journal article·2025-03Open access

Investigation of the mechanisms affecting corrosion susceptibility of wrought aeronautical aluminium alloys Al–Cu–Li (AA2198) and Al–Cu–Mg (AA2024) for different pre-stretching levels

Christina Margarita Charalampidou, Christiaan C.E. Pretorius, Muhammed Salojee, Dionysios Karousos, Malika Khodja, Roelf J. Mostert, Nikolaos D. Alexopoulos

Abstract

Aluminium (Al) alloy sheets are usually stretched to manufacture aircraft structures with complex geometries. The corrosion susceptibility of AA2198 Al alloy is examined as a function of the extent of pre-stretching, using a wide range of advanced microscopy, electrochemical techniques, and tensile testing. Intergranular corrosion attack manifested in sub-surface secondary cracking for the 1.5 % pre-stretching level. A mechanism of deformation-induced chemical heterogeneity is believed to be responsible for the resulting intergranular corrosion, in which δ΄ -phase nucleation following pre-stretching allows for the removal of matrix Li within highly deformed grains, creating a micro-galvanic coupling between neighbouring grains. At pre-stretching levels of 4.0 % and higher, a transition to transgranular corrosion was observed, whilst the EBSD results indicated that recovery occurs at these pre-stretching levels. At 7.5. % pre-stretching level, the charge transfer resistance values were essentially increased due to the segregation of Li to sub-grain boundaries, allowing for more matrix Li removal and, hence, to the more rapid transgranular attack. On the contrary, the level of corrosion degradation of the tensile properties of AA2024-T3, although being more severe than that of the AA2198 alloy, is not essentially influenced by varying the extent of pre-stretching.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (88)

