Intermetallic compound and martensitic transformation in Ag/Cu co-modified Ti6Al4V alloy
Source abstract
Abstract
Titanium and its alloys are promising materials for engine production, special pump manufacturing, and bone implants. However, the abrasion resistance and fracture toughness of Ti alloys are insufficient to withstand extreme high loading conditions and harsh environments. Surface modification is an effective way to improve the performance of Ti alloys. In this study, Ag and Cu were added to Ti6Al4V alloy through friction stir processing to modify its surface. The different ratios of the Ag/Cu powder mixture were designed to optimize the surface modification of Ti6Al4V, and the relationship between intermetallic compounds and martensitic transformation was analyzed. The martensitic transformation was induced by AgCuTi phases. The submicron-size martensite was distributed outside the AgCuTi particle, while the nano-laminar martensitic band was generated inside the AgCuTi particle. Under the co-modification of Ti alloy using Ag and Cu, the surface of Ti6Al4V alloy exhibited higher hardness (4.3 GPa) values and lower modulus (100.6 GPa), which gave the credit to the formation of AgCuTi and martensitic transformation. The alloy specimen was subjected to short heat treatment at 600 °C for 30 min to further modify the gradient structure. After the short heat treatment of the Ag/Cu co-modified specimen, a lower modulus (88.8 GPa) and a high level of hardness (4.1 GPa) were achieved. In addition, superelastic strain recovery was also enhanced, showing the further induced martensitic transformation. This work provides new insight into the surface modification of titanium alloys using the FSP method to achieve the ideal hardness and elastic modulus balance.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Advanced Welding Techniques Analysis · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (100+)
Show source-provided references
1. Improving fatigue performance of TiZrN/TiZr-coated Ti-6Al-4V alloy by inducing a stabile compressive residual stress field10.1016/j.jallcom.2022.166799 ↗
2. Perspectives on titanium science and technology10.1016/j.actamat.2012.10.043 ↗
3. Microstructure evolution and deformation mechanism of α+β dual-phase Ti-xNb-yTa-2Zr alloys with high performance10.1016/j.jmst.2022.04.052 ↗
4. Porous NiTiNb alloys with superior strength and ductility induced by modulating eutectic microregion10.1016/j.actamat.2022.118295 ↗
5. Metastable pitting corrosion behavior and characteristics of passive film of laser powder bed fusion produced Ti–6Al–4V in NaCl solutions with different concentrations10.1016/j.corsci.2023.111017 ↗
6. On the design evolution of hip implants: a review10.1016/j.matdes.2022.110552 ↗
7. Metastable pitting corrosion behavior of laser powder bed fusion produced Ti-6Al-4V in Hank's solution10.1016/j.corsci.2022.110333 ↗
8. Morphology, microstructure, and hardness of titanium (Ti-6Al-4V) blocks deposited by wire-feed additive layer manufacturing (ALM)10.1016/j.msea.2011.10.095 ↗
9. Towards uniform and enhanced tensile ductility of additively manufactured Ti−5Al−5Mo−5V−3Cr alloy through designing gradient interlayer deposition time10.1016/j.scriptamat.2022.115066 ↗
10. Short-time heat treatments in oxygen strengthened Ti-Zr α titanium alloys: a simple approach for optimized strength-ductility trade-off10.1016/j.matlet.2022.132114 ↗
11. Research on suitable strength, elastic modulus and abrasion resistance of Ti–Zr–Nb medium entropy alloys (MEAs) for implant adaptation10.1016/j.intermet.2021.107401 ↗
12. The effect of TiC on microstructure and mechanical properties of Ti-5553 beta phase titanium alloy10.1016/j.matdes.2022.110395 ↗
13. Corrosion behaviour of aluminide coatings on Ti-based alloy in the marine environment at high temperature10.1016/j.corsci.2022.110750 ↗
14. Effect of coating thickness on fatigue behavior of TiAlN coated Ti-alloys
15. Laser alloying of Ti–Si compound coating on Ti–6Al–4V alloy for the improvement of bioactivity10.1016/j.apsusc.2014.02.140 ↗
