Casting of film-cooling holes for single-crystal blades
Source abstract
Abstract
The flawless formation of film-cooling holes (FCHs) is critical for manufacturing single-crystal blade. Presently, high-energy beam drilling is mostly used to process gas film holes, which introduces the limitations of complex hole structures that are difficult to form and processing thermal defects that are difficult to eliminate. This study demonstrates an approach to form FCHs using casting, where an indirect additive manufacturing technology using a core/shell integral ceramic mold is applied for casting. Cylindrical 0.4, 0.8, and 4.0 mm-diameters hole are cast. The influence of fine ceramic cores on the microstructure of single-crystal blades during directional solidification is investigated using simulations and experiments. The fine ceramic cores of the FCHs affect the growth morphology of dendrites around the hole, which is determined by the hole diameter, primary dendrite spacing, and local temperature filed. Owing to the thermal conductivity difference between the alloy and ceramic, the local temperature filed around the holes changes abruptly, leading to the formation of shrinkage porosity and cavities. Furthermore, the process window for the casting of FCHs is determined using the longitudinal temperature gradient (GZ) and solidification rate (VZ). The proposed approach is of practical significance for the defect-free casting of tiny structures in single-crystal blades.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Solidification and crystal growth phenomena · Aluminum Alloy Microstructure Properties · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Alloy design for aircraft engines10.1038/nmat4709 ↗
2. Sliver defect formation in single crystal Ni-based superalloy castings10.1016/j.matdes.2020.109138 ↗
3. Review on additive manufacturing of single-crystal Nickel-based superalloys
4. Experimental investigation of film cooling effectiveness on a gas turbine blade pressure surface with diffusion slot holes10.1016/j.applthermaleng.2019.114851 ↗
5. A review of shaped hole turbine film-cooling technology10.1115/1.1860562 ↗
6. Prediction method for creep life of thin-wall specimen with film cooling holes in Ni-based single-crystal superalloy10.1016/j.ijmecsci.2018.04.018 ↗
7. Self-adjusting EDM/ECM high speed drilling of film cooling holes10.1016/j.jmatprotec.2018.06.026 ↗
8. Tube electrode high-speed electrochemical discharge drilling using low-conductivity salt solution10.1016/j.ijmachtools.2015.02.011 ↗
9. Investigation on geometric precision and surface quality of microholes machined by ultrafast laser10.1016/j.optlastec.2019.105834 ↗
10. Femtosecond laser high-quality drilling of film cooling holes in nickel-based single superalloy for turbine blades with a two-step helical drilling method10.1016/j.jmatprotec.2022.117827 ↗
11. Femtosecond laser ablation regimes in a single-crystal superalloy10.1007/s11661-007-9260-0 ↗
12. Removal of recast layer in the laser drilled film cooling holes by a two-step inner streaming electrochemical technique10.1088/1361-6439/ac0516 ↗
13. Coaxial waterjet-assisted laser drilling of film cooling holes in turbine blades10.1016/j.ijmachtools.2019.103510 ↗
14. Breakthrough phenomena in drilling micro holes by EDM10.1016/j.ijmachtools.2019.103436 ↗
15. Laser assisted casting of cooling hole and related system
16. Method for casting cooling holes
17. Turbine airfoil cooling system with leading edge impingement cooling system turbine blade investment casting using film hole protrusions for integral wall thickness control
18. Roadmap for additive manufacturing: toward intellectualization and industrialization
19. A review on distortion and residual stress in additive manufacturing
20. Quantitative analysis of withdrawal rate on stray grain formation in the platforms of a Ni-Based single crystal dummy blade10.1016/j.jallcom.2018.09.217 ↗
21. Temperature evolution and grain defect formation during single crystal solidification of a blade cluster10.1007/s41230-017-7150-7 ↗
22. Effect of platform dimension on the dendrite growth and stray grain formation in a Ni-base single-crystal superalloy10.1007/s11661-012-1527-4 ↗
23. Role of dendrite branching and growth kinetics in the formation of low angle boundaries in Ni–base superalloys10.1016/j.msea.2005.09.030 ↗
24. Variation of crystal orientation and dendrite array generated in the root of SX turbine blades10.3390/ma12244126 ↗
25. Effect of polydimethylsiloxane on the mid-temperature strength of gelcast Al2O3 ceramic parts10.1016/j.matdes.2015.09.150 ↗
26. Researches on the pyrolyzing strength of gelcasting Al2O3-based ceramic molds for double-wall blade10.1111/jace.16651 ↗
27. Fabrication of single-crystal superalloy hollow blade based on integral ceramic mold10.1016/j.jmatprotec.2019.04.037 ↗
28. Effect of processing parameters and shape of blade on the solidification of single-crystal CMSX-4 Ni-Based superalloy10.1007/s11663-018-1347-z ↗
29. Experimental study on film cooling and heat transfer characteristics of a twisted vane with staggered counter-inclined film-hole and laid-back-shaped-hole10.1016/j.ijheatmasstransfer.2021.121377 ↗
30. Optimization of film cooling arrays on a gas turbine vane by using an integrated approach of numerical simulation and parameterized design10.1016/j.applthermaleng.2022.119464 ↗
31. Primary spacing selection in directionally solidified alloys10.1016/0956-7151(94)90045-0 ↗
32. On directional dendritic growth and primary spacing-A review10.3390/cryst10070627 ↗
33. Interaction of porosity with a planar solid/liquid interface10.1007/s11661-004-0260-z ↗
34. Designing homogenization–solution heat treatments for single crystal superalloys10.1016/j.msea.2010.05.019 ↗
35. Solidification characteristics and as-cast microstructures of a Ru-containing nickel-based single crystal superalloy10.1016/j.jmrt.2021.01.043 ↗
36. Stability of dendrite growth during directional solidification in the presence of a non-axial thermal field10.1016/j.actamat.2014.05.040 ↗