New insight into the fitness of 13Cr stainless steel in H2S-containing environment at high temperature
Source abstract
Abstract
In the oil and gas industry, the selection of tubing and casing materials is required to follow international standard ISO 15156. However, it does not provide guidance on selecting stainless steel materials for H2S-containing wells above 232 °C, which raises uncertainty about the suitability of 13Cr steel. This work focuses on investigating the mechanical degradation and failure mechanisms of 13Cr stainless steel exposed to high-temperature conditions and proposed a creep constitutive model. Then, the corrosion and cracking mechanisms of 13Cr stainless steel at temperatures ranging from 150 °C to 350 °C were elucidated. Results show that 13Cr stainless steel meets the current material selection criteria (GB/T34907-2017) for mechanical properties and creep resistance. In the range of 150 ∼ 250 °C, the localized corrosion is dominant, and stress-oriented hydrogen-induced cracking occurs at 150 °C. As the temperature increases from 250 °C to 350 °C, although the maximum value of uniform corrosion rate is as high as 0.2960 mm/a, the cracking does not happen. Therefore, with the implementation of suitable protective measures, 13Cr stainless steel can be utilized in wells that the temperatures ranging from 250 °C to 350 °C and H2S partial pressures up to 0.17 MPa. This aligns with the global carbon-neutral agenda.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Fatigue and fracture mechanics · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (41)
Show source-provided references
1. Experimental study of the autothermic pyrolysis in-situ conversion process (ATS) for oil shale recovery10.1016/j.energy.2022.124878 ↗
2. Production performance of oil shale in-situ conversion with multilateral wells10.1016/j.energy.2019.116145 ↗
3. Reliability analysis of super 13Cr tubing in ultra-deep gas well10.4236/eng.2019.117030 ↗
4. Well safety and integrity evaluation of offshore wells: a review of past, present, and future10.1016/j.petrol.2022.110329 ↗
5. Insight into the galvanic corrosion behavior of the LHE Cd-Ti 300 M steel coupled with TC4 titanium alloy in different atmospheric environments10.1016/j.jelechem.2022.116827 ↗
6. Corrosion behavior of two low alloy steel in simulative deep-sea environment coupling to titanium alloy10.1016/j.colcom.2019.01.003 ↗
7. Design of a new 11Cr martensitic steel and evaluation of its long-term creep rupture strengths10.1016/j.jmrt.2022.08.116 ↗
8. Long-term creep rupture strength prediction for a new grade of 9Cr martensitic creep resistant steel (G115)—an application of a new tensile creep rupture model10.1016/j.jmrt.2020.03.079 ↗
9. Creep crack growth behavior analysis of the 9Cr-1Mo steel by a modified creep-damage model10.1016/j.msea.2017.09.112 ↗
10. Influence of a small velocity variation on the evolution of the corrosion products and corrosion behaviour of super 13Cr SS in a geothermal CO2 containing environment10.1016/j.corsci.2020.108983 ↗
11. Effect of extremely aggressive environment on the nature of corrosion scales of HP-13Cr stainless steel10.1016/j.apsusc.2018.10.237 ↗
12. Insight into the stress corrosion cracking of HP-13Cr stainless steel in the aggressive geothermal environment10.1016/j.corsci.2021.109699 ↗
13. Corrosion behaviour of 13Cr stainless steel under stress and crevice in 3.5 wt.% NaCl solution10.1016/j.corsci.2019.108290 ↗
14. The influence of composition on the hot ductility of steels and to the problem of transverse cracking10.2355/isijinternational.39.833 ↗
