journal article·2025-11Open access

Effect of variations in peak and background currents during pulsed current gas tungsten arc welding on the dissimilar welded joint of ASTM A105-AISI 316L: Microstructural changes, mechanical properties and fracture mechanism

M. Sabzi, H.R. Jafarian, A. Abdollahzadeh, S.H. Mousavi Anijdan, A.R. Eivani

Abstract

Abstract The aim of this study was to investigate the effect of variations in peak (I p ) and background (I b ) currents during Pulsed Current Gas Tungsten Arc Welding (PCGTAW) on microstructural changes, significant improvement of mechanical properties and fracture mechanism of dissimilar welded joints of ASTM A105-AISI 316L. For this purpose, 12 mm thick AISI 316L stainless steel sheets and ASTM A105 steel sheets were welded together by PCGTAW process with I p values of 180, 220 and 260A, and I b values of 70, 110 and 150A. Optical microscopy, Field Emission Scanning Electron Microscopy (FE-SEM), Energy-Dispersive X-Ray Spectroscopy (EDS), and X-Ray Diffraction (XRD) were used to analysisthe microstructural and phase changes. Similarly, tensile, Vickers microhardness and Charpy impact tests were utilizedto evaluate the effect of changes in I b and I p currents on mechanical properties. The fracture mechanism after tensile and Charpy impact tests was investigated by FE-SEM. Microscopic studies indicated that the microstructure of the weld metal (WM) contained austenite dendrites with a small amount of grain boundary delta ferrite, to the extent that with increasing I b and decreasing I p , the microstructure of the WM was changed from columnar dendrites to extremely small and coaxial dendrites. Likewise, the increased I b and decreased I p reduced the size of dendrites as well as the amount of grain boundary delta ferrite in WM and sodidthe width of the heat-affected zone (HAZ) and partial melted zone (PMZ). The results of XRD analysis indicate the predominance of the austenite phasein WM. In the tensile test, all welded joints were fractured from the ASTM A105 steel side. The welded joints built up yield strength of approximately 250 ± 8 MPa, a tensile strength of around 484 ± 9 MPa, and a fracture strain close to 30 ± 2 %.The results of Charpy impact and microhardness tests showed that with increasing I b and decreasing I p , the hardness (from 250 ± 5 HV to 289 ± 4 HV) and fracture energy (from 140 ± 3 J to 173 ± 3 J) of WM are increased. Fractography of the fracture surfaces indicates the occurrence of fully ductile fracture in both tensile and Charpy impact tests.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Welding Techniques and Residual Stresses · Hydrogen embrittlement and corrosion behaviors in metals · Engineering and Environmental Studies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (50)

