journal article·2024-01Open access

Assessing underdeposit corrosion inhibitor performance for carbon steel in CO2/Sulfide environment

Eman M. Fayyad, Mostafa H. Sliem, Noora Al-Qahtani, Mary P. Ryan, Aboubakr M. Abdullah

Abstract

Under deposit corrosion (UDC) that occurs due to the deposition of solid particles, like iron sulfide or organic solids, and CO2 corrosion, cause disasters for pipelines and fluid-handling apparatus. This research investigated the impact of mineral deposits, like iron disulfide, iron sulfide, and sand, on the inhibition performance of the commercial UDC inhibitor in sulfated CO2-saturated brine solution at 60 °C and 1000 rpm flow rates for different immersion times. The deposit characteristics, type, and coverage technique on the steel (full/partial) were explored. The surface morphology, elemental analysis, and particle size of deposits in the absence and presence of the inhibitor were analyzed. The inhibitive effect at different inhibitor concentrations and the corrosion rates of steel in the absence and presence of the deposits were calculated from the fitting process of the electrochemical impedance spectroscopy (EIS) results. The utilized UDC inhibitor has the highest efficiency (about 95 %) at a concentration of 400 ppm. The FeS, FeS2 and SiO2 deposits in the presence of the inhibitor offered a 77.5 %, 94.5 % and 94.6 % inhibition efficiency after 6h of immersion time, resulting in about 77.5 %, 25.6 % and 60.1 % increase in their efficiencies before the addition of the inhibitor. Therefore, the inhibitor can effectively inhibit the UDC triggered by FeS and SiO2 deposits in an aqueous environment containing sulfated CO2. However, it is unavailable in the steel underneath the FeS2 deposit to inhibit corrosion. EDX and XPS analyses confirm the success of the inhibitor movement through deposits and its adsorption on steels.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Concrete Corrosion and Durability · Hydrogen embrittlement and corrosion behaviors in metals

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (88)

