journal article·2024-09Open access

Enhancing mechanical properties and corrosion resistance of Fe–Cr–B–Mo alloy via the 'Divide and Conquer' strategy for Ti regulation

Zicheng Ling, Wenguang Yang, Xingxing Wang, Xianman Zhang, Junyi Jiang, Zenglei Ni, Jin Peng, Zhipeng Yuan, Jianjun Shi, Weiping Chen

Abstract

The corrosion of molten aluminium on components in the aluminium industry poses a significant bottleneck, hindering the development of aluminium products and equipment. This study focused on the Fe–Cr–B–Mo alloy, addressing challenges related to the susceptibility of the matrix to corrosion, the excessive brittleness of M 2 B borides (M = Fe, Cr, etc.), and the detachment of corrosion products. A comprehensive study was performed to study the microstructure evolution, mechanical properties, and corrosion behavior of Fe–Cr–B–Mo alloy, considering the 'Divide and Conquer' strategy for Ti regulation. The findings indicate that the heterogeneous nucleation, induced by in situ TiB 2 particles, significantly impacts the refinement of M 2 B borides size and enhances the matrix strength. Notably, the addition of 4.5 wt. % Ti to the T3 alloy significantly enhances its mechanical properties and corrosion resistance. The T3 alloy exhibits an impact toughness of 32.4 kJ/m 2 and a compressive fracture strain of 19.5 %, representing a considerable increase of 58 % and 167 % over the Ti-free alloy, respectively. Furthermore, the alloy has a volume loss rate of 11.0 mm 3 cm −2 h −1 , which is substantially lower, by 73.5 % compared to H13 steel and by 21.4 % compared to the Ti-free alloy. The synergistic presence of TiB 2 and M 2 B borides, along with their corrosion products, functions as an effective diffusion barrier against molten aluminium corrosion.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced materials and composites · Metal Alloys Wear and Properties · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (40)

