock peened Ti6Al4V titanium alloy10.1016/j.jallcom.2021.161427 ↗
12. Crack growth behavior in dissimilar welded Ti based alloys under biaxial fatigue loading10.1016/j.ijfatigue.2018.09.013 ↗
13. Quasi-static and dynamic fracture toughness of a γ-TiAl alloy: measurement techniques, fractography and interpretation10.1016/j.engfracmech.2021.108081 ↗
14. Effect of primary α phase on the fatigue crack path of laser melting deposited Ti–5Al–5Mo–5V–1Cr–1Fe near β titanium alloy10.1016/j.ijfatigue.2018.06.041 ↗
15. Microstructure and fracture toughness of the aged ,β-Ti Alloy Ti-10V-2Fe-M10.1007/BF02628388 ↗
16. Fatigue behaviors of a titanium alloy in the VHCF regime based on a vibration-based bending fatigue test10.1111/ffe.13766 ↗
17. Anisotropic failure behavior of ordered intermetallic TiAl alloys under pure mode-I loading10.1088/1361-651X/aba738 ↗
18. Unravelling the lamellar size-dependent fracture behavior of fully lamellar intermetallic γ-TiAl10.1016/j.actamat.2022.117698 ↗
19. Twin-boundary assisted crack tip plasticity and toughening in lamellar γ-TiA10.1016/j.actamat.2021.116924 ↗
20. Dynamic mechanical behavior of WC-Co coated A356.2 aluminum alloy10.1016/j.jallcom.2018.07.203 ↗
21. Crystallographic selection rule for the propagation mode of microstructurally small fatigue crack in a laminated Ti-6Al-4V alloy: roles of basal and pyramidal slips10.1016/j.ijfatigue.2019.105200 ↗
22. Ceramic coatings: a phenomenological modeling for damping behavior related to microstructural features10.1016/j.msea.2006.04.140 ↗
23. Crack propagation during Charpy impact toughness testing of TiAlVMoZr alloy tubes containing equiaxed and lamellar microstructures
24. Higher damping capacity induced by negative magnetostriction of Fe-16Cr-2.5Mo-0∼0.2V alloys10.1016/j.jallcom.2020.156673 ↗
25. Optimization and damping performance of constrained damping boring bar
26. Dynamic mechanical behavior of WC-Co coated A356.2 Aluminum alloy10.1016/j.jallcom.2018.07.203 ↗
27. New high-modulus and high-strength Mg-Gd-Ag-Mn-Ge alloys
28. Experimental and statistical investigation of the effect of cutting parameters on surface roughness, vibration and energy consumption in machining of titanium 6Al-4V ELI (grade 5) alloy
29. A statistical model of fatigue failure incorporating effects of specimen size and load amplitude on fatigue life
30. Effect of long term aging on the microstructural stability and mechanical properties of Ti-6Al-2Cr-2Mo-2Sn-2Zr alloy
31. Obtaining heterogeneous α laths in selective laser melted Ti–5Al–5Mo–5V–1Cr–1Fe alloy with high strength and ductility10.1016/j.msea.2022.142624 ↗
32. Microstructural and geometrical size effects on the fatigue of metallic materials10.1016/j.ijmecsci.2021.107058 ↗
33. Effect of α phase morphology on fatigue crack growth behavior of Ti−5Al−5Mo−5V−1Cr−1Fe alloy10.1016/S1003-6326(20)65392-4 ↗
34. Microstructure and properties of monolayer, bilayer and multilayer Ta2O5-based coatings on biomedical Ti-6Al-4V alloy by magnetron sputtering10.1016/j.ceramint.2020.08.230 ↗
35. Anelastic relaxation caused by interstitial atoms in -type sintered Ti–Nb alloys10.1016/j.jallcom.2011.04.090 ↗
36. Investigation of the martensitic transformation and the damping behavior of a superelastic Ti-Ta-Nb alloy10.1016/j.actamat.2012.09.065 ↗
37. Investigation on the deformation mechanism of Ti–5Al-2.5Sn ELI titanium alloy at cryogenic and room temperatures10.1016/j.msea.2021.141380 ↗
38. Effect of crystallographic orientation and geometrical compatibility on fatigue crack initiation and propagation in rolled Ti-6Al-4V alloy10.1016/j.actamat.2019.07.025 ↗
39. Processing and machining mechanism of ultrasonic vibration-assisted grinding on sapphire10.1016/j.mssp.2022.106470 ↗
40. Influence of cooling rate on ω phase precipitation and deformation mechanism of a novel metastable β titanium alloy10.1016/j.msea.2021.142151 ↗
41. Deformation behavior and microstructure in the low-frequency vibration upsetting of titanium alloy10.1016/j.jmatprotec.2021.117360 ↗
42. Deformation mechanism and in-situ TEM compression behavior of TB8 β titanium alloy with gradient structure10.1016/j.jmst.2020.12.037 ↗