15. Corrosion behavior of 13Cr stainless steel under stress and crevice in high pressure CO2/O2 environment10.1016/j.jmst.2021.02.018 ↗
16. Effects of warm laser peening on the elevated temperature tensile properties and fracture behavior of IN718 nickel-based superalloy10.1016/j.engfracmech.2016.11.016 ↗
17. Orientation and temperature dependence of yielding and deformation behavior of a nickel-base single crystal superalloy10.1016/j.msea.2008.12.039 ↗
18. Hot tensile deformation and fracture behaviors of a typical ultrahigh strength steel10.1016/j.vacuum.2019.108863 ↗
19. Martensite–ferrite interface strength in a low-carbon bainitic steel10.1016/j.scriptamat.2005.09.012 ↗
20. The effect of martensite particle size on tensile fracture of surface-carburised AISI 8620 steel with dual phase core microstructure10.1016/S0261-3069(02)00065-1 ↗
21. Experimental investigation on martensitic transformation and fracture morphologies of austenitic stainless steel10.1016/j.ijplas.2009.03.003 ↗
22. Study on high temperature creep behavior of the accident-resistant cladding Fe–13Cr–4Al-1.85Mo-0.85Nb alloy10.1016/j.msea.2020.140688 ↗
23. Effect of extremely high CO2 pressure on the formation of the corrosion film on 13Cr stainless steel10.1039/C9RA08373A ↗
24. Evolution and characterization of the film formed on super 13Cr stainless steel in CO2-saturated formation water at high temperature10.1016/j.corsci.2019.108277 ↗
25. Corrosion of low alloy steel containing 0.5% chromium in supercritical CO2-saturated brine and water-saturated supercritical CO2 environments10.1016/j.apsusc.2018.01.181 ↗
26. XPS study of the reaction of chromium (VI) with mackinawite (FeS)10.1002/sia.1303 ↗
27. Descostes · Appl Surf Sci · 2000 · 165 · 28810.1016/S0169-4332(00)00443-8 ↗
28. A thermodynamic and kinetic study of the formation and evolution of corrosion product scales on 13Cr stainless steel in a geothermal environment10.1016/j.corsci.2020.108640 ↗
29. Interactions of SO2 with sodium deposited on silica10.1016/0021-9797(85)90280-2 ↗
30. J. Auger parameters for sulfur-containing compounds using a mixed aluminum-silver excitation source10.1016/0368-2048(90)87059-W ↗
31. Effects of flow velocity on the corrosion behaviour of super 13Cr stainless steel in ultra-HTHP CO2–H2S coexistence environment10.1016/j.corsci.2022.110235 ↗
32. J. Relaxation energies in XPS and XAES of solid sulfur compounds10.1016/0368-2048(94)02129-5 ↗
33. X-ray photoelectron spectroscopic analysis of surface products on pyrite formed by bacterial leaching10.2116/bunsekikagaku.40.11_609 ↗
34. An x‐ray photoelectron spectroscopic study of some chromium–oxygen systems10.1002/sia.740130210 ↗
35. An XPS characterization of FeCO3 films from CO2 corrosion10.1016/S0010-938X(98)00180-2 ↗
36. Surface reactions of chlorine molecules and atoms with water and sulfuric acid at low temperatures10.1016/0021-9797(79)90062-6 ↗
37. Molecular spectroscopy by means of ESCA II. Sulfur compounds. Correlation of electron binding energy with structure10.1088/0031-8949/1/5-6/020 ↗
38. Porous FeS nanofibers with numerous nanovoids obtained by Kirkendall diffusion effect for use as anode materials for sodium-ion batteries10.1007/s12274-016-1346-9 ↗
39. Corrosion behavior and mechanism of irradiated 304 nuclear grade stainless steel in high-temperature water10.1007/s40195-020-01123-y ↗
40. Addition of niobium in Fe-13Cr-4.5 Al-2Mo alloy used as ATF cladding: effect on high temperature water corrosion and in-situ electrochemistry10.1016/j.matdes.2022.110854 ↗
41. The contribution of hydrogen to the corrosion of 2024 aluminium alloy exposed to thermal and environmental cycling in chloride media10.1016/j.corsci.2012.12.005 ↗