journal article·2023-07Open access

Effect of compression bonding temperature on the strength-ductility balance of AA7075 alloy

Hamid Ghorbani, Roohollah Jamaati

Abstract

In this study, the effect of compression bonding temperature on the microstructure and strength-ductility balance of AA7075 alloy was investigated. The results showed that dynamic recovery (DRV) was the dominant restoration mechanism in the compressed samples at 25, 100, 200, and 300 °C decreasing the dislocation density of elongated grains, while dynamic recrystallization (DRX) was predominant in the compressed sample at 400 °C forming fine equiaxed grains. By increasing the compression temperature, the bonding quality is improved. Several MgZn2 peaks could be observed in the diffraction pattern of the processed sample at 400 °C, confirming the occurrence of overaging. By increasing the compression temperature from 25 °C to 300 °C, the texture parameter of {200} (as recrystallization texture) was continuously reduced from 2.13 to 1.11, while the texture parameter of {220} (as deformation texture) was continuously enhanced from 2.09 to 4.91 due to the higher height reduction in the larger compression temperature. By further increasing the compression temperature to 400 °C, the texture parameter of {200} is significantly increased from 1.11 to 3.21, while the texture parameter of {220} is remarkably decreased from 4.91 to 0.83 owing to the occurrence of DRX. By increasing the temperature from 25 °C to 400 °C, the hardness of both AA7075 and pure aluminum layers was decreased due to the intensifying recovery and recrystallization. After the compression bonding, no evidence of the Portevin Le Chatelier was found and the stress-strain curves exhibited normal behavior. With increasing the temperature from 25 °C to 400 °C, yield and ultimate tensile strength were decreased from 672.7 MPa and 689.8 MPa to 187.4 MPa and 374.9 MPa, respectively, while the total elongation and energy absorption were increased from 6.2% to 40.6 J/cm3 to 33.7% and 108.1 J/cm3, respectively. At the early stage of plastic deformation, the strain hardening rate of the compressed sample at 400 °C was significantly lower than that of other compressed samples. However, when the ε reaches 0.09, the strain hardening rate of the sample became larger than that of other processed samples due to the recovery of the strain hardening rate (RSHR) phenomenon at stage III in the compressed sample at 400 °C. The fracture features of all samples were characterized by dimples and cleavage facets, indicating the occurrence of a mixed ductile/brittle mode of fracture. However, by increasing the compression temperature, the dimpled portion of the fracture surface was increased. The dimples were coarsened when the compression temperature increased owing to the softening of samples as well as coarsening of MgZn2 precipitates at higher temperatures.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties · Magnesium Alloys: Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (52)

