Muti-mechanism of the improving wear performance for titanium alloy via laser powder bed fusion
Source abstract
Abstract
Wear is the key issue hindering the further application of titanium alloy. The aim of this work was to explore the strengthening mechanisms for the wear properties of Ti–15Mo alloys via laser powder bed fusion (LPBF) by the La2O3 addition. The results showed that the grain of LPBF-fabricated Ti–15Mo/La2O3 composites was obviously refined after La2O3 addition by heterogeneous nucleation and inhibited grain growth. The average grain size of Ti–15Mo/(0.2 wt%, 0.4 wt%, 0.6 wt% and 0.8 wt%) La2O3 composites is 11.75 μm, 10.85 μm, 10.39 μm, and 9.99 μm, respectively. The wear rate of Ti–15Mo/(0.2 wt% - 0.8 wt%) La2O3 composites is 1.5916 × 10−4mm3N−1m−1, 1.2885 × 10−4mm3N−1m−1, 0.6821 × 10−4mm3N−1m−1 and 0.6063 × 10−4mm3N−1m−1, respectively. Thanks to the combined effect of fine grain strengthening, grain boundary strengthening, precipitation strengthening, dispersion strengthening and dislocation strengthening, the wear resistance of the obtained sample exceeds that of the LPBF-fabricated Ti–15Mo sample more than five times and that of the LPBF-fabricated CP-Ti sample more than ten times.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Titanium Alloys Microstructure and Properties · Additive Manufacturing Materials and Processes · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (44)
Show source-provided references
1. Microstructure and mechanical properties of Ti–6Al–4V alloy fabricated using electron beam freeform fabrication10.1016/j.vacuum.2019.06.030 ↗
2. The effect of a novel low-temperature vacuum heat treatment on the microstructure and properties of Ti–6Al–4V alloys manufactured by selective laser melting10.1016/j.vacuum.2021.110554 ↗
3. Additive manufacturing hybrid Ni/Ti-6Al-4V structural component via selective laser melting and cold spraying10.1016/j.vacuum.2018.02.040 ↗
4. Ti based biomaterials, the ultimate choice for orthopaedic implants – a review10.1016/j.pmatsci.2008.06.004 ↗
5. Development of a new β Ti alloy with low modulus and favorable plasticity for implant material10.1016/j.msec.2015.12.076 ↗
6. Dzogbewu · Laser powder bed fusion of Ti15Mo[J] · 2020
7. The anisotropic of corrosion and tribocorrosion behaviors of Ti 15Mo alloy fabricated by selective laser melting
8. Characterization of NiTi SMA in its unusual behaviour in wear tests10.1016/j.triboint.2019.05.005 ↗
9. Wear resistance of experimental Ti–Cu alloys10.1016/S0142-9612(03)00157-1 ↗
10. Microstructure and mechanical behaviour of Ti-6Al-4V matrix Reinforced with WCp developed by squeeze casting[J]. V. Vijayan10.1155/2022/6381265 ↗
11. Room and high temperature dry sliding wear behavior of Boron modified as-cast Ti-6Al-4V alloys against hardened steel10.1016/j.wear.2018.10.021 ↗
12. Selective laser melting of pure tantalum: densification, microstructure and mechanical behaviors10.1016/j.msea.2017.09.083 ↗
13. Microstructure tailoring to enhance strength and ductility in pure tantalum processed by selective laser melting10.1016/j.msea.2020.139352 ↗
14. Effects of Ta content on phase transformation in selective laser melting processed Ti-13Nb-13Zr alloy and its correlation with elastic properties10.1016/j.vacuum.2020.109798 ↗
15. Additive manufacturing of high-strength commercially pure titanium through lanthanum oxide addition10.1016/j.matchar.2021.111074 ↗
16. Promoting the columnar to equiaxed transition and grain refinement of titanium alloys during additive manufacturing10.1016/j.actamat.2019.02.020 ↗
17. Effect of addition of micron-sized lanthanum oxide particles on morphologies, microstructures and properties of the wire laser additively manufactured Ti–6Al–4V alloy10.1016/j.msea.2020.140475 ↗
18. Corrosion behaviour of Ti–15Mo alloy for dental implant applications10.1016/j.jdent.2008.03.007 ↗
19. Comparison of wear properties of commercially pure titanium prepared by selective laser melting and casting processes10.1016/j.matlet.2014.11.156 ↗
20. Corrosion and tribocorrosion behaviour of β-type Ti-Nb and Ti-Mo surfaces designed by diffusion treatments for biomedical applications10.1016/j.corsci.2018.06.024 ↗
21. Microstructure tailoring of Ti–15Mo alloy fabricated by selective laser melting with high strength and ductility10.1016/j.msea.2021.141962 ↗
22. Realization of synergistic enhancement for strength, wear resistance and ductility via adding La2O3 particles in (TiB+TiC)/Ti6Al4V composite
23. Mostafa M Y A. XRD peak broadening modelling for Al-alloys characterization compared with Rietveld profile analysis[J]. Mater Today,..