Show source-provided references
1. Recent developments in advanced aircraft aluminium alloys10.1016/j.matdes.2013.12.002 ↗
2. 2011
3. Recycling and life cycle issues for lightweight vehicles
4. The evolution of Al-Li base products for aerospace and space applications10.1007/s11661-012-1155-z ↗
5. Considerations regarding aluminum alloys used in the aeronautic/aerospace industry and use of wire arc additive manufacturing WAAM for their industrial applications
6. Quasi-static strength, deformation, and fracture behavior of aluminum-lithium alloys
7. Fatigue behavior of the aeronautical Al–Li (2198) aluminum alloy under constant amplitude loading10.1016/j.ijfatigue.2013.07.009 ↗
8. Mechanical properties degradation of (Al-Cu-Li) 2198 alloy due to corrosion exposure10.1016/j.prostr.2016.06.077 ↗
9. Effect of localized corrosion on fatigue–crack growth in 2524-T3 and 2198-t851 aluminum alloys used as aircraft materials10.1007/s11665-018-3244-7 ↗
10. Corrosion behavior of 2198 Al–Cu–Li alloy in different aging stages in 3.5 wt % NaCl aqueous solution
11. Corrosion and fatigue behavior of new Al alloys10.1016/j.proeng.2011.04.254 ↗
12. SVET, SKP and EIS study of the corrosion behaviour of high strength Al and Al–Li alloys used in aircraft fabrication10.1016/j.corsci.2014.03.001 ↗
13. Comparison of the corrosion resistance of an Al–Cu alloy and an Al–Cu–Li alloy10.1080/1478422X.2019.1605472 ↗
14. Exfoliation and intergranular corrosion resistance of the 2198 Al–Cu–Li alloy with different thermomechanical treatments
15. Effect of ageing time on strength and microstructures of an Al–Cu–Li–Zn–Mg–Mn–Zr alloy10.1016/j.msea.2008.08.001 ↗
16. Prasad · 2013
17. Strengthening mechanisms of T1 precipitates and their influence on the plasticity of an Al–Cu–Li alloy10.1016/j.msea.2014.03.024 ↗
18. Improved toughness in Al–Li–Cu–Mg–Ag–Zr alloy X209510.1016/0956-716X(92)90540-U ↗
19. Mechanical behavior of double-aged AA809010.1007/BF02656504 ↗
20. Microstructural development in Al_2 % Li_3 %Cu alloy
21. The effect of precipitate shape and orientation on dispersion strengthening in high strength aluminium alloys10.4028/www.scientific.net/MSF.217-222.1257 ↗
22. Strengthening mechanisms, deformation behavior, and anisotropic mechanical properties of Al-Li alloys: a review10.1016/j.jare.2017.12.004 ↗
23. Effects of a small addition of magnesium and silver on the precipitation of T1 phase in an A1-4 %Cu-l.l %Li-0.2 % Zr alloy10.1016/0921-5093(95)10157-8 ↗
24. Microstructural evolution during ageing of Al–Cu–Li–x alloys10.1016/j.actamat.2013.12.001 ↗
25. Structure and deformation behavior of T1 precipitate plates in an Al- 2Li- 1 Cu alloy10.1007/BF02647717 ↗
26. On the form of the age-hardening response in high strength aluminium alloys10.1016/S0921-5093(01)01054-1 ↗
27. Corrosion of AA2024-T3 Part I: localised corrosion of isolated IM particles10.1016/j.corsci.2010.09.009 ↗
28. Localized corrosion of 2024-T351 aluminum alloy in chloride media10.1016/S0010-938X(98)00116-4 ↗
29. The role of precipitates enriched with copper on the susceptibility to pitting corrosion of the 2024 aluminum alloy10.1016/S0010-938X(97)86099-4 ↗
30. Localised corrosion in AA2099-T83 aluminium-lithium alloy: the role of grain orientation10.1016/j.corsci.2016.02.018 ↗
31. Crystallographic defects induced localised corrosion in AA2099-T8 aluminium alloy10.1179/1743278214Y.0000000237 ↗
32. Effects of Li content on precipitation in Al–Cu–(Li)–Mg–Ag–Zr alloys10.1016/S1359-6462(97)00503-4 ↗
33. The influence of Cu/Li ratio on precipitation in Al–Cu–Li–x alloys10.1016/j.actamat.2012.12.041 ↗
34. Effect of precipitates on mechanical properties of AA219510.1016/j.jallcom.2016.01.229 ↗
35. The influence of artificial ageing on the corrosion behaviour of a 2050 aluminium-copper-lithium alloy10.1016/j.corsci.2013.11.060 ↗
36. Influence of chloride ions concentration on the development of severe localised corrosion and its effects on the electrochemical response of the 2198-T8 alloy10.1080/1478422X.2020.1862390 ↗
37. Microstructural, electrochemical and localized corrosion characterization of the aa2198-t851 alloy10.1590/1980-5373-mr-2020-0161 ↗
38. Aerospace applications of aluminum–lithium alloys
39. Hot stamping of high-strength aluminium alloy aircraft parts using quick heating10.1016/j.cirp.2017.04.117 ↗
40. Martin · 1998
41. The role of plastic deformation on the competitive microstructural evolution and mechanical properties of a novel Al-Li-Cu-X alloy10.1016/S1471-5317(00)00002-X ↗
42. The effect of plastic deformation on Al2CuLi (T1) precipitation10.1007/BF02656799 ↗
43. Effects of cold work on precipitation in Al-Cu-Mg-(Ag) and Al-Cu-Li-(Mg-Ag) alloys10.1007/BF02670753 ↗
