journal article·2024-03Open access

Extrusion limit diagram of Mg–5Bi–3Al–1Zn alloy and effects of extrusion parameters on its microstructures and mechanical properties

Qinghang Wang, Li Wang, Jiaze Xu, Haowei Zhai, Yang Chen, Shouxin Xia, Xu Qin, Yongfei Li, Bin Jiang, Daolun Chen

Abstract

Hot-compressive tests and finite element simulations were carried out to construct an extrusion limit diagram of a Mg–5Bi–3Al–1Zn (wt.%) alloy in this work. It was observed that 310 °C became a dividing line, below which the safe extrusion zone was narrow because the stress required to induce the plastic flow of alloy was higher than the pressure limit. Once the temperature exceeded this critical temperature, a wide safe extrusion zone controlled by the cracking limit was attained. The theoretical maximum ram extrusion speed was calculated as approximately 48 mm/s at 310 °C. No hot cracks occurred on the surface of alloys extruded at 30 and 44 mm/s; while at 56 mm/s, obvious orange peel defects were observed. Through further microstructural observation, the 44 mm/s extruded alloy exhibited a complete dynamic recrystallization structure with an average grain size of 21.9 μm, along with a relatively weak basal fiber texture (with a maximum pole intensity of 5.8) and plentiful nano-Mg3Bi2 phases. These microstructure features led to superior tensile properties (namely a tensile yield strength of 270 MPa, an ultimate tensile strength of 375 MPa and an elongation of 15%) at the high-speed extrusion.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. The wear and arc erosion behavior of novel copper based functionally graded electrical contact materials fabricated by hot pressing assisted electroless plating10.1016/j.apt.2021.05.053 ↗
2. Characterization of nanocrystalline Cu25Mo electrical contact material synthesized via ball milling10.12693/APhysPolA.132.886 ↗
3. Optimization of mechanical alloying parameters of Cu25W electrical contact material10.12693/APhysPolA.132.909 ↗
4. Arc-erosion behavior of boric oxide-reinforced silver-based electrical contact materials produced by mechanical alloying10.1007/s11664-014-3399-4 ↗
5. Effect of cubic and hexagonal boron nitride additions on the synthesis of Ag-SnO2 electrical contact material10.1166/jno.2019.2592 ↗
6. Research advances of magnesium and magnesium alloys worldwide in 202210.1016/j.jma.2023.07.011 ↗
7. Significant improvement in extrudability of Mg–9Al–0.8Zn–0.9Ca–0.6Y alloy through mischmetal addition10.1007/s12540-020-00822-6 ↗
8. Effects of cerium addition on the microstructure, mechanical properties and hot workability of ZK60 alloy10.1016/j.msea.2012.09.026 ↗
9. Influence of Bi addition on dynamic recrystallization and precipitation behaviors during hot extrusion of pure Mg10.1016/j.jmst.2019.10.036 ↗
10. Novel Mg–Bi–Al alloy with extraordinary extrudability and high strength10.1016/j.jallcom.2020.156026 ↗
11. Comparative study of extrudability, microstructure, and mechanical properties of AZ80 and BA53 alloys10.1016/j.jma.2021.07.009 ↗
12. Enhancing tensile strength and ductility of high-speed-extruded Mg–5Bi–2Al through trace Mn addition10.1016/j.matchar.2021.111500 ↗
13. Influence of Ca addition on microstructural characteristics and mechanical properties of Mg–5Bi–3Al alloy extruded at extremely high speed10.1016/j.msea.2022.144490 ↗
14. Extrusion limit diagram of AZ91–0.9Ca–0.6Y–0.5MM alloy and effects of extrusion parameters on its microstructure and mechanical properties10.1016/j.jma.2021.06.002 ↗
15. Effect of scandium on the hot extrudability of 7075 aluminum alloy10.1007/s12540-010-0823-z ↗
16. Extrusion limit diagram of IN 690 super-alloy tube based on hot processing map10.1007/s00170-016-9271-3 ↗
17. Extrusion limits of magnesium alloys10.1007/s11661-007-9323-2 ↗
18. Construction of extrusion limit diagram for AZ31 magnesium alloy by FE simulation10.1016/j.jmatprotec.2003.12.003 ↗