24. Significance of grain refinement on micro-mechanical properties and structures of additively-manufactured CoCrFeNi high-entropy alloy
25. Coherent ω phase induced yield strength improvement in Ti-19Nb-1.5Mo-4Zr-8Sn alloy10.1016/j.rinp.2020.103366 ↗
26. Effect of lanthanum oxide addition on microstructure and wear performance of iron-chromium alloy manufactured by laser direct deposition additive manufacturing10.3390/ma15093234 ↗
27. Corrosion and wear properties of TB2 titanium alloy borided by pack boriding with La2O310.1016/S1003-6326(22)65839-4 ↗
28. Effect of trace lanthanum hexaboride and boron additions on microstructure, tensile properties and anisotropy of Ti-6Al-4V produced by additive manufacturing10.1016/j.msea.2018.02.012 ↗
29. Numerical investigation of interfacial dynamics for the melt pool of Ti-6Al-4V powders under a selective laser10.1016/j.ijheatmasstransfer.2019.01.030 ↗
30. Densification behavior, microstructure evolution, and wear performance of selective laser melting processed commercially pure titanium10.1016/j.actamat.2012.04.006 ↗
31. Suppression of epitaxial grain growth in laser powder bed fusion fabricated Inconel 625 through intermittent variation of the build layer thickness10.1016/j.msea.2023.145679 ↗
32. Microstructure and room-temperature tensile property of Ti-5.7Al-4.0Sn-3.5Zr-0.4Mo-0.4Si-0.4Nb-1.0Ta-0.05C with near equiaxed β grain fabricated by laser directed energy deposition technique10.1016/j.jmst.2021.03.012 ↗
33. Effect of substrate preheating on the texture, phase and nanohardness of a Ti–45Al–2Cr–5Nb alloy processed by selective laser melting10.1016/j.scriptamat.2016.02.022 ↗
34. Li L, Liu J, Ding N. Substructure evolution in two phases based constitutive model for hot deformation of TC18 in a + b phase region[J]..
35. Selective electron beam melting of Ti–48Al–2Nb–2Cr: microstructure and aluminium loss10.1016/j.intermet.2014.01.004 ↗
36. Influence of secondary thermal cycle on softening behavior and mechanism of heat affected zone in TIG-welded spray formed 7055 aluminum alloy10.1016/j.jmrt.2022.10.062 ↗
37. Microstructure, solidification behavior and mechanical properties of Al-Si-Mg-Ti/TiC fabricated by selective laser melting
38. Anisotropic mechanical behavior of biomedical Ti-13Nb-13Zr alloy manufactured by selective laser melting10.1016/j.jallcom.2018.05.179 ↗
39. Effect of the scanning strategy on microstructure and mechanical anisotropy of Hastelloy X superalloy produced by Laser Powder Bed Fusion
40. Wear behavior of the plasma and thermal oxidized Ti-15Mo and Ti-6Al-4V alloys10.1088/1757-899X/174/1/012055 ↗
41. Effect of rare earth oxide on the properties of laser cladding layer and machining vibration suppressing in side milling10.1016/j.apsusc.2014.09.195 ↗
42. Microstructure and mechanical behavior of the laser synthesized composites modified by micro/nano scale rare earth oxides10.1016/j.jallcom.2021.162641 ↗
43. Effect of β (110) texture intensity on α-variant selection and microstructure morphology during β→α phase transformation in near α titanium alloy10.1016/j.actamat.2016.12.069 ↗
44. Densification, microstructure evolution and fatigue behavior of Ti-13Nb-13Zr alloy processed by selective laser melting10.1016/j.powtec.2018.09.073 ↗