16. The improved corrosion and wear properties of Ti-Zr based alloys with oxide coating in simulated seawater environment10.1016/j.surfcoat.2022.128415 ↗
17. Preparation of TiNbTaZrMo high-entropy alloy with tunable Young's modulus by selective laser melting10.1016/j.jmapro.2022.11.046 ↗
18. Microstructure and wear behaviors of (TiB2+TiB+TiC)/Ti coating fabricated by laser wire deposition10.1016/j.matlet.2022.133132 ↗
19. A high-hydrophilic Cu2O-TiO2/Ti2O3/TiO coating on Ti-5Cu alloy: perfect antibacterial property and rapid endothelialization potential10.1016/j.bioadv.2022.213044 ↗
20. Preparation and properties of conductive Ti4O7 surface coating for Ti bipolar plates of proton exchange membrane fuel cells10.1016/j.jallcom.2022.165098 ↗
21. Influence of oxidation protective SiAl coatings on the tensile and fatigue behavior of Ti–48Al–2Cr–2Nb at elevated temperatures10.1016/j.msea.2022.144182 ↗
22. Microstructure and properties of a Ti doped Fe-based SMA coating produced by laser cladding10.1016/j.jmrt.2021.07.138 ↗
23. Half-Heusler alloys: enhancement of ZT after severe plastic deformation (ultra-low thermal conductivity)10.1016/j.actamat.2019.11.010 ↗
24. Effects of ternary alloy additions on the microstructure of highly immiscible Cu alloys subjected to severe plastic deformation: an evaluation of the effective temperature model10.1016/j.actamat.2019.03.023 ↗
25. The role of pyramidal dislocations in the grain refinement mechanism in Ti-6Al-4V alloy processed by severe plastic deformation10.1016/j.actamat.2020.08.076 ↗
26. Effect of severe plastic deformation by high-pressure torsion at different temperatures and subsequent annealing on structural and phase transformations in Zr-2.5% Nb alloy10.1016/j.jallcom.2021.158874 ↗
27. Severe plastic deformation induced precipitation of the ordered α2-Ti3Al phase in Ti–5Al–2Sn–2Zr–4Mo–4Cr
28. Effect of multi-pass friction stir processing on the microstructure evolution and corrosion behavior of ZrO2/AZ31 magnesium matrix Composite10.1016/j.jmrt.2022.02.127 ↗
29. Microstructure evolution and superelastic behavior in Ti-35Nb-2Ta-3Zr alloy processed by friction stir processing10.1016/j.actamat.2017.03.079 ↗
30. Surface microstructure and mechanical properties of Ti-6Al-4V/Ag nanocomposite prepared by FSP10.1016/j.matchar.2019.05.002 ↗
31. Tensile and superelastic behaviors of Ti-35Nb-2Ta-3Zr with gradient structure10.1016/j.matdes.2020.108961 ↗
32. An efficient approach to endow TiNbTaZr implant with osteogenic differentiation and antibacterial activity in vitro10.1016/j.matdes.2022.110987 ↗
33. Electrochemical and in vitro behavior of the nanosized composites of Ti-6Al-4V and TiO2 fabricated by friction stir process10.1016/j.apsusc.2017.06.141 ↗
34. TEM characterization on microstructure of Ti–6Al–4V/Ag nanocomposite formed by friction stir processing10.1016/j.mtla.2018.08.007 ↗
35. Microstructure and mechanical properties of Ti basic bionic gradient heterogeneous alloy prepared by multi-wire arc additive manufacturing10.1016/j.jallcom.2022.166813 ↗
36. Hierarchical transition structure induced by gradient composition distribution in layered Ti-TiNb alloy10.1016/j.scriptamat.2022.114854 ↗
37. Balance of strength and plasticity of additive manufactured Ti-6Al-4V alloy by forming TiB whiskers with cyclic gradient distribution
38. Gradient microstructure and mechanical properties of Ti-6Al-4V titanium alloy fabricated by high-frequency induction quenching treatment10.1016/j.matdes.2022.111031 ↗
39. Phase transformation pathways in Ti-6Al-4V manufactured via electron beam powder bed fusion10.1016/j.actamat.2021.117131 ↗
40. Effect of ball milling time on microstructure and mechanical properties of graphene nanoplates and TiBw reinforced Ti–6Al–4V alloy composites10.1016/j.msea.2022.144240 ↗
41. Highly oxidation-resistant Ti-Mo alloy with two-scale network Ti5Si3 reinforcement10.1016/j.jmst.2021.08.072 ↗
42. High-temperature creep behavior of TiC particulate reinforced Ti–6Al–4V alloy composite10.1016/S1359-6454(02)00261-6 ↗
