journal article·2024-05Open access

Comparison of the corrosion and cavitation erosion behaviors of the cast and surface-modified manganese-aluminum bronzes in sodium chloride solution

Q.N. Song, Y. Wang, Z.T. Jin, Y.C. Zhang, N. Xu, Y.F. Bao, Y.F. Jiang, Q.Q. Lu, J.H. Zhao, Y. Gao, H.L. Zhang

Abstract

Modified layers with refined and homogenized microstructure were obtained on a cast manganese aluminum bronze (MAB) by friction stir processing (FSP) and laser surface melting (LSM). In 3.5% NaCl solution, a much more protective film was formed and uniform corrosion occurred for the two surface-modified MABs. The corrosion rate of the cast sample was reduced by a factor of 29.73% after FSP and 51.35% after LSM. The cavitation erosion (CE) rate of the cast MAB was about 1.83 and 3.07 times larger than that of the FSP and LSM samples, respectively. The CE resistance increment was highly attributed to the improved hardness and enhanced nano-indentation behavior after FSP or LSM. For each MAB, the CE resistance decreased with extended pre-immersion time. Compared with the result of the correspondingly freshly-prepared sample, the CE rate was raised by a factor of 36.22%, 42.97% and 44.00% after 30 days’ pre-immersion for the cast, FSP and LSM MABs, respectively. For the cast and FSP MABs, mechanical impact was the leading factor accounting for CE degradation. For the pre-corroded samples, corrosion damage at the β and κ phases weakened the mechanical properties and thus triggered more grievous material exfoliation under CE. For the LSM MAB, CE-corrosion synergy dominantly gave rise to the CE damage. Corrosion at grain boundaries after pre-immersion also deteriorated the CE performance. The LSM MAB possessed the highest corrosion and CE resistances because the fine single-phase microstructure reduced the galvanic corrosion effect and crack propagation tendency under CE impact.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metallurgy and Material Science · Materials Engineering and Processing · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (38)

Show source-provided references
1. Characterization of phases in an as-cast copper-manganese-aluminum alloy
2. Effect of laser surface melting on the corrosion and cavitation erosion behaviors of a manganese-nickel-aluminium bronze10.1016/j.msea.2004.01.016 ↗
3. Effects of Ce, Sm and Yb on cavitation erosion of NAB alloy in 3.5% NaCl solution10.1016/j.ultsonch.2022.106093 ↗
4. The role of Ti in cavitation erosion and corrosion behaviours of NAB alloy in 3.5% NaCl solution10.1016/j.jallcom.2022.165728 ↗
5. Microstructure design to improve the corrosion and cavitation corrosion resistance of a nickel-aluminum bronze10.1016/j.corsci.2018.04.043 ↗
6. Corrosion and cavitation erosion resistance enhancement of cast Ni–Al bronze by laser surface melting10.1007/s42243-021-00674-3 ↗
7. Microstructure modification and improving corrosion resistance of laser surface quenched nickel–aluminum bronze alloy10.1016/j.corsci.2020.108744 ↗
8. Effect of laser surface melting on microstructure evolution and cavitation behavior of nickel aluminum bronze10.1016/S1003-6326(23)66246-6 ↗
9. Friction stir processing of a cast manganese-aluminum bronze for improving corrosion and cavitation erosion resistances
10. Strengthening mechanism of friction stir processed and post heat treated NiAl bronze alloy: effect of rotation rates10.1016/j.msea.2016.12.050 ↗
11. Erosion-corrosion behaviour of shot peening treated nickel-aluminium bronze in simulated sand-containing seawater10.1016/j.corsci.2022.110908 ↗
12. Effect of shot peening on surface characterization and cavitation resistance of nickel aluminum bronze
13. Effect of sulfide concentration on the corrosion and cavitation erosion behavior of a manganese-aluminum bronze in 3.5% NaCl solution10.1007/s11665-019-04150-8 ↗
14. Corrosion evaluation of welded nickel aluminum bronze and manganese aluminum bronze in synthetic sea water10.1002/maco.202213328 ↗
15. Correlation between electron work functions of multiphase Cu-8Mn-8Al and de-alloying corrosion10.1016/j.apsusc.2018.01.018 ↗
16. Synergistic effect between cavitation erosion and corrosion for various copper alloys in sulphide-containing 3.5% NaCl solutions
17. Friction stir welding and processing10.1016/j.mser.2005.07.001 ↗
18. Effect of pre-corrosion on the cavitation erosion performance of two aluminum bronzes in 3.5% NaCl solution
19. 2010
20. Inhomogeneous microstructure and mechanical properties of friction stir processed NiAl bronze10.1016/j.msea.2009.06.013 ↗
21. Improvement in cavitation erosion resistance of a copper-based propeller alloy by laser surface melting10.1016/j.surfcoat.2003.08.048 ↗
22. On the significance of the H/E ratio in wear control: a nanocomposite coating approach to optimised tribological behavior10.1016/S0043-1648(00)00488-9 ↗
23. Cavitation erosion resistance enhancement of martensitic stainless steel via low-temperature plasma carburizing
24. The effects of the H/E ratio of various Cr-N interlayers on the adhesion strength of CrZrN coatings on tungsten carbide substrates10.1016/j.surfcoat.2015.06.077 ↗
25. Effect of modulation period on microstructure and mechanical properties of (AlSiTiVNbCr)N/(AlSiTiVNbCr)CN nano-multilayer films10.1016/j.vacuum.2022.111660 ↗
26. Influence of scanning speed on the microstructure, nanoindentation characteristics and tribological behavior of novel maraging steel coatings by laser cladding10.1016/j.matchar.2023.113335 ↗
27. Effect of solution treatment on cavitation erosion behavior of high-nitrogen austenitic stainless steel10.1016/j.wear.2019.01.098 ↗
28. Observation of microstructure and corrosion behaviour of some aluminium bronzes10.1179/000705986798272046 ↗
29. Cavitation erosion of materials10.1179/imr.1986.31.1.1 ↗
30. Correlation of microstructure with cavitation erosion behaviour of a nickel-aluminum bronze in simulated seawater10.1016/j.triboint.2019.03.071 ↗
31. Marine wear and tribocorrosion10.1016/j.wear.2017.01.076 ↗
32. Different methods of measuring synergy between cavitation erosion and corrosion for nickel aluminium bronze in 3.5% NaCl solution
33. Synergistic effects of cavitation erosion and corrosion for nickel aluminium bronze with oxide film in 3.5% NaCl solution10.1016/j.wear.2017.01.047 ↗
34. Effect of compressive stress on cavitation erosion-corrosion behavior of nickel-aluminum bronze alloy10.1016/j.ultsonch.2022.106143 ↗
35. 2015
36. Effect of passivity on electrochemical corrosion behavior of alloys during cavitation in aqueous solutions10.1016/j.wear.2007.01.006 ↗
37. Synergistic effect of cavitation erosion and corrosion of various engineering alloys in 3.5% NaCl solution10.1016/S0921-5093(00)00899-6 ↗
38. Cavitation erosion corrosion behaviour of manganese-nickel-aluminum bronze in comparison with manganese-brass