Hot corrosion behavior analysis and diffusion equation construction based on laser wire additive manufacturing GH3039
Source abstract
Abstract
Laser wire additive manufacturing GH3039 samples with different process parameters are prepared. Then, hot corrosion test (Na2SO4+NaCl at 900 °C) is carried out. High power (5000 w), parallel to the deposition layer interface processing sample has good hot corrosion resistance due to the excellent internal organization. Element diffusion is the main factor affecting the hot corrosion performance. The element diffusion equation based on the multi-reaction interface is established and the degree of hot corrosion reaction can be directly judged. At the same time, the concept of determining the degree of hot corrosion reaction and predicting the trend of reaction by means of sulfides is proposed.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Welding Techniques and Residual Stresses · Additive Manufacturing and 3D Printing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Injeti · 2015
2. Application status and development of superalloy in energy industry10.3724/SP.J.1037.2009.00860 ↗
3. Elhajjar · 2017
4. Srivastava · 2019
5. Design and development of a high-performance Ni-based superalloy WSU 150 for additive manufacturing10.1016/j.jmst.2020.01.041 ↗
6. Role of alloy composition on micro-cracking mechanisms in additively manufactured Ni-based superalloys10.1016/j.actamat.2023.119089 ↗
7. Alloys-by-design: application to new superalloys for additive manufacturing10.1016/j.actamat.2020.09.023 ↗
8. Numerical modeling of microstructure evolution during laser additive manufacturing of a nickel-based superalloy10.1016/j.actamat.2014.05.039 ↗
9. Additive manufacturing of a functionally graded material from Ti-6Al-4V to Invar: experimental characterization and thermodynamic calculations10.1016/j.actamat.2016.12.070 ↗
10. Anisotropic tensile behavior of Ti–6Al–4V components fabricated with directed energy deposition additive manufacturing10.1016/j.actamat.2014.12.054 ↗
11. Additive manufacturing of titanium and nickel- based superalloys: a review10.1016/j.matpr.2023.07.082 ↗
12. Improving the deposition efficiency and mechanical properties of additive manufactured Inconel 625 through hot wire laser metal deposition10.1016/j.jmatprotec.2023.118175 ↗
13. Effect of thermomechanical processing on compressive mechanical properties of Ti–15Mo additively manufactured by laser metal deposition10.1016/j.msea.2023.145834 ↗
14. Additive manufacturing of functionally graded metallic materials using laser metal deposition
15. Directed Energy Deposition of stainless steel wire with laser beam: evaluation of geometry and affection depth10.1016/j.procir.2021.03.121 ↗
16. Influence of isothermal tempering on microstructures and hydrogen-environmentally embrittlement susceptibility of laser additively manufactured ultra-high strength AerMet100 steel10.1016/j.msea.2023.145167 ↗
17. Scapin · 2022
18. Shear punch testing for evaluation of mechanical properties of post heat-treated Inconel 718 nickel-based superalloy fabricated by additive manufacturing10.1016/j.jmrt.2023.09.149 ↗
19. Additive manufacturing in the aerospace and automotive industries: recent trends and role in achieving sustainable development goals10.1016/j.asej.2023.102516 ↗
20. Revolutionizing manufacturing: a comprehensive overview of additive manufacturing processes, materials, developments, and challenges10.1016/j.jmapro.2023.10.024 ↗
21. Insight into the passivation and corrosion behavior of additive manufacturing repaired single crystal superalloy10.1016/j.corsci.2022.110340 ↗
22. Improving oxidation resistance of wire arc additive manufactured Inconel 625 Ni-based superalloy by pack aluminizing10.1016/j.cirpj.2023.07.011 ↗
23. Corrosion behavior of wire arc additive manufactured Inconel 718 superalloy10.1016/j.jallcom.2020.154455 ↗
24. High-temperature oxidation behaviour of high chromium superalloys additively manufactured by conventional or extreme high-speed laser metal deposition10.1016/j.corsci.2020.108922 ↗
25. Hot corrosion behaviour of wire-arc additive manufactured Ni-based superalloy ATI 718Plus10.1016/j.corsci.2019.07.010 ↗
26. Influence of post heat treatment on metallurgical, mechanical, and corrosion analysis of wire arc additive manufactured inconel 62510.1016/j.jmrt.2023.11.074 ↗
27. A review: interlayer joining of nickel base alloys10.1016/j.jajp.2020.100030 ↗
28. Effect of ultrasonic micro-forging treatment on microstructure and mechanical properties of GH3039 superalloy processed by directed energy deposition10.1016/j.jmst.2020.09.001 ↗
29. Influence of Cr content on hot corrosion and a special tube sealing test of single crystal nickel base superalloy10.1016/j.corsci.2019.05.001 ↗
30. Young · 2016
31. Hot corrosion performance of a NiCr coated Ni-based alloy10.1016/j.scriptamat.2006.03.054 ↗
32. Hot corrosion and electrochemical behavior of NiCrAlY, NiCoCrAlY and NiCoCrAlYTa coatings in molten NaCl-Na2SO4 at 800 °C10.1016/j.surfcoat.2022.128503 ↗
33. Hot corrosion behaviour of low Al NiCoCrAlY cladded coatings reinforced by nano-particles on a Ni-base super alloy10.1016/j.corsci.2010.07.011 ↗
34. Influence of Cr content on hot corrosion and a special tube sealing test of single crystal nickel base superalloy10.1016/j.corsci.2019.05.001 ↗
35. Oxidation and hot corrosion behaviors of Mo-doped NiMoAlY alloys at 750 °C10.1016/j.corsci.2022.110262 ↗