Show source-provided references
1. Electrochemical corrosion performance of Cr and Al alloy steels using J55 carbon steel as base alloy10.1016/j.corsci.2014.04.023 ↗
2. Review of corrosion kinetics and thermodynamics of CO2 and H2S corrosion effects and associated prediction/evaluation on oil and gas pipeline system
3. Inhibition of API 5L X60 steel corrosion in CO2 saturated 3.5% NaCl solution by tannic acid and synergistic effect of KI additive10.1016/j.molliq.2017.04.064 ↗
4. Comparison of corrosion behavior for X-65 carbon steel in supercritical CO2-saturated water and water-saturated/unsaturated supercritical CO210.1016/j.supflu.2014.12.005 ↗
5. The influence of microstructure and chemical composition of carbon and low alloy steels in CO2 corrosion. A state-of-the-art appraisal10.1016/S0261-3069(03)00158-4 ↗
6. Key issues related to modelling of internal corrosion of oil and gas pipelines-a review10.1016/j.corsci.2007.06.006 ↗
7. Predictive model for CO2 corrosion engineering in wet natural gas pipelines10.5006/1.3585212 ↗
8. Inhibition of hydrogen sulfide corrosion of steel in gas phase by tributylamine10.1016/j.corsci.2012.07.010 ↗
9. Application of corrosion inhibitors for steels in acidic media for the oil and gas industry: a review10.1016/j.corsci.2014.04.044 ↗
10. Effect of H2S on the CO2 corrosion of carbon steel in acidic solutions10.1016/j.electacta.2010.08.049 ↗
11. Electrochemical characteristics of the early corrosion stages of API X52 steel exposed to H2S environments10.1016/j.matchemphys.2014.10.020 ↗
12. Influence of sand production on design and operations of piping systems
13. Internal CO2 corrosion of mild steel pipelines under inert solid deposits
14. CO2 corrosion inhibitor performance in the presence of solids: test method development
15. Under-deposit caustic corrosion on sodium carbonate pipeline10.1016/j.proeng.2015.08.026 ↗
16. Top of the REAC tube corrosion induced by under deposit corrosion of ammonium chloride and erosion corrosion10.1016/j.engfailanal.2015.08.022 ↗
17. Under deposit corrosion (UDC) in the oil and gas industry: a review of mechanisms, testing and mitigation
18. Lepková · 2010
19. De Reus · 2005
20. Composition and properties of deposits formed on the internal surface of oil pipelines10.1007/s10812-018-0619-3 ↗
21. Nature of sulphides and their corrosive effect on ferrous metals: a review10.1179/000705975798320701 ↗
22. Chemistry of iron sulfide10.1021/cr0503658 ↗
23. Under-deposit corrosion
24. Dispersive adsorption of xylopia aethiopica constituents on carbon steel in acid-chloride medium: a combined experimental and theoretical approach10.1016/j.molliq.2017.11.051 ↗
25. Pyranpyrazole derivatives as novel corrosion inhibitors for mild steel useful for industrial pickling process: experimental and quantum chemical study10.1016/j.jiec.2017.03.044 ↗
26. Inhibition of acid corrosion of mild steel using delonix regia leaves extract10.56431/p-28ci51 ↗
27. Natural products for materials protection: mechanism of corrosion inhibition of mild steel by acid extracts of piper guineense10.1021/jp300791s ↗
28. Electrochemical, theoretical, and surface morphological studies of corrosion inhibition effect of green naphthyridine derivatives on mild steel in hydrochloric acid10.1021/acs.jpcc.5b11901 ↗
29. A green corrosion inhibitor for carbon steel in oil well acidizing environment10.1016/j.molliq.2018.05.058 ↗
30. Theoretical study of the mechanism of corrosion inhibition of carbon steel in acidic solution by 2-aminobenzothiazole and 2- mercaptobenzothiazole10.20964/2018.04.50 ↗
31. Ye · 2018
32. Guidelines for corrosion inhibitor selection for oil and gas production
33. Corrosion and corrosion inhibition in wet gas pipelines
34. Effect of Cr/Mo on the protectiveness of corrosion scales on carbon steel in sweet medium under high flow Regime10.1149/08010.0509ecst ↗
35. Local supersaturation and the growth of protective scales during CO2 corrosion of steel: effect of pH and solution flow10.1016/j.corsci.2017.05.026 ↗
36. Chloride-induced corrosion of steel rebars in simulated pore solutions of alkali activated concretes10.1016/j.cemconres.2017.08.006 ↗
37. Electrochemical characteristics of reinforced concrete corrosion as determined by impedance spectroscopy10.1179/bcj.1992.27.2.113 ↗
38. Corrosion inhibition of carbon steel in alkaline chloride media by Na3PO410.1016/j.electacta.2007.03.003 ↗
39. Organic corrosion inhibitor mixtures for reinforcing steel embedded in carbonated alkali-activated fly ash mortar10.1016/j.conbuildmat.2012.02.078 ↗
40. AEO7 surfactant as an Eco-friendly corrosion inhibitor for carbon steel in HCl solution10.1038/s41598-018-37254-7 ↗
41. The localized corrosion of AI 6XXX alloys10.1007/s11837-001-0087-7 ↗
42. Effectiveness of O-bridged cationic gemini surfactants as corrosion inhibitors for stainless steel in 3M HCl: experimental and theoretical studies10.1016/j.molliq.2017.11.142 ↗
43. Adsorption and inhibitive properties of some new Mannich bases of Isatin derivatives on corrosion of mild steel in acidic media10.1016/j.corsci.2010.01.015 ↗
