Nanostructure modification of titanium alloy to achieve ultra-high interfacial bond strength between titanium alloy and polyphenylene sulfide
Source abstract
Abstract
Metal-polymer composite components are widely used in aerospace, automotive, and other industries as lightweight composite parts that can result in significant weight savings. Injection-molded direct joining (IMDJ) technology has a broad application prospect for achieving a close connection between metal and polymer without destroying the metal matrix. This study subjected the titanium alloy surface to sandblasting, anodizing, etching, and annealing, resulting in uniformly distributed claw-like nanostructures generated on the surface. This treatment also improved the surface roughness, exhibiting excellent wettability with a contact angle of only 10.7°. The injection-molded direct joining technique was employed to join Ti alloy and polyphenylene sulfide (PPS) composite components. Tensile testing revealed a bond strength of 33.5 MPa, and analysis of the peeled specimens' residual elements indicated that failure of the composite components occurred in the form of polymer cohesion damage, showcasing excellent bonding effects.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Orthopaedic implants and arthroplasty · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. The fracture properties of a smart fiber metal laminate10.1002/pc.20319 ↗
2. Fracture properties of a fiber-metal laminates based on magnesium alloy10.1023/B:JMSC.0000012949.94672.77 ↗
3. Considerations for the industrial application of structural adhesive joints in the aluminium–composite material bonding10.1016/j.compositesb.2012.04.026 ↗
4. Experimental characterization of hybrid composite-to-metal bolted joints under flexural loading10.1016/j.compositesb.2006.03.013 ↗
5. Interlaminar fracture properties of surface treated Ti-CFRP hybrid composites under long-term hygrothermal conditions10.1016/j.compositesa.2017.02.011 ↗
6. Metal surface nanopatterning for enhanced interfacial adhesion in fiber metal laminates10.1016/j.compscitech.2021.108651 ↗
7. Novel thermoplastic fiber metal laminates manufactured with an innovative acrylic resin at room temperature10.1016/j.compositesa.2020.106043 ↗
8. Effect of different preparation methods on mechanical behaviors of carbon fiber-reinforced PEEK-Titanium hybrid laminates10.1016/j.polymertesting.2020.106462 ↗
9. Effects of a silane coupling agent on the tensile adhesive strength between resin and titanium10.1002/app.38917 ↗
10. Joining of metal to plastic using friction lap welding10.1016/j.matdes.2013.08.056 ↗
11. Friction spot welding between porous TC4 titanium alloy and ultra high molecular weight polyethylene10.1016/j.matdes.2017.06.071 ↗
12. Characteristics and formation mechanism of porosities in CFRP during laser joining of CFRP and steel10.1016/j.compositesb.2014.10.023 ↗
13. Laser direct joining of metal and plastic10.1016/j.scriptamat.2008.08.026 ↗
14. Ultrasonic joining: a novel direct-assembly technique for metal-composite hybrid structures10.1016/j.matlet.2016.01.137 ↗
15. Ultrasonic metal welding of Aluminium sheets to carbon fibre reinforced thermoplastic composites10.1002/adem.200800271 ↗
16. Formation of boehmite crystals on microblasted aluminum surface to enhance performance of metal–polymer direct joining10.1016/j.matlet.2019.126963 ↗
17. Joining strength dependence on molding conditions and surface textures in blast-assisted metal-polymer direct joining10.1016/j.cirp.2018.04.112 ↗
18. Aluminum/polypropylene composites produced through injection molding10.1016/j.jmatprotec.2018.01.008 ↗
19. PBT–anodized aluminum alloy direct joining: characteristic injection speed dependence of injected polymer replicated into nanostructures10.1016/j.polymertesting.2019.02.006 ↗
20. The effects of grit-blasting on surface properties for adhesion10.1016/S0143-7496(98)00061-X ↗
21. An overview of the polymer-to-metal direct-adhesion hybrid technologies for load-bearing automotive components10.1016/j.jmatprotec.2007.06.058 ↗
22. How to optimize adhesion in hard-soft overmolding
23. Effect of surface topography on injection joining Ti alloy for improved bonding strength of metal-polymer10.1016/j.surfcoat.2022.128132 ↗
24. Formation mechanism of porous anodic Aluminium and titanium oxides10.1002/adma.200800845 ↗
25. Investigations of corrosion on the surface of titanium substrate caused by combined alkaline and heat treatment10.1016/j.corsci.2014.01.014 ↗
26. The effect of heat treatment on bone-bonding ability of alkali-treated titanium10.1016/S0142-9612(98)90203-4 ↗
27. Effect of heat treatment on apatite-forming ability of Ti metal induced by alkali treatment10.1023/A:1018524731409 ↗
28. Surface modifications of Ti alloy with tunable hierarchical structures and chemistry for improved metal–polymer interface used in deepwater composite riser10.1016/j.apsusc.2014.12.081 ↗
29. Wetting of textured surfaces10.1016/S0927-7757(02)00061-4 ↗
30. Resistance of solid surfaces to wetting by water10.1021/ie50320a024 ↗
31. Surface roughness and contact angle10.1021/j150474a015 ↗
32. Light-induced amphiphilic surfaces10.1038/41233 ↗