Show source-provided references
1. Effect of single roll drive cross rolling on the microstructure, crystallographic texture, and mechanical behavior of Al–Zn–Mg–Cu alloy10.1007/s43452-021-00362-9 ↗
2. Edge-crack free and high mechanical properties of AA7075 sheets by using cryorolling and subsequent aging10.1016/j.jallcom.2022.167556 ↗
3. Cryogenic deformation behavior and failure mechanism of AA7075 alloy sheets tempered at different conditions10.1016/j.msea.2022.143396 ↗
4. Asymmetric cold rolling of AA7075 alloy: the evolution of microstructure, crystallographic texture, and mechanical properties10.1016/j.msea.2021.141801 ↗
5. Investigation on mechanical behavior and plastic damage of AA7075 aluminum alloy by thermal small punch test: experimental trials, numerical analysis10.1016/j.jmapro.2019.12.012 ↗
6. The effects of Cu, Zn and Zr on the solution temperature and quenching sensitivity of Al–Zn–Mg–Cu alloys10.1016/j.matchemphys.2020.122853 ↗
7. A novel technique to form gradient microstructure in AA5052 alloy10.1016/j.msea.2020.139075 ↗
8. Effect of gradient microstructure on the mechanical properties of aluminum alloy10.1016/j.matchar.2021.111023 ↗
9. Interfacial microstructure evolution and mechanical properties of AlCoCrFeNi2.1 alloy by multilayer additive hot compression bonding10.1016/j.intermet.2023.107867 ↗
10. Accumulative channel-die compression bonding (ACCB): a new severe plastic deformation process to produce bulk nanostructured metals10.1016/j.jmatprotec.2013.02.016 ↗
11. Heterogeneous microstructure and enhanced mechanical properties in annealed multilayered IF steel10.1016/j.msea.2019.05.034 ↗
12. Effect of friction, annealing conditions and hardness on the bond strength of Al/Al strips produced by cold roll bonding process10.1016/j.matdes.2010.04.022 ↗
13. Investigation of the parameters of the cold roll bonding (CRB) process10.1016/j.msea.2009.11.069 ↗
14. Cold roll bonding bond strengths: review10.1179/026708310X12815992418256 ↗
15. The role of surface preparation parameters on cold roll bonding of aluminum strips10.1007/s11665-010-9664-7 ↗
16. Effect of Al2O3 nano-particles on the bond strength in CRB process10.1016/j.msea.2010.04.020 ↗
17. Effect of heat treatment on bonding mechanism and mechanical properties of high strength Cu/Al/Cu clad composite10.1016/j.jallcom.2019.06.132 ↗
18. Segregation behavior, microstructure and properties of TA2/AA7005 composite plates manufactured by horizontal twin-roll casting under the effect of an electromagnetic oscillation field10.1016/j.msea.2022.143752 ↗
19. Insight into the bonding mechanism in Cu/Al/Cu clad sheets via introduction of thin SUS304 interlayer10.1016/j.jmrt.2022.11.076 ↗
20. Tensile properties, microstructures and fracture behaviors of an Al-Zn-Mg-Cu alloy during ageing after solution treating and cold-rolling10.1016/j.msea.2018.03.098 ↗
21. In situ evaluation of dynamic precipitation during plastic straining of an Al–Zn–Mg–Cu alloy10.1016/j.actamat.2012.01.002 ↗
22. An improved thermo-mechanical treatment of high-strength Al–Zn–Mg–Cu alloy for effective grain refinement and ductility modification10.1016/j.jmatprotec.2016.08.027 ↗
23. Enhanced grain refinement in AA7050 Al alloy by deformation-induced precipitation10.1016/j.msea.2012.04.011 ↗
24. Microstructure evolution of multilayered composite sheets of AA1050/AA7050 Al alloys produced by Asymmetric Accumulative Roll-Bonding10.1016/j.matchar.2020.110226 ↗
25. Synergistic effects of hybrid (HA+Ag) particles and friction stir processing in the design of a high-strength magnesium matrix bio-nano composite with an appropriate texture for biomedical applications10.1016/j.jmbbm.2021.104983 ↗
26. Deformation behavior of as-cast and as-extruded Mg97Zn1Y2 alloys during compression, as tracked by in situ neutron diffraction10.1016/j.ijplas.2018.08.001 ↗
27. Investigation of microstructure, crystallographic texture, and mechanical behavior of magnesium-based nanocomposite fabricated via multi-pass FSP for biomedical applications10.1016/j.jmbbm.2021.104894 ↗
28. Water-assisted crystallization of nanoporous tin oxide formed by anodic oxidation on cold sprayed tin coating10.1016/j.jallcom.2021.160207 ↗
29. Effect of traverse and rotational speeds on microstructure, texture, and mechanical properties of friction stir processed AZ91 alloy10.1016/j.matchar.2021.111235 ↗
30. Simultaneous improvement of strength and toughness in Al–Zn–Mg–Cu/pure Al laminated composite via heterogeneous microstructure10.1016/j.msea.2023.145362 ↗
31. Effect of two-step annealing on recrystallized structure and mechanical properties in AA7075/AA1100 laminated metal composites processed by accumulative roll bonding10.1016/j.matchar.2019.109951 ↗
32. Improved mechanical anisotropy and texture optimization of a 3xx aluminum alloy by differential temperature rolling10.1016/j.msea.2020.140278 ↗
33. Improved tensile properties in heterostructured 1050/7050 Al sheets produced by accumulative roll bonding10.1016/j.jmrt.2022.01.151 ↗
34. Investigation on microstructure and mechanical properties of Al/Al-Zn-Mg–Cu laminated composite fabricated by accumulative roll bonding (ARB) process10.1016/j.msea.2018.01.130 ↗
35. Improving mechanical properties of laminate heterogeneous GW103K/AZ31 alloys10.1016/j.jallcom.2023.169156 ↗
36. Dual-phase hetero-structured strategy to improve ductility of a low carbon martensitic steel10.1016/j.msea.2021.142584 ↗
37. Impact of short range ordering on the anomalous four-stage strain hardening behavior of low solid-solution hardening Ni–Cr alloys10.1016/j.msea.2021.141193 ↗
38. Influence of Co addition on the deformation behavior and mechanical properties of Ni–16Cr–11Mo–2Cu alloy10.1016/j.msea.2019.138442 ↗
39. Reverse partitioning of Al from κ-carbide to the γ-matrix upon Ni addition and its strengthening effect in Fe–Mn–Al–C lightweight steel10.1016/j.msea.2021.141563 ↗
40. The dual effect of grain size on the strain hardening behaviors of Ni-Co-Cr-Fe high entropy alloys10.1016/j.jmst.2022.06.001 ↗
41. Achieving high hetero-deformation induced (HDI) strengthening and hardening in brass by dual heterostructures10.1016/j.jmst.2021.03.088 ↗
42. Interface regulation effects on mechanical behavior of heterostructure Ti6Al4V/TiAl-based laminated composite sheets10.1016/j.ceramint.2022.05.278 ↗
43. Effect of heterostructure and hetero-deformation induced hardening on the strength and ductility of brass10.1016/j.actamat.2020.01.037 ↗
44. Hetero-deformation induced (HDI) hardening does not increase linearly with strain gradient10.1016/j.scriptamat.2019.08.022 ↗
45. Microstructure and mechanical properties of IF/St52 steel composite produced by friction stir lap welding10.1016/j.msea.2019.138775 ↗
46. Microstructure and mechanical properties of 1060/7050 laminated composite produced via cross accumulative extrusion bonding and subsequent aging10.1016/j.jallcom.2020.154094 ↗
47. Design of pure aluminum laminates with heterostructures for extraordinary strength-ductility synergy10.1016/j.jmst.2021.05.030 ↗
48. Effect of layer thickness on the enhanced strength and ductility of laminated Ti/Al composite10.1016/j.msea.2022.144230 ↗
49. Microstructure and enhanced cryogenic tensile property of a heterostructured Al–AlN/Al–Mg composite fabricated by accumulative roll bonding (ARB)10.1016/j.jmrt.2022.09.037 ↗
50. Mesoscale hetero-deformation induced (HDI) stress in FeAl-based metallic-intermetallic laminate (MIL) composites10.1016/j.actamat.2021.116949 ↗
51. Revealing hetero-deformation induced (HDI) stress strengthening effect in laminated Al-(TiB2+TiC)p/6063 composites prepared by accumulative roll bonding10.1016/j.jallcom.2019.152285 ↗
52. Tailoring of interface structure and mechanical properties in ARBed 1100/7075 laminated composites by cold rolling10.1016/j.msea.2019.03.075 ↗