Abstract

The microstructural characteristics of brazing seams significantly influence the mechanical properties of brazed joints. In this study, a novel Ni3Al-based single crystal superalloy(Alloy 1) with high Mo content was brazed with a Ni-B-Si-Ti filler. The evolution of microstructure and mechanical properties of brazed joints were investigated after thermal exposure at 1000°C up to 300h. The brazed joint was mainly composed of the athermally solidified zone (ASZ), isothermal solidification zone (ISZ), diffusion affected zone (DAZ), and base metal (BM). As the increase of thermal exposure time, the tensile strength of the joint at 980°C decreases from 625MPa at 0h of thermal exposure to 443MPa after 300h of thermal exposure. It is suggested that as the duration of thermal exposure increases, the skeleton phases gradually aggregate at the ASZ/ISZ interface, reducing the relative barrier effect of the skeleton in ASZ. Simultaneously, the ASZ/ISZ interface becomes smoother over time, which in turn leads to rapid crack propagation.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High Temperature Alloys and Creep · Intermetallics and Advanced Alloy Properties · Aluminum Alloy Microstructure Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. Microstructure and cracking behavior of Ni3Al-based IC21 alloy fabricated by selective laser melting10.1016/j.matchar.2022.112592 ↗
2. Microstructural characteristics and mechanical properties of IC10 superalloy and (CoCrNi)94Al3Ti3 MEA joint brazed using NiCrSiB filler10.1016/j.matchar.2022.111964 ↗
3. Microstructural evolution and phase transformation of Ni3Al-based superalloys after thermal exposure10.1016/j.vacuum.2019.109038 ↗
4. Effect of heat input on microstructure and mechanical properties of IC10 Ni3Al-based superalloy electron beam welding joint10.1016/j.vacuum.2020.109765 ↗
5. Investigation on microstructure and mechanical properties of a vacuum brazed joint of γ′-strengthened Co-based single crystal superalloy before and after the post-bond heat treatment10.1016/j.vacuum.2020.109413 ↗
6. Surface modification of Ni3Al-based alloy IC6 with intense pulsed ion beams10.1016/S0042-207X(02)00505-5 ↗
7. Multi-scale characterization of stray grain in the platform of nickel-base single crystal turbine blade10.1016/j.vacuum.2016.06.016 ↗
8. The effects of graphene content on the mechanical properties and thermal conductivity of Inconel 718 superalloy brazed using BNi-2/graphene composite filler metal10.1016/j.rinp.2019.102828 ↗
9. A high-strength vacuum-brazed TiAl/Ni joint at room temperature and high temperature with an amorphous foil Zr-Al-Ni-Co filler metal10.1016/j.jmapro.2019.05.024 ↗
10. A new high entropy alloy brazing filler metal design for joining skutterudite thermoelectrics to copper10.1016/j.jallcom.2020.157750 ↗
11. Performance of GH4169 brazed joint using a new designed nickel-based filler metal via cluster-plus-glue-atom model10.1016/j.jmst.2019.08.028 ↗
12. Brazing TiC/Ti matrix composite using Ti Ni eutectic braze alloy10.1016/j.vacuum.2018.08.012 ↗
13. Effects of brazing temperature on microstructure and properties of interface between cBN and Co-based active filler metals10.1016/j.vacuum.2017.08.021 ↗
14. Experimental investigations on creep rupture strength and failure mechanism of vacuum brazed joints of a DS superalloy at elevated temperature10.1016/j.msea.2012.02.099 ↗
15. Elastic modulus and hardness characterization for microregion of Inconel 625/BNi-2 vacuum brazed joint by high temperature nanoindentation10.1016/j.vacuum.2020.109582 ↗
16. Joining of superalloy Inconel 600 by diffusion induced isothermal solidification of a liquated insert metal10.1016/j.matchar.2007.08.023 ↗