43. Strengthening mechanism and micropillar analysis of high-strength NiTi–Nb eutectic-type alloy prepared by laser powder bed fusion10.1016/j.compositesb.2020.108358 ↗
44. Influence of SiC particles and post-heat treatment on the properties of Ti-6Al-4V-based surface nanocomposite fabricated by friction stir processing10.1016/j.surfcoat.2022.128985 ↗
45. Microstructure evolution and electrochemical properties of TiO2/Ti-35Nb-2Ta-3Zr micro/nano-composites fabricated by friction stir processing10.1016/j.matdes.2019.107680 ↗
46. Surface modification and twinning behavior in gradient graphene-based TiC/Ti6Al4V composite10.1016/j.apsusc.2022.152495 ↗
47. Microstructure evolution and mechanical properties of TiC/Ti6Al4V medical composite processed by severe plastic deformation10.1016/j.jmrt.2021.11.090 ↗
48. Six new transformation pathways connecting simple crystal structures and common intermetallic crystal structures10.1016/j.actamat.2021.117429 ↗
49. Elemental site occupancy in the L12 A3B ordered intermetallic phase in Co-based superalloys and its influence on the microstructure10.1016/j.actamat.2018.09.049 ↗
50. Bifurcation of the Kirkendall plane during interdiffusion in the intermetallic compound β-NiAl10.1016/j.actamat.2004.05.028 ↗
51. Displacive precursor phenomena in Ti–22Al–27Nb intermetallic compound prior to diffusional transformation10.1016/S1359-6454(01)00288-9 ↗
52. Effects of laser pulse modulation on intermetallic compounds formation for welding of Ti-6Al-4V and AA7075 using AA4047 filler10.1016/j.matdes.2021.110325 ↗
53. Effects of Si solution in θ-Al13Fe4 on phase transformation between Fe-containing intermetallic compounds in Al alloys10.1016/j.jallcom.2022.167587 ↗
54. Effect of the Ag addition on the compressibility, sintering and properties of Ti6Al4V/xAg composites processed by powder metallurgy10.1016/j.jallcom.2021.161813 ↗
55. Manufacturing and characterization of in-situ alloyed Ti6Al4V(ELI)-3 at.% Cu by laser powder bed fusion
56. Spray-deposited Ag nanoparticles on micro/nano structured Ti6Al4V surface for enhanced bactericidal property and cytocompatibility10.1016/j.surfcoat.2021.128010 ↗
57. Structural design and performance evaluation of Ti6Al4V/5%Cu produced by electron-beam additive technology with simultaneous double-wire feeding10.1016/j.matlet.2021.131586 ↗
58. Microstructure evolution and joining strength of diamond brazed on Ti-6Al-4V substrates using Ti-free eutectic Ag-Cu filler alloy10.1016/j.diamond.2022.109198 ↗
59. Revealing extraordinary intrinsic tensile plasticity in gradient nano-grained copper10.1126/science.1200177 ↗
60. Design of a metallic glass dispersion in pure copper by friction stir processing10.1016/j.jallcom.2022.164522 ↗
61. Microstructure and corrosion behavior of Al-Ti-TiC-CNTs/AZ31 magnesium matrix composites prepared using laser cladding and high speed friction stir processing10.1016/j.optlastec.2022.108078 ↗
62. Structural evolution of contact parts of the friction stir processing heat-resistant nickel alloy tool used for multi-pass processing of Ti6Al4V/(Cu+Al) system
63. Processing and microstructure of Ti-Cu binary alloys: a comprehensive review10.1016/j.pmatsci.2022.100933 ↗
64. Reversible dislocation movement, martensitic transformation and nano-twinning during elastic cyclic loading of a metastable high entropy alloy10.1016/j.actamat.2019.12.040 ↗
65. Uncovering the role of nanoscale precipitates on martensitic transformation and superelasticity10.1016/j.actamat.2022.117790 ↗
66. Control of microstructural characteristics and martensitic transformation behavior of Ti–Ni–Cu alloys by Pt doping10.1016/j.jallcom.2019.06.217 ↗
67. Formation of nanocrystalline β structure in metastable beta Ti alloy during high pressure torsion: the role played by stress induced martensitic transformation10.1016/j.actamat.2015.06.042 ↗
68. Mueller · 1963 · vol. 227 · 4712302
69. The liquidus surface of the system titanium-copper-silver
70. Enhanced tensile properties by heterogeneous grain structures and coherent precipitates in a CoCrNi-based medium entropy alloy10.1016/j.msea.2021.142440 ↗