Show source-provided references
1. Experiments on dynamic mechanical properties of austenitic stainless steel S30408 and S3160810.1016/j.jcsr.2021.106556 ↗
2. Microstructural evolution of a 304-type austenitic stainless steel during rolling at temperatures of 773–1273 K10.1016/j.actamat.2014.09.023 ↗
3. About metastable cellular structure in additively manufactured austenitic stainless steels
4. Was · 2019 · 293
5. Deformation-induced martensite in austenitic stainless steels: a review10.1007/s43452-020-00130-1 ↗
6. Effects of welding technique, filler metal and post-weld heat treatment on stainless steel and mild steel dissimilar welding joint10.1016/j.jmapro.2021.02.058 ↗
7. Effect of selective laser melting (SLM) process parameters on microstructure and mechanical properties of 316L austenitic stainless steel10.1016/j.jmatprotec.2017.05.042 ↗
8. Research status of welding technology of ferritic stainless steel10.1007/s00170-021-08128-6 ↗
9. Effects of heat treatment on microstructure, mechanical and corrosion properties of 15-5 PH stainless steel parts built by selective laser melting process10.1016/j.jmapro.2019.12.048 ↗
10. On the role of molybdenum on the microstructural, mechanical and corrosion properties of the GTAW AISI 316 stainless steel welds10.1016/j.jmrt.2021.05.095 ↗
11. Influence of different frequency pulse on weld bead phase ratio in gas tungsten arc welding by ferritic stainless steel AISI-409L10.1155/2022/9530499 ↗
12. Influence of PC-GTAW parameters on the microstructural and mechanical properties of thin AISI 1008 steel joints10.1007/s11665-016-2211-4 ↗
13. Improvement of penetration ability of heat source for 316 stainless steel welds produced by alternating magnetic field assisted laser-MIG hybrid welding10.1016/j.jmatprotec.2021.117329 ↗
14. Lippold · 2005 · 1
15. Aging constants for efficient fracture toughness prediction of thermally aged GTAW/SMAW of 316L stainless steel10.1016/j.ijpvp.2022.104632 ↗
16. Welding of fully –Austenitic stainless steel using pcgtaw process; part I: bead structure10.1016/j.jmapro.2018.12.037 ↗
17. Optimization of PC-GTAW orbital welding parameters of AISI 304L stainless steel pipe using ANOVA and taguchi method
18. Thermal field and residual stress analyses of similar and dissimilar weldments joined by constant and pulsed current TIG welding techniques10.1080/2374068X.2021.1959114 ↗
19. An experimental and numerical evaluation of steel A105 friction coefficient using different lubricants at high temperature10.1080/10402004.2021.1966147 ↗
20. Failure analysis of welded steam boiler flange10.21608/ijmti.2023.204369.1083 ↗
21. Effect of fillers and autogenous welding on dissimilar welded 316L austenitic and 430 ferritic stainless steels10.1007/s11665-020-05395-4 ↗
22. Dissimilar welding of duplex stainless steel with Ni alloys: a review
23. A-TIG welding of dissimilar P92 steel and 304H austenitic stainless steel: mechanisms, microstructure and mechanical properties10.1016/j.jmapro.2019.06.003 ↗
24. Effect of buffer-layered buttering on microstructure and mechanical properties of dissimilar metal weld joints for nuclear plant application10.1016/j.msea.2016.04.053 ↗
25. Microstructure, tensile property and corrosion performance of GTAW 316 L/Q345 under compound-magnetic field10.1016/j.jcsr.2025.109468 ↗
26. Microstructure and mechanical behavior study of the GTAW joint of AISI 310 and modified 9Cr-1Mo (P91) steel10.1007/978-981-96-3821-5 ↗
27. An experimental investigation on the effect of gas tungsten arc welding current modes upon the microstructure, mechanical, and fractography properties of welded joints of two grades of AISI 316L and AISI310S alloy metal sheets10.1016/j.msea.2022.142877 ↗
28. Investigation on effects of flux assisted GTAW welding process on mechanical, metallurgical characteristics of dissimilar metals SS 304 and SS 316 L10.1016/j.matpr.2020.04.143 ↗
29. Microstructure and mechanical properties of active gas arc welding between 304 austenitic stainless steel and Q235B low carbon steel10.1007/s11665-022-06808-2 ↗
30. Effect of heat input on geometry of austenitic stainless steel weld bead on low carbon steel
31. Sour corrosion performance and sensitivity to hydrogen induced cracking in the X70 pipeline steel: effect of microstructural variation and pearlite percentage
32. Effects of different cooling rates on the microstructure, crystallographic features, and hydrogen induced cracking of API X80 pipeline steel10.1016/j.jmrt.2021.07.060 ↗
33. The effect of pulse current changes in PCGTAW on microstructural evolution, drastic improvement in mechanical properties, and fracture mode of dissimilar welded joint of AISI 316L-AISI 310S stainless steels10.1016/j.msea.2021.141700 ↗
34. Metallurgical, mechanical and corrosion behaviour of pulsed and constant current TIG dissimilar welds of AISI 430 and inconel 71810.1016/j.jmrt.2023.04.231 ↗
35. Microstructural and mechanical characterization of welded joints between stainless steel and hastelloy made using pulsed current gas tungsten arc welding10.1007/s11665-022-07197-2 ↗
36. Effects of types of GTAW including superior GTAW-PC with superimposed HF current on mechanical and metallurgical properties of super duplex stainless steel weld joints
37. Drastic improvement in mechanical properties and weldability of 316L stainless steel weld joints by using electromagnetic vibration during GTAW process10.1016/j.jmapro.2018.05.002 ↗
38. Distinct properties of tungsten austenitic stainless alloy as a potential nuclear engineering material10.1016/j.net.2018.12.021 ↗
39. Structural, compositional, and mechanical characterization of WxCryFe1−x−y layers relevant to nuclear fusion, obtained with TVA technology10.3390/ma12244072 ↗
40. Comparing the effect of continuous and pulsed current in the GTAW process of AISI 316L stainless steel welded joint: microstructural evolution, phase equilibrium, mechanical properties and fracture mode10.1016/j.jmrt.2021.07.154 ↗
41. On the performance of weld overlay characteristics of Ni–Cr–Si–B deposition on 304 ASS using synergetic pulse-GMAW process10.1080/13621718.2020.1846935 ↗
42. The effects of filler metal and butter layer on the microstructure and mechanical properties of API 5L X65/AISI 304L joint10.1016/j.jmrt.2023.02.063 ↗
43. Hadfield manganese austenitic steel: a review of manufacturing processes and properties10.1088/2053-1591/ab3ee3 ↗
44. Dynamic strain aging mechanisms in a metastable austenitic stainless steel10.1016/j.actamat.2021.116888 ↗
45. Effect of grain size on mechanical characteristics and work-hardening behavior of fine-grained Mg-0.8Mn alloy via adjusting extrusion temperature
46. The influence of austenitization temperature on microstructural developments, mechanical properties, fracture mode and wear mechanism of hadfield high manganese steel10.1016/j.jmrt.2020.12.003 ↗
47. Regulating microstructure and mechanical properties of the as-cast Mg-4Zn-0.5Y-0.5Nd alloy by heat treatment
48. Post weld heat treatment of hypereutectoid hadfield steel: characterization and control of microstructure, phase equilibrium, mechanical properties and fracture mode of welding joint10.1016/j.jmapro.2018.06.009 ↗
49. Welding of additively and conventionally manufactured 316L stainless steel
50. Effect of creep fracture mode transition of P91 steel welded joints on long-term creep fracture life10.1016/j.jmrt.2024.10.214 ↗