17. Effect of post-bond heat treatment on microstructure and mechanical properties of the wide gap TLP bonded IC10 superalloy with a low boron Ni3Al-based interlayer10.1016/j.jmapro.2020.03.002 ↗
18. The role of TLP process variables in improvement of microstructure and mechanical properties in TLP joints of GTD-111/Ni-Cr-Fe-B-Si/GTD-111 system10.1016/j.jmapro.2018.03.036 ↗
19. Vacuum TLP bonding of Inconel 617 superalloy using Ni-Cr-Si-Fe-B filler metal: metallurgical structure and mechanical properties10.1016/j.vacuum.2018.03.048 ↗
20. Effects of post-weld heat treatment on microstructure and mechanical properties of TLP bonded Inconel 718 superalloy10.1016/j.msea.2013.10.013 ↗
21. The joint properties of a high-chromium Ni-based superalloy made by diffusion brazing: microstructural evolution, corrosion resistance and mechanical behavior10.1016/j.jmapro.2018.11.025 ↗
22. Microstructure and mechanical properties of transient liquid phase (TLP)-bonded Ni3Al intermetallic compounds
23. Transient liquid phase bonding of IC10 single crystal with GH3039 superalloy using BNi2 interlayer: microstructure and mechanical properties10.1016/j.matdes.2015.11.041 ↗
24. Microstructural evolution and mechanical properties of TLP bonded joints of Mar-M247 superalloys with Ni-Cr-Co-W-Ta-B interlayer10.1016/j.jmatprotec.2017.03.021 ↗
25. TLP bonding of cast IN718 nickel based superalloy: process–microstructure–strength characteristics10.1016/j.msea.2013.01.029 ↗
26. Microstructure and tensile properties of nickel-based superalloy K417G bonded using transient liquid-phase infiltration10.1016/j.matdes.2013.04.024 ↗
27. Effect of holding time on microstructure and properties of transient liquid-phase-bonded joints of a single crystal alloy10.1007/s11665-015-1504-3 ↗
28. Post-bond heat treatment effects on the wide gap transient liquid phase bonding of Inconel 718 with BNi-2 paste filler metal10.1016/j.msea.2019.138267 ↗
29. Microstructure evolution mechanism during post-bond heat treatment of transient liquid phase bonded wrought IN718 superalloy: an approach to fabricate boride-free joints10.1016/j.jallcom.2017.06.206 ↗
30. Microstructural characterization and phase separation sequences during solidification of Ni3Al-based superalloy10.1007/s40195-017-0634-z ↗
31. Transient liquid phase bonding of Ni3Al based superalloy using Mn–Ni–Cr filler10.1016/j.jmrt.2021.02.018 ↗
32. On the influence of boron-addition on TLP bonding time in a Ni3Al-based intermetallic10.1016/j.intermet.2009.10.011 ↗
33. Microstructure evolution and mechanical behavior of Ni-based single crystal superalloy joint brazed with mixed powder at elevated temperature10.1016/j.jmst.2017.01.027 ↗
34. Effect of transient liquid phase bonding time on the microstructure, isothermal solidification completion and the mechanical properties during bonding of Inconel 625 superalloy using Cr-Si-B-Ni filler metal10.1016/j.jmapro.2019.01.019 ↗
35. The effect of heat treatment sequence on microstructure and mechanical properties of diffusion brazed IN-939 superalloy10.1016/j.jmatprotec.2018.11.020 ↗
36. Transient liquid phase bonding of in738lc/MBF-15/in738lc: solidification behavior and mechanical properties10.1016/j.jmst.2016.07.017 ↗
37. Okamoto · 2016
38. Effect of filler metal on the microstructural evolution and mechanical properties of wide gap brazed K417G superalloy joints10.1016/j.vacuum.2020.109967 ↗
39. Topologically inverse microstructure in single-crystal superalloys: microstructural stability and properties at ultrahigh temperature10.1080/21663831.2021.1982785 ↗
40. Influence of chemical composition on coarsening kinetics of coherent L12 precipitates in FCC complex concentrated alloys10.1016/j.jallcom.2023.171711 ↗