Porosity suppression of nickel-based superalloy by modulated base temperature in laser welding and mechanism analysis
Source abstract
Abstract
This paper investigates the distribution pattern of welding porosity defects in annular weld seams of superalloy during laser welding. The results reveal that the initial portion of the annular weld seam exhibits a higher density and larger size of porosity defects compared to the ending portion. At a laser power of P=360 W, the numerical simulation combination showed that the A1 region's average cooling rate is 8.767×103 °C/s and the A2 region is 8.151×103 °C/s that the thermal conduction effect at the initial welding position leads to an elevation in the base metal temperature in the subsequent unwelded region, thereby reducing the solidification rate of the molten pool in the latter half of the weld seam and effectively decreasing the porosity rate at the weld seam. Furthermore, the study demonstrates that elevating the base metal temperature can effectively modify the cooling rate of the molten pool, thereby influencing the formation of porosity defects. At a laser power of P=360 W, increasing the base metal temperature to 600 °C reduces the cooling rate of the molten pool from 8.767×103 °C/s at a base metal temperature of T=20 °C to 7.451×103 °C/s, leading to a decrease in the porosity rate from 3.357% to 0.022%. At a laser power of P=672 W, increasing the base metal temperature to 600°C reduces the cooling rate of the molten pool from 6.781×103 °C/s at a base metal temperature of T=20 °C to 5.056×103 °C/s, leading to a decrease in the porosity rate from 8.214% to 0.002%. The increase in laser power brings more heat input, so the solidification rate of the molten pool decreases, but the porosity increases significantly. However, increasing the base temperature can effectively suppress the porosity defects under different laser powers. The research further reveals the relationship between welding porosity rate and cooling conditions, providing a control strategy for achieving low porosity rate welds.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Welding Techniques and Residual Stresses · Additive Manufacturing Materials and Processes · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (50)
Show source-provided references
1. Investigation of macrostructure, microstructure, and hot cracking susceptibility of laser-welded inconel-718 superalloy under various post-cold treatment environments10.1016/j.cirpj.2022.01.007 ↗
2. The effect of pulsed laser welding on hot cracking susceptible region size and molten pool internal geometry of inconel 718: numerical and experimental approaches10.1016/j.cirpj.2021.09.001 ↗
3. Gcp and tcp phases presented in nickel-base superalloys10.1016/j.matpr.2016.03.024 ↗
4. Study on the structural transition and thermal properties of ni3nb-d022 phase: first-principles calculation10.1016/j.matdes.2017.10.065 ↗
5. Effect of a gradient structure on the mechanical performance of inconel 718 ni-based superalloy at elevated temperatures10.1016/j.jmrt.2023.01.121 ↗
6. Thermodynamic study of δ-ni3nb, nucleation phase γ and transformation phase γ″ under high pressure: first-principles calculations10.1016/j.physb.2022.414087 ↗
7. Effects of coupling between the laser plasma and two arcs on metal transfer in co2 laser double-wire mig hybrid welding10.1016/j.optlastec.2018.02.044 ↗
8. Study on coupling characteristics of different welding modes in laser-double tig hybrid welding10.1016/j.optlastec.2023.109621 ↗
9. A study of the radiation of a nd:yag laser–mig hybrid plasma10.1016/j.optlastec.2009.05.010 ↗
10. [Invited] an overview of the state of art in laser welding simulation10.1016/j.optlastec.2015.09.015 ↗
11. K. V. PP, R. R, K. GM, S. N. Microstructure and properties of inconel 718 and aisi 416 laser welded joints10.1016/j.jmatprotec.2018.10.039 ↗
12. A study of the mechanism of laser welding defects in low thermal expansion superalloy gh90910.1016/j.matchar.2013.01.008 ↗
13. Comparative study on fiber laser welding of gh3535 superalloy in continuous and pulsed waves10.1016/j.matdes.2016.08.055 ↗
14. Finite element simulation of magnesium alloys laser beam welding10.1016/j.jmatprotec.2010.02.023 ↗
15. Development of welding technology for improving the metallurgical and mechanical properties of 21st century nickel based superalloy 68610.1016/j.msea.2017.03.042 ↗
16. Improvement of wear resistance of hastelloy c-276 through laser surface melting10.1016/j.matdes.2012.10.024 ↗
17. Detection of weld defects by high speed imaging of the vapor plume10.1016/j.phpro.2013.03.113 ↗
18. Influence of welded pores on very long-life fatigue failure of the electron beam welding joint of tc17 titanium alloy10.3390/ma12111825 ↗
