Improving tension fatigue performance of gray cast iron by LSPwC-induced gradient structure and carbon diffusion
Source abstract
Abstract
HT250 Gray cast iron (GCI) commonly utilized in diesel engine cylinders, is susceptible to fatigue failure under alternating stress conditions. To address this issue, the investigation involved the application of laser shock peening without coating (LSPwC) on HT250 GCI to assess its impact on the high cycle tension fatigue properties of the material. Both experimental and simulation methodologies were employed to analyze the effects of LSPwC on residual stress, microhardness, and microstructure in HT250 GCI. The LSPwC resulted in a substantial 29% enhancement in the high cycle tension fatigue limit of the HT250 GCI, which is attributed to a synergistic combination of factors induced by LSPwC, including high-amplitude compressive residual stresses, elevated microhardness, grain refinement, and carbon diffusion. This study contributes valuable insights into the reinforcement of complex cast components.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Surface Treatment and Residual Stress · Metal Alloys Wear and Properties · Tribology and Wear Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (49)
Show source-provided references
1. Effects of quench-tempering and laser hardening treatment on wear resistance of gray cast iron10.1016/j.jmrt.2020.05.006 ↗
2. Fatigue strength optimization of gray cast iron processed by different austempering temperatures10.1016/j.ijfatigue.2023.107831 ↗
3. The effect of niobium addition on the microstructure and properties of cast iron used in cylinder head10.1016/j.jmrt.2019.11.076 ↗
4. Reliability study for diesel engine cylinder head through fatigue failure analysis and structural optimization10.1016/j.engfailanal.2022.106768 ↗
5. Investigations on electrochemical corrosion behavior of 7075 aluminum alloy with femtosecond laser modification10.1016/j.vacuum.2023.112911 ↗
6. Twin and dislocation induced grain subdivision and strengthening in laser shock peened Ti10.1016/j.ijplas.2022.103476 ↗
7. Laser shock peening induced surface nanocrystallization and martensite transformation in austenitic stainless steel10.1016/j.jallcom.2015.06.268 ↗
8. Microstructure and mechanical properties of composite strengthened high-chromium cast iron by laser quenching and laser shock peening10.1016/j.jmrt.2022.08.148 ↗
9. Fatigue behaviour of laser shock peened AISI D2 tool steel10.1016/j.ijfatigue.2022.107226 ↗
10. Microstructure and residual stress modulation of 7075 aluminum alloy for improving fatigue performance by laser shock peening10.1016/j.ijmachtools.2022.103979 ↗
11. Gradient microstructure and fatigue properties of TC21 titanium alloy processed by laser shock peening10.1016/j.jallcom.2022.168139 ↗
12. The effect of laser shock peening on the rotating bending fatigue resistance of S51740 stainless steel10.1007/s10853-024-09578-5 ↗
13. High energy laser shock peening of Ti6Al4V alloy without any protective coating10.1016/j.apsusc.2023.158110 ↗
14. Wear resistance of AISI 5140 steel with Micro-laser shock peening10.1016/j.matlet.2023.134328 ↗
15. Quarter century development of laser peening without coating10.3390/met10010152 ↗
16. Influence of laser shock peening on surface characteristics and corrosion behavior of zirconium alloy10.1016/j.matchar.2023.113387 ↗
17. Optimization of residual stress field and improvement of fatigue properties of thin-walled pipes by filling laser shock peening10.3390/met12101733 ↗
18. Effect of laser shock peening without coating on fretting wear behavior of GH4169 superalloy at high-temperature
19. Mechanical properties and deformation dependent microstructural aspects of laser shock peened 7075-T6 aluminum alloy without coating10.1016/j.matchar.2021.111620 ↗
20. Effect of multiple laser shock peening without coating on residual stress distribution and high temperature dry sliding wear behaviour of Ti-6Al-4 V alloy10.1016/j.optlastec.2023.109398 ↗