Show source-provided references
1. A study of advancement in application opportunities of aluminum metal matrix composites10.1016/j.matpr.2020.02.516 ↗
2. Characterisation of oxide films formed on Co–29Cr–6Mo alloy used in die-casting moulds for aluminium10.1016/j.corsci.2013.03.026 ↗
3. Corrosion mechanisms of steel and cast iron by molten aluminum10.1007/s11661-010-0306-3 ↗
4. Die soldering: mechanism of the interface reaction between molten aluminum alloy and tool steel10.1007/s11663-002-0057-7 ↗
5. Evaluation of soldering, washout and thermal fatigue resistance of advanced metal materials for aluminum die-casting dies10.1016/j.msea.2004.03.020 ↗
6. Investigation of erosive-corrosive wear in the low pressure die casting of aluminum A35610.1016/j.msea.2006.07.052 ↗
7. A new Fe-Cr-Mo-B-Al steel with outstanding tribo-corrosion resistance in liquid aluminium10.1016/j.corsci.2022.110484 ↗
8. Tribo-corrosion resistance of Ti-Nb-Cr-Mo-Al refractory high-entropy alloys in molten aluminum10.1016/j.corsci.2023.111521 ↗
9. Interfacial morphology and tribo-corrosion behaviour of Fe-15.3 wt % Cr-3.1 wt % B-6.2 wt % Mo alloy in molten aluminium10.1016/j.wear.2019.04.002 ↗
10. Intermetallic formation and its relation to interface mass loss and tribology in die casting dies10.1016/j.wear.2003.08.001 ↗
11. Interfacial reactions of solid Co and solid Fe with liquid Al10.1016/j.corsci.2012.04.015 ↗
12. Formation and growth of titanium aluminide layer at the surface of titanium sheets immersed in molten aluminum
13. Corrosion behaviour of a surface-treated AISI H11 hot work tool steel in molten aluminium alloy10.1016/S0257-8972(00)00530-2 ↗
14. Degradation of TiB2 ceramics in liquid aluminum10.1016/j.jeurceramsoc.2008.05.011 ↗
15. Interaction of molten aluminum with porous TiB2-based ceramics containing Ti–Fe Additives10.1016/j.jeurceramsoc.2011.10.053 ↗
16. Corrosion of CrN and CrN/TiN coated heat-resistant steels in molten A356 aluminum alloy10.1016/S0257-8972(01)01484-0 ↗
17. Effects of boron concentration on the corrosion resistance of Fe–B alloys immersed in 460 °C molten zinc bath10.1016/j.surfcoat.2009.12.010 ↗
18. Interfacial morphology and corrosion-wear behavior of cast Fe-3.5 wt % B steel in liquid zinc10.1016/j.corsci.2017.12.003 ↗
19. Multiscale corrosion-resistance mechanisms of novel ferrous alloys in dynamic aluminum melts10.1016/j.corsci.2019.108276 ↗
20. Influence of Cr on the interfacial boride reaction between Fe-Cr-B cast steel and molten aluminium10.1016/j.corsci.2019.108098 ↗
21. Microstructure and mechanical properties of a spark plasma sintered Fe-11Cr-2.3 B-6Al-15Mn alloy10.1016/j.vacuum.2018.01.029 ↗
22. Effects of chromium on the morphology and mechanical properties of Fe2B intermetallic in Fe-3.0 B alloy10.1007/s10853-017-1936-2 ↗
23. Enhancement of hardness, modulus and fracture toughness of the tetragonal (Fe, Cr)2B and orthorhombic (Cr, Fe)2B phases with addition of Cr10.1016/j.matdes.2018.06.040 ↗
24. Effects of hot rolling and titanium content on the microstructure and mechanical properties of high boron Fe–B alloys10.1016/j.matdes.2011.10.043 ↗
25. Effect of variable heat treatment modes on microstructures in Fe-Cr-B cast iron alloy
26. Effect of boron concentration on microstructures and properties of Fe–B–C alloy steel10.1557/jmr.2017.304 ↗
27. Microstructures, heat treatment, and properties of boron‐alloyed tool steels10.1002/srin.201900416 ↗
28. Influence of Ce on microstructure and properties of high-carbon high-boron steel10.1016/S1875-5372(15)30085-0 ↗
29. Effect of rare earth and titanium additions on the microstructures and properties of low carbon F-B cast steel10.1016/j.msea.2007.02.032 ↗
30. The influence of A Mo addition on the interfacial morphologies and corrosion resistances of novel Fe-Cr-B alloys immersed in molten aluminum10.3390/ma12020256 ↗
31. Interaction between liquid aluminium and non-oxide ceramics (AlN, Si3N4, SiC)10.4028/www.scientific.net/KEM.113.177 ↗
32. Interface structure and chemistry in a novel steel-based composite Fe–TiB2 obtained by eutectic solidification10.1016/j.actamat.2012.08.017 ↗
33. Effect of Fe content in Fe–Ti–B system on fabricating TiB2 particulate locally reinforced steel matrix composites10.1016/j.msea.2006.02.012 ↗
34. Microstructure refinement for high modulus in-situ metal matrix composite steels via controlled solidification of the system Fe–TiB210.1016/j.actamat.2015.06.017 ↗
35. A step towards designing Fe–Cr–B–C cast alloys10.1016/S0921-5093(00)01808-6 ↗
36. Boron-alloyed Fe–Cr–C–B tool steels—thermodynamic calculations and experimental validation10.1016/j.matdes.2015.08.157 ↗
37. Kinetics of heterogeneous nucleation10.1063/1.1747588 ↗
38. Phase equilibria in TiB2-reinforced high modulus steel10.1361/105497199770335730 ↗
39. Effect of the content of B4C on microstructural evolution and wear behaviors of the laser-clad coatings fabricated on Ti6Al4V10.1016/j.optlastec.2015.07.010 ↗
40. Interfacial morphologies and corrosion behaviours of novel Fe-Cr-B alloys immersed in molten aluminium10.1088/2053-1591/aafeb1 ↗