Phase constitution, microstructure and corrosion performance of binary Sn–Bi alloys
Source abstract
Abstract
In the present paper, the phase constitution, microstructure, and corrosion behavior of a series of binary Sn–xBi alloys (x = 40, 57 and 80 wt.%) have been studied. The materials were prepared by induction melting of high purity Bi and Sn lumps in argon. Subsequently, the alloys were rapidly solidified to form cast ingots. The as-cast Sn-57Bi alloy had a near-eutectic microstructure. The as-cast Sn–40Bi alloy consisted of dendritic Sn(ss) and eutectic grains, while the as-cast Sn–80Bi alloy consisted of dendritic Bi(ss) and eutectic. The corrosion behavior of the alloys was studied by open circuit potential measurements (OCP) and linear sweep voltammetry in an aqueous NaCl solution (1 wt.%). The experiments were carried out at room temperature in a three-electrode cell controlled by a potentiostat. The results were compared with those for pure Sn and Bi. The open circuit potentials of the Sn-Bi alloys increased in the following order: Sn<Sn-80Bi<Sn-40Bi<Sn-57Bi<Bi. The corrosion currents of the hypoeutectic Sn-40Bi and hypereutectic Sn-80Bi alloys were found to be higher compared to Sn-57Bi alloy. These results indicate that the near-eutectic Sn-57Bi alloy has a higher corrosion resistance compared to the Sn-80Bi and Sn-40Bi alloys. The corrosion behavior of the binary Sn-Bi alloys was found to take place by a galvanic mechanism. The eutectic regions in the alloys were preferentially attacked. Corrosion products on the alloy surfaces were identified using a combination of SEM/EDS and room-temperature XRD. The results are compared with those of previously studied Sn-Bi alloys. The corrosion mechanism is discussed.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · Aluminum Alloy Microstructure Properties · Metallurgical Processes and Thermodynamics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. High entropy alloys as filler metals for joining10.3390/e23010078 ↗
2. Development of lead-free interconnection materials in electronic industry during the past decades: Structure and properties
3. A review of lead-free solders for electronics applications10.1016/j.microrel.2017.06.016 ↗
4. Recent progress on the development of Sn–Bi based low-temperature Pb-free solders10.1007/s10854-019-00701-w ↗
5. Recent advances on SnBi low-temperature solder for electronic interconnections10.1007/s10854-021-06820-7 ↗
6. Microstructure and corrosion behavior of Sn–Zn alloys10.3390/ma15207210 ↗
7. Interfacial reaction and mechanical properties of Sn-Bi solder joints10.3390/ma10080920 ↗
8. Characterization of eutectic Sn-Bi solder joints10.1007/BF02655427 ↗
9. Microstructure evolution in Sn-Bi and Sn-Bi-Cu solder joints under thermal aging10.1016/S0254-0584(01)00298-X ↗
10. Microstructural development and mechanical properties of a near-eutectic directionally solidified Sn-Bi solder alloy10.1016/j.matchar.2015.06.026 ↗
11. Low melting point solders based on Sn, Bi, and in elements
12. Microstructure and mechanical properties of Pb-free solder alloys for low-cost electronic assembly: a review10.1007/BF02651361 ↗
13. Microstructure and mechanical properties of Sn-Bi, Sn-Ag and Sn-Zn lead-free solder alloys10.1016/j.jallcom.2013.03.234 ↗
14. Low melting temperature sn-bi solder: effect of alloying and nanoparticle addition on the microstructural, thermal, interfacial bonding, and mechanical characteristics10.3390/met11020364 ↗
15. Effects of trace amounts of rare earth additions on microstructure and properties of Sn-Bi-based solder alloy10.1007/s11664-008-0458-8 ↗
16. Microstructure of ternary Sn-Bi-xCu alloy on mechanical properties, current endurance and corrosion morphology via cycling corrosion test
17. Effects of alloying element on mechanical properties of Sn-Bi solder alloys: a review10.1108/SSMT-06-2021-0035 ↗
18. Alloying influences on low melt temperature SnZn and SnBi solder alloys for electronic interconnections10.1016/j.jallcom.2016.01.006 ↗
19. The effect of aging on microstructure, room temperature deformation, and fracture of Sn-Bi/Cu solder joints10.1007/BF02653346 ↗
20. Presentation of an Atlas of chemical and electrochemical equilibria in the presence of a gaseous phase10.4028/www.scientific.net/MSF.251-254.143 ↗
21. Electrochemical series
22. Comparative corrosion behaviour of different Sn-based solder alloys10.1007/s10854-014-2422-0 ↗
23. Microstructures of ternary Sn-Bi-xZn alloys on mechanical and electrochemical properties analysis for connection packaging
24. Immersion corrosion of Sn-Ag and Sn-Bi alloys as successors to Sn-Pb alloy with electronic and jewelry applications10.5006/2039 ↗
25. Effect of Bi content on microstructure and corrosion behaviour of Zn–8Al–(Bi) alloys10.1080/1478422X.2021.1916235 ↗
26. et Interf acia
27. Lu · 2024 · 1
28. Influence of electrochemical properties on electrochemical migration of SnPb and SnBi solders10.1007/s12540-010-1007-6 ↗
29. The effects of chloride and sulphate ions on the electrochemical behaviour of tin in aqueous solutions10.4152/pea.201801011 ↗
30. Electrochemical corrosion behaviour of Bi-11Ag alloy for electronic packaging applications10.1016/j.corsci.2010.03.031 ↗
31. Effect of bismuth and silver on the corrosion behavior of lead-free solders in 3.5 wt% NaCl solution10.3311/PPee.9706 ↗
32. 2005 · vol. 2005
33. The influence of the potential sweep rate on the shape of polarization curves10.1016/S0010-938X(98)00076-6 ↗
34. The influence of the potential sweep rate on the computation of the polarization resistance10.1016/S0010-938X(96)00064-9 ↗
35. McCafferty · 2010
36. Pitting corrosion10.1007/978-3-319-97625-9_11 ↗
37. Popov · 2015
38. Properties of ternary Sn-Ag-Bi solder alloys: Part I - thermal properties and microstructural analysis10.1007/s11664-999-0250-4 ↗
39. Popov · 2015
40. Effect and mechanism of bismuth doped lead oxide on the performance of lead-acid batteries10.1016/S0378-7753(00)00640-6 ↗
41. Id A., Seience M. Ko 2004;11(4). https://doi.org/10.1007/s11771-004-0085-3.10.1007/s11771-004-0085-3 ↗
42. Bismuth as a new chloride-storage electrode enabling the construction of a practical high capacity desalination battery10.1021/jacs.7b01119 ↗