journal article·2023-11Open access

Impact reliability enhancement approach of Sn–Bi–Zn–in alloy bumps under high-humidity and high-temperature tests

Zhi Jin, Shunsuke Fujiwara, Junichi Takenaka, Koichi Hagio, Hiroshi Nishikawa

Abstract

Sn–45Bi–2.6Zn–0.5In and Sn–45Bi–2.6Zn–1In alloys have previously been shown to be superior to Sn–58Bi under the thermal aging test. In this study, a comparative analysis of the microstructure and impact strength of Sn–58Bi, Sn–45Bi–2.6Zn–0.5In, and Sn–45Bi–2.6Zn–1In alloy bumps was conducted before and after high-humidity and high-temperature tests. Cross-sectional microstructure observations and impact tests were performed on all alloy bumps. The results indicated that the high-humidity and high-temperature conditions had a slight influence on the Sn–58Bi alloy bump, but it reduced the maximum force of Sn–45Bi–2.6Zn–0.5In and Sn–45Bi–2.6Zn–1In to almost zero and generated voids at the interface between the alloy and Cu pad after the test. This deterioration was mainly attributed to the formation of voids on the accumulated Zn at the interface under the effects of both high-humidity and high-temperature conditions. In addition, a possible approach for enhancing the impact strength of Zn-containing alloy bumps by adjusting the heating profile was proposed, and it was verified that the maximum force of the Zn-containing alloy bumps was significantly improved.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · Aluminum Alloy Microstructure Properties · Advanced Welding Techniques Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. A review of lead-free solders for electronics applications10.1016/j.microrel.2017.06.016 ↗
2. Reliability-enhanced microscale Ag sintered joint doped with AlN nanoparticles
3. Lead-free solders in microelectronics10.1016/S0927-796X(00)00010-3 ↗
4. Review of microstructure and properties of low temperature lead-free solder in electronic packaging10.1080/14686996.2020.1824255 ↗
5. Microstructure and mechanical properties of Sn–Bi, Sn–Ag and Sn–Zn lead-free solder alloys10.1016/j.jallcom.2013.03.234 ↗
6. The effect of aging on microstructure, room temperature deformation, and fracture of Sn-Bi/Cu solder joints10.1007/BF02653346 ↗
7. Effect of low Bi content on reliability of Sn-Bi alloy joints before and after thermal aging
8. Elastic modulus, hardness and creep performance of SnBi alloys using nanoindentation10.1016/j.msea.2012.07.120 ↗
9. Deformation mechanism of various Sn-xBi alloys under tensile tests10.1007/s42114-021-00231-2 ↗
10. Microstructure and fracture behavior of non eutectic Sn–Bi solder alloys10.1007/s10854-015-4143-4 ↗
11. Microstructure and mechanical behavior of Sn–40Bi–xCu alloy10.1007/s10854-017-7464-7 ↗
12. Effect of in on microstructure, thermodynamic characteristic and mechanical properties of Sn–Bi based lead-free solder10.1016/j.jallcom.2015.01.219 ↗
13. Effect of Sb content on properties of Sn—Bi solders10.1016/S1003-6326(14)63046-6 ↗
14. Interfacial reactions between molten Sn–Bi–X solders and Cu substrates for liquid solder interconnects10.1016/j.actamat.2006.02.030 ↗
15. Reactions of Sn-3.5 Ag-based solders containing Zn and Al additions on Cu and Ni (P) substrates10.1007/s11664-010-1382-2 ↗
16. Intermetallic compound growth suppression at high temperature in SAC solders with Zn addition on Cu and Ni–P substrates10.1016/j.jallcom.2011.09.024 ↗
17. Electronics assembly and high temperature Reliability using Sn-3.8 Ag-0.7 Cu solder paste with Zn additives10.1109/TCPMT.2013.2279055 ↗
18. Controlling Ag 3 Sn plate formation in near-ternary-eutectic Sn-Ag-Cu solder by minor Zn alloying
19. The newly developed Sn–Bi–Zn alloy with a low melting point, improved ductility, and high ultimate tensile strength10.1016/j.mtla.2019.100300 ↗
20. Interfacial behavior and joint strength of Sn–Bi solder with solid solution compositions10.1007/s10854-018-9233-7 ↗
21. Recent advances on SnBi low-temperature solder for electronic interconnections10.1007/s10854-021-06820-7 ↗
22. Ductile-to-brittle transition in Sn–Zn solder joints measured by impact test10.1016/j.scriptamat.2004.06.027 ↗
23. Evaluation of solder joint strengths under ball impact test10.1016/j.microrel.2006.11.015 ↗
24. A review of board level solder joints for mobile applications10.1016/j.microrel.2008.08.006 ↗
25. The reliability of lead-free solder joint subjected to special environment: a review10.1007/s10854-019-01333-w ↗
26. Novel transient liquid phase bonding method using In-coated Cu sheet for high-temperature die attach10.1016/j.materresbull.2021.111713 ↗
27. Thermal conductivity and reliability reinforcement for sintered microscale Ag particle with AlN nanoparticles additive
28. Three-dimensional interface and property of SnPb solder joint under extreme thermal shocking10.1080/13621718.2022.2029102 ↗
29. Correlation between microstructure and mechanical properties of Sn–Bi–X solders10.1016/j.msea.2015.11.038 ↗
30. Effects of in and Zn double addition on eutectic Sn-58Bi alloy
31. Improvement in the mechanical properties of eutectic Sn58Bi alloy by 0.5 and 1 wt% Zn addition before and after thermal aging10.1016/j.jallcom.2018.06.121 ↗
32. Oxidation behavior of Sn–Zn solders under high-temperature and high-humidity conditions10.1016/j.jallcom.2007.08.007 ↗
33. Effects of Bi and Pb on oxidation in humidity for low-temperature lead-free solder systems10.1007/s11664-006-0182-1 ↗
34. Polarity effect of electromigration on kinetics of intermetallic compound formation in Pb-free solder V-groove samples10.1063/1.1861151 ↗
35. Micro-galvanic corrosion effects on patterned copper-zinc samples during exposure in humidified air containing formic acid10.1149/2.113308jes ↗
36. Principles and prevention