44. Effect of pre-deformation on the microstructures and properties of 2219 aluminum alloy during aging treatment10.1016/j.jallcom.2016.12.006 ↗
45. Effect of pre-deformation on microstructure and mechanical properties of WE43 magnesium alloy10.1016/j.msea.2017.02.082 ↗
46. Influence of pre-deformation and subsequent ageing on the hardening behavior and microstructure of 2219 aluminum alloy forgings10.1016/j.jallcom.2016.06.111 ↗
47. Quantification of the influence of increased pre-stretching on microstructure-strength relationships in the Al-Cu-Li alloy AA219510.1016/j.actamat.2016.02.017 ↗
48. Correlation between localized plastic deformation and localized corrosion in AA2099 aluminum-lithium alloy10.1002/sia.5817 ↗
49. Crystallographic defects induced localised corrosion in AA2099-T8 aluminium alloy10.1179/1743278214Y.0000000237 ↗
50. The influence of stored energy on grain boundary chemistry and intergranular corrosion development in AA2024-T3 alloy10.3390/ma11112299 ↗
51. Intergranular corrosion in AA2024-T3 aluminium alloy: the influence of stored energy and prediction10.1016/j.corsci.2019.04.031 ↗
52. Effect of pre-deformation and artificial aging on fatigue life of 2198 Al-Li alloy
53. Effects of pre-stretching and aging treatments on microstructure, mechanical properties, and corrosion behavior of spray-formed Al-Li alloy 219510.1007/s11665-020-05142-9 ↗
54. ASTM B918, Aluminium alloy nomenclature and temper designations.
55. The effect of solution aggressiveness on the corrosion-induced degradation mechanism of Al-Cu-Li 2198 alloy10.1016/j.tafmec.2023.104241 ↗
56. 2009
57. 1999
58. 2001
59. Sprowls · 1972 · vol. 516
60. Mechanical properties degradation of (Al-Cu-Li) 2198 alloy due to corrosion exposure10.1016/j.prostr.2016.06.077 ↗
61. The effect of solution aggressiveness on corrosion-induced mechanical properties degradation of aeronautical aluminum alloy 219810.1016/j.prostr.2022.12.215 ↗
62. The effect of artificial ageing heat treatments on the corrosion-induced hydrogen embrittlement of 2024 (Al–Cu) aluminium alloy10.1016/j.corsci.2015.10.034 ↗
63. Covino · 2003 · 13A · 419
64. Effect of varying conditions of exposure to an aggressive medium on the corrosion behavior of the 2050 Al–Cu–Li alloy10.1016/j.corsci.2014.04.042 ↗
65. Engler · 2010
66. Chapter 5: texture and its effects on properties in aluminum À lithium alloys
67. 2010
68. Strain amount dependent grain size and orientation developments during hot compression of a polycrystalline nickel based superalloy10.3390/ma10020161 ↗
69. Texture formation in metal alloys with cubic crystal structures10.1080/02670836.2016.1231746 ↗
70. Thermomechanical treatment and corrosion resistance correlation in the AA2198 Al-Cu-Li alloy10.1080/1478422X.2019.1637077 ↗
71. 2014 · 457
72. A review of dynamic recrystallization phenomena in metallic materials10.1016/j.matdes.2016.09.012 ↗
73. Recovery and recrystallisation: phenomenon, physics, models, simulations
74. Influence of strain path dependent microstructural evolution on corrosion behaviour in Al-Li alloy10.1016/j.matlet.2023.134608 ↗
75. Microstructure evolution and precipitation characteristics of spray-formed and subsequently extruded 2195 Al-Li alloy plate during solution and aging process10.1016/j.jmatprotec.2020.116718 ↗
76. Dispersion of impedances at solid electrodes
77. Characterization of AA2024-T3 by scanning kelvin probe force microscopy10.1149/1.1838633 ↗
78. Corrosion inhibition of 2024-T3 aluminum alloy in 3.5 % NaCl by thiosemicarbazone derivatives10.1016/j.corsci.2018.03.021 ↗
79. High effective organic corrosion inhibitors for 2024 aluminum alloy10.1016/j.electacta.2007.05.058 ↗
80. The importance of phase composition for corrosion resistance of borided layers produced on nickel alloys10.3390/ma13225131 ↗
81. The passive film characteristics of several plastic deformation 2099 Al-Li alloy10.1016/j.jallcom.2015.12.051 ↗
82. Lüders strain of the fine-grained material under the electric current10.1016/j.msea.2021.141924 ↗
83. Effect of solution aggressiveness on the crack growth resistance and cracking mechanism of AA2024-T310.5006/3839 ↗
84. Quantitative effects of pre-deformation prior to non-isothermal aging on the mechanical properties-microstructure relationships in an Al-3.5Cu-1.01Li alloy10.1016/j.matdes.2022.111137 ↗
85. Liquid metal induced embrittlement in corrosion: fundamentals, testing, and protection
86. Stress-corrosion cracking in corrosion: fundamentals, testing, and protection
87. Ageing response of Al-Cu-Li 2198 alloy10.1016/j.matdes.2014.04.063 ↗
88. Heterogeneous nucleation and growth of δ’ in Al-8 at % Li10.1016/0956-7151(92)90127-Z ↗