Improving fatigue life and toughness in electron beam welded Ti–6Al–4V achieved through beta heat treatment for microstructure uniformity
Source abstract
Abstract
Electron beam welding (EBW) offers significant production efficiency advantages for Ti alloys in aerospace applications. However, the formation of martensitic α' in the weld joint reduces toughness and fatigue properties, posing safety challenges. To address these issues, this study investigates the effects of annealing below the β transus temperature (mill annealing, MA) and above the β transus temperature (beta annealing, BA) on the microstructure and mechanical properties of EBWed Ti-6Al-4V (Ti64). EBW produced α' in both the fusion zone (FZ) and heat-affected zone due to rapid heating and cooling. MA transformed α' into an α+β basketweave structure, but did not eliminate microstructural gradients. Conversely, BA produced a homogenized microstructure across all regions, characterized by a transformed β phase with a coarse α+β basketweave structure dominantly oriented with prismatic plane. Both annealing processes reduced the amount of low-angle grain boundaries in the FZ compared to the EBWed condition. BA achieved superior mechanical improvements, including a 20 % increase in tensile toughness, a 56 % improvement in fatigue life, and a 100 % improvement in impact toughness. These enhancements are attributed to uniform strain distribution and enhanced fracture resistance facilitated by the basketweave structure. Therefore, this study suggests that BA is the obtimal heat treatment for Ti64 weld joint, significantly improving fatigue cycle and impact toughness, and is refommened for aerospace structural applications.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Welding Techniques and Residual Stresses · Titanium Alloys Microstructure and Properties · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Fatigue and anisotropic behavior of wire-arc additive manufactured TC17 titanium alloy10.1016/j.jmrt.2023.12.214 ↗
2. Introduction to titanium and its alloys
3. Boyer · 1994
4. Inagaki · 2014 · vol. 106 · 22
5. Technologies for process design of titanium alloy forging for aircraft parts
6. Light-weight structures produced by laser beam joining for future applications in automobile and aerospace industry10.1016/S0924-0136(01)00756-7 ↗
7. Zavadski · 2018
8. Welding of titanium (Ti-6Al-4V) alloys: a review
9. Microstructure and mechanical properties in electron beam scanning welded joints of super thick titanium alloy plates10.1016/j.jmrt.2024.08.077 ↗
10. Effect of three-stage heat treatment on mechanical properties and micro-deformation mechanism of TC4 titanium alloy welded joint
11. Electron beam welding, laser beam welding and gas tungsten arc welding of titanium sheet10.1016/S0921-5093(99)00662-0 ↗
12. The effect of constraint conditions on microstructure and properties of titanium alloy electron beam welding10.1016/j.msea.2018.02.069 ↗
13. Fatigue behaviour of additive manufactured Ti6Al-4V, with as-built surfaces, exposed to variable amplitude loading10.1016/j.ijfatigue.2017.06.023 ↗
14. Static structural analysis of fighter aircraft's spars
15. Lütjering · 2007 · 203
16. Dynamic strength and failure behavior of titanium alloy Ti-6Al-4V for a variation of heat treatments10.1007/s11043-008-9060-y ↗
17. Improved mechanical properties of Ti–6Al–4V alloy by electron beam welding process plus annealing treatments and its microstructural evolution10.1016/j.matdes.2014.04.037 ↗
18. Effect of beam oscillation on fatigue life of Ti–6Al–4V electron beam weldments10.1016/j.msea.2007.03.040 ↗
19. Effect of postweld heat treatment on microstructure, hardness, and tensile properties of laser-welded Ti-6Al-4V10.1007/s11661-012-1230-5 ↗
20. Microstructures and mechanical properties of a titanium alloy thick plate joint after electron beam welding plus solution-aging10.1016/j.jmrt.2022.05.091 ↗
21. Microstructure and mechanical properties of Ti6Al4V alloy electron beam weldment at varying heat treatment conditions10.1007/s12666-020-01981-1 ↗
22. Effect of heat treatment on microstructures and properties of vacuum laser welding Ti6Al–4V titanium alloy10.1016/j.jmrt.2024.04.265 ↗
23. Enhancing the mechanical properties of electron beam welded TC17 titanium alloy joint by post-weld heat treatment10.1016/j.jallcom.2019.151937 ↗
24. Enhancement of fatigue resistance by direct aging treatment in electron beam welded Ti–5Al–2Sn–2Zr–4Mo–4Cr alloy joint10.1016/j.msea.2021.142168 ↗
25. Effect of microstructure transformations on fatigue properties of laser beam welded Ti-6Al-4V butt joints subjected to postweld heat treatment
26. Annealing heat treatment for homogenizing the microstructure and mechanical properties of electron-beam-welded thick plate of Ti-6Al-4V alloy10.3390/ma16237423 ↗
27. Titanium alloy bars, wire, forgings, rings, and drawn shapes 6Al-4V annealed. AMS 4928W
28. Titanium alloy damage tolerant grade plate 6Al-4V beta annealed. AMS 4905F
29. Temperature-gradient induced microstructure evolution in heat-affected zone of electron beam welded Ti-6Al-4V titanium alloy10.1016/j.jmst.2019.04.004 ↗
30. Fatigue life evaluation of Ti–6Al–4V welded joints manufactured by electron beam melting10.1111/ffe.13490 ↗
31. Effect of heat treatments on tensile fracture behaviour of Ti-6Al-4V alloy friction welds
32. Influence of heat treatments on microstructural and mechanical properties of Grade 5 titanium friction welds
33. Temperature-gradient induced microstructure evolution in heat-affected zone of electron beam welded Ti-6Al-4V titanium alloy10.1016/j.jmst.2019.04.004 ↗
34. Inverse Pole figures and the anisotropy of the properties of HCP alloys10.1134/S0036029522040048 ↗
35. Preferred orientation relationship of intra- and inter-granular precipitates in titanium alloys10.1016/S0921-5093(01)01829-9 ↗
36. β grain evolution and static recrystallization mechanism during hot rolling and annealing of Ti-35421 titanium alloy10.1007/s11665-022-06977-0 ↗
37. Changes in misorientations of grain boundaries in titanium during deformation10.1016/j.matchar.2010.04.005 ↗
38. Effect of multidirectional isothermal forging on microstructure and mechanical properties in Ti-6Al-4V alloy10.3390/ma15093156 ↗
39. Abbaschian · 2024
40. Influence of microstructure on tensile properties and deformation mechanism of Ti-5Al-1V-1Sn-1Zr-0.8Mo alloy: bimodal versus basketweave structures10.1007/s11665-023-07846-0 ↗
41. Effect of content and configuration of equiaxed α and lamellar α on deformation mechanism and tensile properties of a near-α titanium alloy10.1016/j.msea.2023.145192 ↗
42. Comparative research on fatigue performance of high-strength Bainitic steel with or without corrosion10.1007/s11665-020-05207-9 ↗
43. Grain boundary characterization and its influence on fatigue crack initiation and propagation in Ti-15-3 sheet
44. Grain boundary effects on cyclic deformation and fatigue damage10.1016/j.pmatsci.2008.06.001 ↗
45. Effect of linear friction welding process on microstructure evolution, mechanical properties and corrosion behavior of GH4169 superalloy10.1016/j.cja.2024.03.039 ↗
46. Strengthening mechanism and forming control of linear friction welded GH4169 alloy joints10.1016/j.cja.2024.01.026 ↗