21. Surface strengthening and fatigue life improvement of single crystal Ni-based superalloys via laser shock peening without coating10.1016/j.matdes.2023.112097 ↗
22. Remarkable near-surface microstructure of nanoparticles and oxide film in laser shock peened Al-Zn-Mg-Cu alloy10.1016/j.scriptamat.2021.114012 ↗
23. Plastic deformations of 42CrMo4 under LSPwC and subsequent cyclic stresses10.1016/j.ijmecsci.2023.108623 ↗
24. Maxwell
25. Unveiling the origins of work-hardening enhancement and mechanical instability in laser shock peened titanium10.1016/j.actamat.2022.117810 ↗
26. Simulation analyzing the influence of cutting HT250 by self-prepared Si3N4 insert at different feed rate10.1088/1757-899X/242/1/012042 ↗
27. Comparison of surface integrity of GH4169 superalloy after high-energy, low-energy, and femtosecond laser shock peening10.1016/j.vacuum.2022.111740 ↗
28. Enhanced fatigue strength of 2A02 aluminum alloy via micro laser shock peening10.1016/j.optlastec.2023.109675 ↗
29. Research on wear resistance of AISI 9310 steel with micro-laser shock peening10.3390/met12122157 ↗
30. Rolling contact fatigue and damage characteristic of AISI 9310 steel with pre-laser shock peening treatment10.1016/j.ijfatigue.2021.106588 ↗
31. Improvement of strength-ductility synergy of Mg–Al–Mn alloy using laser shock peening-induced gradient nanostructure10.1016/j.msea.2023.144844 ↗
32. Warm laser shock peening without coating induced phase transformations and pinning effect on fatigue life of low-alloy steel10.1016/j.matdes.2016.06.026 ↗
33. Effect of dynamic recrystallization on texture orientation and grain refinement of Ti6Al4V titanium alloy subjected to laser shock peening10.1016/j.jallcom.2020.156672 ↗
34. Zhou · 2021 · vol. 314
35. Laser shock peening and its applications: a review10.1007/s40516-019-00098-8 ↗
36. Surface roughness influence in micromechanical fatigue lifetime prediction with crystal plasticity models for steel10.1016/j.ijfatigue.2022.106792 ↗
37. Mechanical properties and strengthening mechanisms of Ti-6Al-4V treated by electro-pulsing assisted laser shock peening10.1016/j.jmatprotec.2024.118316 ↗
38. Laser shock peening regulating residual stress for fatigue life extension of 30CrMnSiNi2A high-strength steel10.1016/j.optlastec.2023.110094 ↗
39. Gradient nanostructure, enhanced surface integrity and fatigue resistance of Ti-6Al-7Nb alloy processed by surface mechanical attrition treatment10.1016/j.jmst.2023.12.011 ↗
40. Improving fatigue initiation life of open-hole fibre metal laminates by laser shock peening10.1016/j.jmrt.2023.12.150 ↗
41. A benchmark study on casting residual stress10.1007/s11661-011-0907-5 ↗
42. Residual stresses in surface induction hardening of steels: comparison between experiment and simulation10.1016/j.msea.2007.10.047 ↗
43. Investigation on the effect of mold constraints and cooling rate on residual stress during the sand-casting process of 1086 steel by employing a thermomechanical model10.1007/s11663-013-0015-6 ↗
44. Fatigue performance improvement of laser shock peened hole on powder metallurgy Ni-based superalloy labyrinth disc10.1016/j.surfcoat.2021.126829 ↗
45. Microstructural evolution and tribological properties of TC6 titanium alloy strengthened by laser peening combined with nitrogen ion implantation10.1016/j.vacuum.2024.112964 ↗
46. Enhanced carbon diffusion efficiency and work hardening effect of AISI 9310 steel via pre-laser shock peening10.1016/j.surfcoat.2023.129932 ↗
47. Surface roughness of selective laser melted Ti-6Al-4V alloy components
48. Enhancing plain fatigue strength in aluminum alloys through shot peening: experimental investigations and a strain energy density interpretation10.1016/j.ijfatigue.2024.108299 ↗
49. The effect of nitriding, severe shot peening and their combination on the fatigue behavior and micro-structure of a low-alloy steel10.1016/j.ijfatigue.2013.04.017 ↗