Improving the defects and mechanical properties via secondary loading in a squeeze casting heat-treated Al–Cu alloy
Source abstract
Abstract
Defects are prone to form during solidification in Al–Cu alloy squeeze castings, especially at locations with significant differences in wall thickness. This work developed a secondary loading technique during squeeze casting to solve this problem. First, the finite element simulation method predicted the defect location in an Al–Cu alloy during squeeze casting. The application of secondary loading helped the alloy melt solidify under pressure and eliminate shrinkage porosity defects caused by solidification shrinkage. Subsequently, T6 heat treatment was performed to further improve the mechanical properties of the casting without solidification defects. The uniform distribution of θ′ nano precipitates in the casting was observed, increasing strength. This study aims to eliminate casting defects during squeeze casting to obtain high-performance castings.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Metallurgy and Material Forming · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. Effect of pressure on the microstructure refinement, solidification mechanism and fracture behavior of wrought Al-Zn-Mg-Cu alloys prepared by squeeze casting10.1016/j.jmatprotec.2023.118239 ↗
2. Effect of T6 heat treatment on microstructure and mechanical properties of large-weight aluminum alloy flywheel housing parts formed by local-loading squeeze casting10.1016/j.jmrt.2023.03.084 ↗
3. Squeeze casting for metal alloys and composites: an overview of influence of process parameters on mechanical properties and microstructure10.1007/s41230-022-2030-1 ↗
4. Numerical simulation and experimental validation of squeeze casting of AlSi9Mg aluminum alloy component with a large size10.3390/ma15124334 ↗
5. Numerical simulation and process optimization of squeeze casting process of an automobile control arm
6. Effect of local loading on microstructure and enhanced mechanical property of large complex castings prepared by Al–Si–Fe–Mn–Mg–Cu alloy during squeeze casting10.1016/j.jmst.2023.12.082 ↗
7. Repelling effect of Si on Cu atoms enhances the strength and ductility of Al alloys: atom probe tomography and first-principles analysis10.1016/j.msea.2025.147888 ↗
8. Influence of Mg and Cu on precipitation behaviors and mechanical properties of Al–Si alloys10.1016/j.msea.2024.146775 ↗
9. Influence of quenching cooling rate on residual stress and tensile properties of 2A14 aluminum alloy forgings10.1016/j.msea.2016.08.017 ↗
10. Effects of pre-stretch on microstructure, mechanical properties and corrosion resistance of 2A14 aluminum alloy10.1016/S1003-6326(23)66454-4 ↗
11. Microstructure and mechanical properties of squeeze-cast Al-5.0Cu-1Mn-based alloys with different Ni content10.1016/j.matdes.2023.111901 ↗
12. Selective laser melting of a novel Al-Si-Fe-Mn-Ni alloy with superior mechanical properties at both room and elevated temperatures: influence of processing parameters and heat treatment10.1016/j.matchar.2024.114098 ↗
13. Effects of post heat treatment on the microstructure and mechanical properties of selective laser melted AlSi10Mg alloys10.1016/j.msea.2024.146195 ↗
14. Revealing hot tear formation dynamics in Al–Cu alloys with X-ray radiography10.1016/j.actamat.2023.119421 ↗
15. The evolution and dissolution mechanism of θ-Al2Cu phase and the analysis of precipitation of a novel AlCu phase during elevated aging10.1016/j.matchar.2024.114454 ↗
16. Temperature-dependent creep aging behavior of 2A14 aluminum alloy10.1016/j.jmrt.2022.05.109 ↗
17. Compositional evolution of Q-phase precipitates in an aluminum alloy10.1016/j.actamat.2014.05.001 ↗
18. Micro-mechanism of simultaneous improvement of strength and ductility of squeeze-cast Al–Cu alloy10.1016/j.msea.2021.142538 ↗
19. Development of bimodal grain-structured Al-Zn-Mg-Cu-Zr alloys for strength-ductility synergy via microalloying with Hf and Sc10.1016/j.matchar.2023.113349 ↗
20. Strength and ductility enhancement of twin-roll cast Al-Zn-Mg-Cu alloys with high solidification intervals through a synergistic segregation-controlling strategy10.1016/j.jmst.2022.09.033 ↗
21. Effects of Ni on the microstructure, hot tear and mechanical properties of Al–Zn–Mg–Cu alloys under as-cast condition10.1016/j.jallcom.2019.153458 ↗
22. Effect of adding Pr on the microstructure and hot tearing sensitivity of as-cast Al-Cu-Mg alloys10.1016/j.matchar.2022.112141 ↗
23. Thermodynamics-guided design of sustainable secondary Al-Si alloys for enhanced Fe-impurity tolerance and optimized Mn doping10.1016/j.actamat.2025.120932 ↗
24. The microstructure characteristics and fracture behavior of the polyhedral primary iron-rich phase and plate-shaped eutectic iron-rich phase in a high-pressure die-cast AlSi10MnMg alloy10.1016/j.jmst.2022.09.014 ↗