19. Influence of spatial power modulation on pore and crack formation in laser beam welding of aluminum10.2351/1.5085460 ↗
20. The effect of pre-heating and pre-cold treatment on the formation of liquation and solidification cracks of nickel-based superalloy welded by laser beam10.1016/j.jmrt.2020.07.053 ↗
21. Selective laser melting of the hard-to-weld in738lc superalloy: efforts to mitigate defects and the resultant microstructural and mechanical properties10.1016/j.jallcom.2019.151662 ↗
22. Effect of the welding position on weld quality when laser welding inconel 617 ni-based superalloy10.1016/j.optlastec.2021.106962 ↗
23. Porosity formation mechanism and suppression procedure in laser welding of aluminium alloys10.1080/09507110109549341 ↗
24. Direct observation of keyhole behaviour during pulse modulated high-power nd:yag laser irradiation10.1088/0022-3727/33/5/304 ↗
25. Optimizing the mechanical properties of weld joint in laser welding of gtd-111 superalloy and aisi 4340 steel10.1016/j.optlastec.2022.108537 ↗
26. Understanding pore formation in laser beam welding10.1016/j.phpro.2011.03.031 ↗
27. Porosity sensitivity of a356 al alloy during fiber laser welding10.1016/S1003-6326(15)63870-5 ↗
28. Dynamics of solid-liquid interface and porosity formation determined through x-ray phase-contrast in laser welding of pure al10.1016/j.jmatprotec.2017.06.033 ↗
29. Keyhole-induced porosity formation during laser welding10.1016/j.jmatprotec.2017.10.038 ↗
30. Improving the microstructure and mechanical properties of laser powder bed fusion-fabricated tantalum by high laser energy density10.1016/j.matlet.2022.133547 ↗
31. Effect of higher laser power remelting on porosity and mechanical performance of part built by laser powder bed fusion10.1007/s00170-023-11067-z ↗
32. Mesoscopic evolution of molten pool during selective laser melting of superalloy inconel 738 at elevating preheating temperature10.1016/j.matdes.2021.110355 ↗
33. Finite element modeling of the linear friction welding of gh4169 superalloy10.1016/j.matdes.2015.08.036 ↗
34. The coupled fem analysis of the transient temperature field during inertia friction welding of gh4169 alloy10.1016/S1006-7191(07)60043-X ↗
35. Microstructure and microhardness of dissimilar weldment of ni-based superalloys in718-in713lc10.1016/j.msea.2019.138894 ↗
36. Investigation on solution heat treatment response and γ′ solvus temperature of a mo-rich second generation ni based single crystal superalloy10.1016/j.intermet.2020.106896 ↗
37. Grain growth competition during melt pool solidification — comparing phase-field and cellular automaton models10.1016/j.commatsci.2022.111882 ↗
38. Comparison of phase-field and cellular automaton models for dendritic solidification in al–cu alloy10.1016/j.commatsci.2011.12.019 ↗
39. Grain growth competition during thin-sample directional solidification of dendritic microstructures: a phase-field study10.1016/j.actamat.2016.09.055 ↗
40. Dependence of competitive grain growth on secondary dendrite orientation during directional solidification of a ni-based superalloy. Metallurgical and Materials Transactions
41. Investigation of microstructure evolution process in circular shaped oscillating laser welding of inconel 718 superalloy10.1016/j.ijheatmasstransfer.2023.124522 ↗
42. Suppression of liquation cracking susceptibility via pre-weld heat treatment for manufacturing of cm247lc superalloy turbine blade welds
43. Research on laser welding process and molding effect under energy deviation10.1007/s00170-020-05431-6 ↗
44. Laves phase control of inconel 718 alloy using quasi-continuous-wave laser additive manufacturing10.1016/j.matdes.2017.03.004 ↗
45. A study on anisotropy in wire arc additively manufactured inconel 625 multi-layered wall and its correlation with molten pool thermal history10.1016/j.msea.2022.142865 ↗
46. Influence of molten-pool cooling rate on solidification structure and mechanical property of laser additive manufactured inconel 71810.1016/j.jmrt.2022.06.162 ↗
47. Study on mechanism of the effect of al element on the arc shape and molten pool fluctuation pattern in flux bands constricting arc welding (fbca)10.1016/j.jmapro.2023.06.044 ↗
48. Relationship between pool characteristic and weld porosity in laser arc hybrid welding of aa6082 aluminum alloy10.1016/j.jmatprotec.2016.10.001 ↗
49. Investigation on clockwise circular oscillating laser welding for the 5a06-h112 aluminum alloy: energy distribution, seam appearance, microstructure, and mechanical properties10.1016/j.optlastec.2024.111026 ↗
50. Towards a self-consistent model of the keyhole in penetration laser beam welding10.1088/0022-3727/26/3/021 ↗