71. Composite structure of α phase in metastable β Ti alloys induced by lattice strain during β to α phase transformation10.1016/j.actamat.2017.04.051 ↗
72. Microstructure of Ti-Ag immiscible alloys with liquid phase separation10.1016/j.jallcom.2017.12.138 ↗
73. Fabrication of nanoporous copper by dealloying of amorphous Ti–Cu–Ag alloys10.1016/j.jallcom.2013.01.087 ↗
74. Interfacial reactions between sapphire and Ag–Cu–Ti-based active braze alloys10.1016/j.actamat.2015.11.019 ↗
75. Factors controlling segregation tendency of solute Ti, Ag and Ta into different symmetrical tilt grain boundaries of tungsten: first-principles and experimental study10.1016/j.actamat.2021.116868 ↗
76. Microstructures and bonding strength of synthetic diamond brazed by near-eutectic Ag–Cu–in–Ti filler alloy10.1016/j.msea.2020.139711 ↗
77. Presence of silver in the strengthening particles of an Al-Cu-Mg-Si-Zr-Ti-Ag alloy during severe overaging and creep10.1016/j.actamat.2016.11.056 ↗
78. Massive transformation in Ti–6Al–4V additively manufactured by selective electron beam melting10.1016/j.actamat.2015.11.011 ↗
79. Thermomechanically influenced dynamic elastic constants of laser powder bed fusion additively manufactured Ti6Al4V10.1016/j.msea.2021.140990 ↗
80. Dilution of Al and V through laser powder deposition enables a continuously compositionally Ti/Ti6Al4V graded structure10.1016/j.jallcom.2018.05.289 ↗
81. Effects of pure Ti or Zr powder on microstructure and mechanical properties of Ti6Al4V and Ti2AlNb joints brazed with TiZrCuNi10.1016/j.msea.2020.139602 ↗
82. The effect of modulated matrix microstructure on the deformation behavior in SiCf/Ti17 composites10.1016/j.matlet.2019.01.122 ↗
83. Biocompatibility and antibacterial properties of TiCu(Ag) thin films produced by physical vapor deposition magnetron sputtering10.1016/j.apsusc.2021.151604 ↗
84. Effect of a Ti diffusion barrier on the cobalt silicide formation: solid solution, segregation and reactive diffusion10.1016/j.actamat.2020.116504 ↗
85. Morphological evolution of transformation products and eutectoid transformation(s) in a hyper-eutectoid Ti-12 at% Cu alloy10.1016/j.actamat.2019.01.044 ↗
86. Microstructural evolution and properties of TLP diffusion bonding super-Ni/NiCr laminated composite to Ti-6Al-4V alloy with Cu interlayer10.1016/j.matdes.2017.09.028 ↗
87. Hexagonal martensite decomposition and phase precipitation in Ti–Cu alloys10.1016/j.matdes.2011.03.040 ↗
88. Role of tetragonal distortion on domain switching and lattice strain of piezoelectrics by in-situ synchrotron diffraction10.1016/j.scriptamat.2020.11.012 ↗
89. Structure of martensite in sputter-deposited (Ni,Cu)-rich Ti–Ni–Cu thin films containing Ti(Ni,Cu)2 precipitates10.1016/j.actamat.2008.11.035 ↗
90. Martensite structure in Ti–Ni–Hf–Cu quaternary alloy ribbons containing (Ti,Hf)2Ni precipitates10.1016/j.actamat.2010.03.015 ↗
91. Tracking the αʺ martensite decomposition during continuous heating of a Ti-6Al-6V-2Sn alloy10.1016/j.actamat.2017.06.018 ↗
92. In-situ observation of nucleation, growth and interaction of deformation-induced αʺ martensite in metastable Ti–10V–2Fe–3Al10.1016/j.msea.2020.140237 ↗
93. {10-12} twinning induced by the interaction between {11-21} twin and β phase in α+β Ti alloys10.1016/j.actamat.2022.117900 ↗
94. Rapid quenching of semisolid Ti-Cu alloys: insights into globular microstructure formation and coarsening10.1016/j.actamat.2017.08.006 ↗
95. Ti–Cu–Ni shape memory bulk metallic glass composites10.1016/j.actamat.2012.09.042 ↗
96. Atomic-resolution studies on reactions between basal dislocations and {10-12} coherent twin boundaries in a Mg alloy10.1016/j.jmst.2020.06.017 ↗
97. Effect of stress-induced α″ martensite on Young's modulus of β Ti–33.6Nb–4Sn alloy10.1016/j.msea.2013.09.053 ↗
98. Formation of typical Cu–Ti intermetallic phases via a liquid-solid reaction approach10.1016/j.intermet.2019.106577 ↗
99. Interfacial microstructure and performance of nano-diamond film/Ti-6Al-4V joint brazed with AgCuTi alloy10.1016/j.diamond.2016.05.011 ↗
100. On the crystallographic anisotropy of nanoindentation in pseudoelastic NiTi10.1016/j.actamat.2012.09.081 ↗