44. Time- and temperature-dependence of the anticorrosion effect of sodium sulfide on Q235 steel for post-combustion CO2 capture system10.1016/j.rechem.2022.100300 ↗
45. Effect of H2S on Fe corrosion in CO2-saturated brine10.1007/s10853-009-3854-4 ↗
46. Microbiologically-influenced corrosion of the electroless deposited NiP-TiNi – Coating10.1016/j.arabjc.2021.103445 ↗
47. Initiation and growth of mesa corrosion attack during CO2 corrosion of carbon steel
48. Oxygen reduction on sulphide minerals: Part I. Kinetics and mechanism at rotated pyrite electrodes10.1016/S0022-0728(75)80327-5 ↗
49. Reliability of electrochemical techniques for determining corrosion rates on carbon steel in sulfide media10.5006/1.3278388 ↗
50. Crolet · 1991 · vol. 22
51. Local corrosion processes in the presence of sulphate-reducing bacteria: measurements under biofilms10.1016/0010-938X(93)90205-U ↗
52. Assessment of corrosion under iron sulfide deposits and CO2/H2S conditions10.5006/0441 ↗
53. Prediction of uniform CO2 corrosion of mild steel under inert solid deposits
54. Development of a test protocol for the evaluation of under deposit corrosion inhibitors in large diameter crude oil pipelines
55. An in situ synchrotron radiation grazing incidence X-ray diffraction study of carbon dioxide corrosion10.1149/1.2007227 ↗
56. In situ synchrotron X-ray diffraction study of surface scale formation during CO2 corrosion of carbon steel at temperatures up to 90°C10.1016/j.corsci.2010.05.025 ↗
57. Huang · 2013
58. A review on under-deposit corrosion of pipelines in oil and gas fields: testing methods, corrosion mechanisms and mitigation strategies10.1016/j.corcom.2022.03.007 ↗
59. Novel multi-electrode test method for evaluating inhibition of under deposit corrosion-Part 1: sweet conditions
60. Performance of corrosion inhibitor with sand deposit in CO2 environment
61. Comparison of mono- to diphosphate ester ratio in inhibitor formulations for mitigation of under deposit corrosion10.5006/1786 ↗
62. CO2 corrosion and the inhibitor effectiveness under sand deposits in offshore pipeline
63. Understanding the propagation of non-uniform corrosion on a steel surface covered by marine sand10.5006/3278 ↗
64. Corrosion of iron in an H2S-CO2-H2O system: influence of (single iron) crystal orientation on hydrogen penetration rate10.5006/0010-9312-20.7.235t ↗
65. Corrosion at higher H2S concentrations and moderate temperatures
66. The influence of hydrogen sulfide on corrosion of iron under different conditions10.1016/S0010-938X(00)00003-2 ↗
67. A study on chloride-induced depassivation of mild steel in simulated concrete pore solution10.1016/S0008-8846(02)00895-5 ↗
68. Electrochemical characterization of mild steel in alkaline solutions simulating concrete environment10.1016/j.jelechem.2014.10.023 ↗
69. Carbon steel passivity examined in alkaline solutions: the effect of chloride and nitrite ions10.1016/j.electacta.2008.01.091 ↗
70. Environmental factors affecting the critical pitting potential of aluminum10.1149/1.2412167 ↗
71. The performance of a surface-applied corrosion inhibitor for the carbon steel in saturated Ca(OH)2 solutions10.1016/j.cemconres.2013.10.005 ↗
72. A comparative study on corrosion behavior of rebar in concrete with fatty acid additive as phase change material10.1016/j.conbuildmat.2017.03.165 ↗
73. Corrosion 13
74. Inhibition of under-deposit corrosion of carbon steel by Thiobenzamide10.1149/2.078309jes ↗
75. Corrosion of pipeline steel X-60 under field-collected sludge deposit in a simulated sour environment10.5006/1237 ↗
76. Mitigation of under-deposit and weldment corrosion with an environmentally acceptable corrosion inhibitor
77. Diffusion behaviors of three thioureidoimidazo-line corrosion inhibitors in a simulated sediment layer10.20964/2018.06.72 ↗
78. Evaluation of corrosion inhibition at sand-deposited carbon steel in CO2-saturated brine10.1016/j.corsci.2013.03.013 ↗
79. CO2 corrosion inhibitors performance at deposit covered carbon steel and their adsorption on different deposits10.5006/3223 ↗
80. Yu · 2014
81. Inhibition performance of benzimidazole derivatives with different heteroatoms on the under-deposit corrosion of carbon steel in CO2-saturated solution10.1016/j.corsci.2021.109841 ↗
82. Corrosion inhibition and adsorption features of novel bioactive cationic surfactants bearing benzenesulphonamide on C1018-steel under sweet conditions: combined modeling and experimental approaches10.1016/j.molliq.2020.114564 ↗
83. Sour corrosion of C1018 carbon steel and its inhibition by 1–benzylimidazole: electrochemical, SEM, FTIR and computational assessment10.1080/01694243.2021.1938474 ↗
84. H2S corrosion inhibition of carbon steel by a coconut-modified imidazoline
85. Miksic · 2009
86. The solubility of iron sulphides in synthetic and natural waters at ambient temperature10.1007/BF00877139 ↗
87. Surface crystal chemistry of phyllosilicates using X-ray photoelectron spectroscopy: a review10.1346/CCMN.2016.064033 ↗
88. Initiation and development stages of steel corrosion in wet H2S environments10.1016/j.corsci.2015.01.024 ↗