19. Effects of extrusion speed on the microstructure and mechanical properties of Mg–9Al–0.8Zn–0.9Ca–0.6Y–0.5MM alloy10.1007/s12540-020-00867-7 ↗
20. Exploiting an as-extruded fine-grained Mg-Bi-Mn alloy with strength-ductility synergy via dilute Zn addition10.1016/j.jallcom.2022.166337 ↗
21. Microstructural evolution and mechanical properties of binary Mg–xBi (x = 2, 5, and 8 wt%) alloys10.1016/j.jma.2020.03.015 ↗
22. Effects of homogenization temperature on microstructure and mechanical properties of high-speed-extruded Mg–5Bi–3Al alloy10.1016/j.jma.2021.07.007 ↗
23. Effect of Bi addition on the heat resistance of as-extruded AZ31 magnesium alloy10.3390/ma16030996 ↗
24. Establishment of constitutive model and analysis of dynamic recrystallization kinetics of Mg-Bi-Ca alloy during hot deformation10.3390/ma15227986 ↗
25. A constitutive model to describe high temperature flow behavior of AZ31B magnesium alloy processed by equal-channel angular pressing10.1016/j.msea.2019.03.106 ↗
26. Effect of the Zener-Hollomon parameter on the dynamic recrystallization kinetics of Mg–Zn–Zr–Yb magnesium alloy10.1016/j.commatsci.2019.05.015 ↗
27. Analysis of dynamic recrystallization behaviors in resistance heating compressions of heat-resistant alloy by multi-field and multi-scale coupling method10.1016/j.commatsci.2018.03.016 ↗
28. Effect of the extrusion conditions on the texture and mechanical properties of indirect-extruded Mg–3Al–1Zn alloy10.1016/j.jmatprotec.2009.07.012 ↗
29. Novel Mg-Bi-Mn wrought alloys: the effects of extrusion temperature and Mn addition on their microstructures and mechanical properties10.1016/j.jma.2021.11.028 ↗
30. Particle effects on recrystallization in magnesium–manganese alloys: particle-stimulated nucleation10.1016/j.actamat.2009.02.032 ↗
31. Achieving high strength near 400 MPa in an ultra-fine grained Mg–Bi–Ca ternary alloy via low-temperature extrusion10.1016/j.jmrt.2023.08.202 ↗
32. Twin recrystallization mechanisms in magnesium-rare earth alloys10.1016/j.actamat.2015.05.044 ↗
33. Twin recrystallization mechanisms and exceptional contribution to texture evolution during annealing in a magnesium alloy10.1016/j.actamat.2016.12.058 ↗
34. Formation of the elliptical texture and its effect on the mechanical properties and stretch formability of dilute Mg-Sn-Y sheet by Zn addition10.1016/j.msea.2019.01.040 ↗
35. Optimization of Mn content for high strengths in high-speed extruded Mg-0.3Al-0.3Ca (wt%) dilute alloy10.1016/j.msea.2016.07.098 ↗
36. Improving tensile properties of dilute Mg-0.27Al-0.13Ca-0.21Mn (at.%) alloy by low temperature high speed extrusion10.1016/j.jallcom.2015.07.051 ↗
37. High-speed extrusion of heat-treatable Mg–Al–Ca–Mn dilute alloy10.1016/j.scriptamat.2015.01.010 ↗
38. Strong and ductile age-hardening Mg-Al-Ca-Mn alloy that can be extruded as fast as aluminum alloys10.1016/j.actamat.2017.03.046 ↗
39. High-speed extrusion of dilute Mg-Zn-Ca-Mn alloys and its effect on microstructure, texture and mechanical properties10.1016/j.msea.2016.10.007 ↗
40. Effect of extrusion speeds on the microstructure, texture and mechanical properties of high-speed extrudable Mg-Zn-Sn-Mn-Ca alloy10.1016/j.vacuum.2018.08.041 ↗
41. Rare earth texture and improved ductility in a Mg-Zn-Gd alloy after high-speed extrusion10.1016/j.msea.2016.04.093 ↗
42. High-speed indirect extrusion of Mg–Sn–Al–Zn alloy and its influence on microstructure and mechanical properties10.1016/j.jallcom.2016.01.163 ↗
43. Hall-Petch relationship in Mg alloys: a review10.1016/j.jmst.2017.07.022 ↗
44. A new strong and ductile multicomponent rare-earth free Mg–Bi-based alloy achieved by extrusion and subsequent short-term annealing10.1016/j.msea.2022.144309 ↗
45. Effects of precipitate shape and orientation on dispersion strengthening in magnesium alloys10.1016/S1359-6462(02)00497-9 ↗