The effects of heat treatment on the microstructure and mechanical properties of cold spraying additive manufacturing Ti
Source abstract
Abstract
ABSTRACT Cold spraying additive manufacturing (CSAM) Ti exhibits minimal plasticity, posing a significant challenge to its broader application. Heat treatment is recognized as a potent strategy to enhance the mechanical properties of additive manufacturing parts. However, prior investigations have struggled to discern the genuine impact of heat treatment on CSAM Ti due to the high porosity in initial deposits. This study addresses this gap by fabricating CSAM Ti deposits with a low porosity of 2.76%. The effects of annealing at varies temperature on the microstructure, porosity, and mechanical properties of the deposits were studied. The results show that annealing can promote recrystallization of CSAM Ti and reduce the porosity of CSAM Ti until to 0.77%. This increases the strength of CSAM Ti to 780 MPa, which even exceeds that of wrought pure Ti. Despite the low elongation of 4.67%, the CSAM Ti after suitable heat treatment can be used in fields in fields don’t require high plasticity.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced materials and composites · Intermetallics and Advanced Alloy Properties · Additive Manufacturing Materials and Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Mechanical behavior of ultrafine-grained Ti-6Al-4V alloy produced by severe warm rolling: the influence of starting microstructure and reduction ratio10.1007/s11661-015-3080-4 ↗
2. Understanding the microstructural evolution of cold sprayed Ti-6Al-4V coatings on Ti-6Al-4V substrates10.1016/j.apsusc.2018.07.175 ↗
3. Perspectives on titanium science and technology10.1016/j.actamat.2012.10.043 ↗
4. Deformation and fracture of Ti/439 stainless steel clad composite at intermediate temperatures10.1016/j.msea.2015.11.041 ↗
5. Manufacturing technology and application trends of titanium clad steel plates10.1016/S1006-706X(15)30099-6 ↗
6. Evaluation of mechanical and wear properties of TixNb7Fe alloys designed for biomedical applications10.1016/j.matdes.2016.09.029 ↗
7. Development of titanium based biocomposite by powder metallurgy processing with in situ forming of Ca-P phases10.1016/j.msea.2006.10.154 ↗
8. High strength biomedical Ti–13Mo–6Sn alloy: processing routes, microstructural evolution and mechanical behavior10.1016/j.msea.2019.138190 ↗
9. Mechanical behavior of porous commercially pure Ti and Ti–TiB composite materials manufactured by selective laser melting10.1016/j.msea.2014.12.036 ↗
10. Additive manufacturing of Ti6Al4V alloy: a review10.1016/j.matdes.2018.107552 ↗
11. Additive manufacturing of titanium alloys by electron beam melting: a review10.1002/adem.201700842 ↗
12. Microstructure optimization of cold sprayed Ti-6Al-4V using post-process heat treatment for improved mechanical properties
13. Enhancing corrosion resistance of Al alloy sheets with potential gradient by arc-sprayed Zn coatings10.1016/j.jmrt.2024.11.026 ↗
14. Wear and erosion performance of flame sprayed rare earth element-doped AlCoCrFeMo high entropy alloy coatings10.1016/j.wear.2025.205773 ↗
15. Thermal protection mechanism of novel high-entropy rare-earth niobate coating deposited by atmospheric plasma spraying10.1016/j.apsusc.2025.162315 ↗
16. Phase evolution and microstructure of suspension HVOF-sprayed alumina coatings10.1016/j.surfcoat.2025.131885 ↗
17. Owoseni T.A., Baiamonte L., Dumm T., Björklund S., Joshi S. Microstructural characteristics and wear behaviour of HVAF sprayed Ni-SiC composite coatings. Ceram Int. doi:10.1016/j.ceramint.2025.03.117 In Press.10.1016/j.ceramint.2025.03.117 ↗
18. Cold spray additive manufacturing and repair: fundamentals and applications
19. Elimination of porosity in directly fabricated titanium via cold gas dynamic spraying10.1016/j.jmatprotec.2008.03.005 ↗
20. Cold spray of Ni-based superalloys: a review on processing and residual stress10.1007/s11666-024-01916-y ↗
21. Ductile and high strength Cu fabricated by solid-state cold spray additive manufacturing10.1016/j.jmst.2022.07.003 ↗
22. Bulk-like ductility of cold spray additively manufactured copper in the as-sprayed state10.1016/j.addlet.2022.100052 ↗
23. Preparation of high-tensile-ductility and high-conductivity alumina dispersion-strengthened copper via a cold spray additive manufacturing-friction stir processing composite process10.1016/j.jallcom.2024.176467 ↗
24. Microstructure optimization of cold sprayed Ti-6Al-4V using post-process heat treatment for improved mechanical properties
25. An innovative and flexible approach to fabricate Mg/Al composite plates: cold spraying and hot rolling post-treatment10.1016/j.msea.2022.143515 ↗
26. Formation of nanoscale interface in a high-performance TA2/Q235 clad plate10.1016/j.matlet.2023.135528 ↗
27. Effect of rolling temperature on microstructure and mechanical properties of Ti/steel clad plates fabricated by cold spraying and hot-rolling10.1016/j.msea.2020.139982 ↗
28. Combinatorial synthesis of AlNi alloys by low-pressure cold spray deposition and post-laser alloying process10.1016/j.surfcoat.2024.131542 ↗
29. Effect of hot isostatic pressing (HIP) on microstructure and mechanical properties of Ti6Al4V alloy fabricated by cold spray additive manufacturing
30. The effects of heat treatment on the mechanical properties of cold-sprayed coatings10.1016/j.surfcoat.2014.11.017 ↗
31. Fe nanoparticles modified pure Ti alloy on microstructure evolution and fine crystallization mechanism fabricated by additive manufacturing10.1016/j.jmrt.2023.08.221 ↗
32. Grain-size-dependent ductile-to-brittle fracture mechanism of titanium sheets10.1016/j.scriptamat.2022.114877 ↗