Influences of deoxidation and VOD slag on the behavior of inclusions in Fe–21Cr ferrite stainless steel
Source abstract
Abstract
The influences of deoxidation process and VOD slag compositions on the behavior of inclusions during refining of Ti–Nb bearing Fe–21%Cr ferrite stainless steels were studied in the present work. The results indicated that the main oxide inclusions by the Al–Si complex deoxidization were MgO·Al2O3. And the main inclusions after Ti addition were MgO·Al2O3–TiOx and Al2O3–TiN complex inclusions. After calcium treatment, the main inclusions became spherical MgO·Al2O3–CaO and Al2O3–SiO2–CaO combined with TiOx and TiN. As the basicity of refining slag was increased from 2.5 to 4.0, the number density of inclusions in the steel reduced, while the average particle size of inclusions increased. When the basicity of CaO–SiO2–(15–20%) Al2O3–10%MgO–5%CaF2 refining slag was 3.5, the number of large inclusions would decrease with the deceasing of the Al2O3 content in the refining slag, and the amount of inclusions in molten steel decreased and the size of most inclusions was distributed within 1–2 μm.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metallurgical Processes and Thermodynamics · High-Temperature Coating Behaviors · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Ultra-pure ferritic stainless steels-grade, refining operation, and application10.1016/S1006-706X(07)60053-3 ↗
2. Mechanisms of solidification structure improvement of ultra pure 17 wt% Cr ferritic stainless steel by Ti, Nb addition10.1016/S1005-0302(11)60073-X ↗
3. Effect of Nb on high-temperature properties for ferritic stainless steel10.1016/1359-6462(96)00214-X ↗
4. Effects of addition of Nb and Ti on solidification structure and surface ridging of an ultra purified ferritic stainless steel
5. Improvements of solidification structure of 430 ferritic stainless steel treated by titanium elements
6. Inclusion control of ultra clean ferritic stainless steel
7. Formation behavior of Ti-based inclusions in nitrogen-containing steel10.2355/tetsutohagane.100.548 ↗
8. Size distribution of multi-phase deoxidation particles for heterogeneous crystallization of TiN and solidification structure in Ti-added ferritic stainless steel10.2355/isijinternational.52.1196 ↗
9. Inclusion control of ferritic stainless steel by aluminum deoxidation and calcium treatment10.1007/s11663-005-0007-2 ↗
10. Modification and minimization of spinel(Al2O3·xMgO) inclusions formed in Ti-added steel melts10.1007/s11663-010-9377-1 ↗
11. Influence of refining slag on the inclusions in sus444 ferrite stainless steel
12. The silicon-aluminum deoxidation and calcium treatment of titanium bearing ultra-pure ferritic stainless steel
13. An experiment study on silicon-aluminum complex deoxidation of titanium bearing ultra-pure ferritic stainless steel
14. Computer applications of thermodynamic databases to inclusion engineering10.2355/isijinternational.44.527 ↗
15. The nitrogen solubility in molten stainless steel10.1002/srin.200506090 ↗
16. Gaye. Thermodynamics of the formation of MgO-Al2O3-TiOx inclusions in Ti-Stabilized 11Cr ferritic stainless steel10.1007/s11663-008-9172-4 ↗
17. Argon. Beijing: Standardization Administration of the People's Republic of China, GB/T4842-2017.
18. Evolution mechanism of oxide inclusions in titanium-stabilized AISI 443 stainless steel10.1007/s11663-018-1331-7 ↗
19. Inclusion evolution after calcium addition in Ti-bearing Al-kill steel10.1080/03019233.2016.1251749 ↗
20. Control of MgO·Al2O3 spinel inclusions in stainless steels10.2355/isijinternational.50.1333 ↗
21. Formation of MgO·Al2O3 Inclusions in high strength alloyed structural steel refined by CaO-SiO2-Al2O3-MgO slag10.2355/isijinternational.48.885 ↗
22. Inclusions in stainless steels − A Review10.1002/srin.201700130 ↗
23. Formation, evolution and removal of MgO·Al2O3 spinel inclusions in steel10.2355/isijinternational.ISIJINT-2020-352 ↗
24. Modification of MgO·Al2O3 spinel inclusions in Al-killed steel by Ca-treatment10.1007/s12613-011-0394-0 ↗
25. Evolution mechanism of inclusions in Al-killed, Ti-bearing 11Cr stainless steel with Ca treatment10.2355/isijinternational.ISIJINT-2017-565 ↗
26. Effect of CaO-Al2O3-MgO slags on the formation of MgO-Al2O3 inclusions in ferritic stainless steel10.1007/s11663-005-0041-0 ↗