journal article·2024-03Open access

Study on the microstructure and mechanical properties of Mg–Al–Li–Zn–Ti multi-component alloy

Chunyu Ma, Chenghao Hou, Xiaohui Zhang, Tongyu Liu, Nan Zhou, Kaihong Zheng

Abstract

A novel magnesium-based multi-principal element alloy with the chemical formula Mg54Al22Li11Zn11Ti2 was prepared using the vacuum induction melting method and subsequently extruded at 350 °C. The phase composition of the alloy in its as-cast state and the microstructural changes after extrusion were investigated using various analytical techniques, including SEM, EBSD, EPMA, and TEM. The presented outcomes showed that the as-cast alloy exhibited lattice distortion and fine grain with segregation, while the average grain size decreased significantly and the second phase became more dispersed after extrusion. The mechanical properties of both the as-cast and extruded alloys, including microhardness, tensile strength, compressive strength, and wear characteristics, were evaluated. The extruded alloy demonstrated significant improvements in mechanical properties compared to the as-cast alloy, with a compressive strength of up to 460 MPa, which can be attributed to both fine grain and precipitation strengthening. Both the as-cast and extruded alloys exhibited high hardness due to the accumulation of local dislocations caused by the interlaced precipitation of sub-grains during the super-solid solution state in the as-cast condition. The hardness enhancement in the extruded state resulted from grain refinement induced by DRX. Furthermore, wear tests revealed that the extruded alloy, characterized by smaller second phase sizes, exhibited excellent wear resistance, with wear failure occurring in the form of abrasive and oxidative wear in both the cast and extruded alloys.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Magnesium Alloys: Properties and Applications · Aluminum Alloys Composites Properties · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (58)

Show source-provided references
1. Recent research and developments on wrought magnesium alloys10.1016/j.jma.2017.09.001 ↗
2. Research for a “new age of magnesium” in the automotive industry10.1016/S0924-0136(01)00780-4 ↗
3. Magnesium: current and potential automotive applications10.1007/BF02701073 ↗
4. Recent development in aluminium alloys for the automotive industry10.1016/S0921-5093(99)00653-X ↗
5. Study of the degradation behavior and the biocompatibility of Mg–0.8 Ca alloy for orthopedic implant applications10.1016/j.jma.2019.02.007 ↗
6. What is going on in magnesium alloys?10.1016/j.jmst.2017.07.019 ↗
7. Sliding friction and wear of magnesium alloy AZ91D produced by two different methods10.1016/S0301-679X(00)00108-0 ↗
8. Microstructures, mechanical properties and corrosion behaviors of Mg–Y–Zn–Zr alloys with specific Y/Zn mole ratios10.1016/j.jallcom.2014.10.177 ↗
9. Constitutive model for AZ31 magnesium alloy based on isothermal compression test10.1179/1743284713Y.0000000341 ↗
10. Corrosion behavior of ECAP-processed AM90 magnesium alloy10.1007/s13369-018-3203-5 ↗
11. Wear properties of ECAP-processed AM80 magnesium alloy10.1007/s11665-017-2764-x ↗
12. Investigation of dry sliding wear properties of multi-directional forged Mg–Zn alloys10.1016/j.jma.2019.05.008 ↗
13. Kinetics in Mg-based hydrogen storage materials: enhancement and mechanism10.1016/j.jma.2018.12.001 ↗
14. Improving ductility of a Mg alloy via non-basal< a> slip induced by Ca addition10.1016/j.ijplas.2019.04.020 ↗
15. Study on microstructure and strengthening mechanism of AZ91-Y magnesium alloy. Mater Res Express
16. Strengthening mechanisms of magnesium-lithium based alloys and composites10.1155/2016/1078187 ↗
17. Microstructural evolution and mechanical strengthening mechanism of Mg-3Sn-1Mn-1La alloy after heat treatments10.1016/j.msea.2018.07.083 ↗
18. Nanostructured high‐entropy alloys with multiple principal elements: novel alloy design concepts and outcomes10.1002/adem.200300567 ↗
19. Solid‐solution phase formation rules for multi‐component alloys10.1002/adem.200700240 ↗
20. Microstructural development in equiatomic multicomponent alloys10.1016/j.msea.2003.10.257 ↗
21. High-entropy alloys: a critical assessment of their founding principles and future prospects10.1080/09506608.2016.1180020 ↗
22. Recent progress in high entropy alloys10.3166/acsm.31.633-648 ↗
23. Anomalous decrease in X-ray diffraction intensities of Cu–Ni–Al–Co–Cr–Fe–Si alloy systems with multi-principal elements10.1016/j.matchemphys.2007.01.003 ↗
24. Physical metallurgy of high-entropy alloys10.1007/s11837-015-1583-5 ↗
25. High-entropy alloys: a critical review10.1080/21663831.2014.912690 ↗
26. A novel low-density, high-hardness, high-entropy alloy with close-packed single-phase nanocrystalline structures10.1080/21663831.2014.985855 ↗
27. Microstructures and mechanical properties of AlxCrFeNiTi0. 25 alloys10.1016/j.jallcom.2014.09.073 ↗
28. Structure and mechanical properties of the AlCrxNbTiV (x= 0, 0.5, 1, 1.5) high entropy alloys10.1016/j.jallcom.2015.08.224 ↗
29. Study to microstructure and mechanical properties of Mg containing high entropy alloys10.4028/www.scientific.net/MSF.650.265 ↗
30. A low-Cost lightweight entropic alloy with high strength10.1007/s11665-018-3720-0 ↗
31. Novel Ultralight-weight complex concentrated alloys with high strength10.3390/ma12071136 ↗
32. Criteria for predicting the formation of single-phase high-entropy alloys
33. Electronic and thermodynamic criteria for the occurrence of high entropy alloys in metallic systems10.1016/j.actamat.2014.04.033 ↗
34. Design of light-weight high-entropy alloys10.3390/e18090333 ↗
35. Solidification microstructure of ZA102, ZA104 and ZA106 magnesium alloys and its effect on creep deformation10.1179/cmq.2000.39.4.503 ↗
36. Simultaneously improving mechanical and anti-corrosion properties of extruded Mg-Al dilute alloy via trace Er addition10.1016/j.jmst.2022.12.014 ↗
37. Toward the development of Mg alloys with simultaneously improved strength and ductility by refining grain size via the deformation process10.1007/s12613-020-2190-1 ↗
38. Developing a low-alloyed fine-grained Mg alloy with high strength-ductility based on dislocation evolution and grain boundary segregation10.1016/j.scriptamat.2021.114414 ↗
39. Lightweight Medium entropy magnesium alloy with exceptional compressive strength and ductility combination10.1007/s11665-021-05478-w ↗
40. Influence of Ce addition on microstructure and mechanical properties of high pressure die cast AM50 magnesium alloy10.1016/S1003-6326(13)62430-9 ↗
41. Effects of Ti3C2Tx size on mechanical properties of Ti3C2Tx/ZK61 alloys10.1016/j.ceramint.2022.10.068 ↗
42. Microstructure and mechanical properties of AM60 magnesium alloy processed by a new severe plastic deformation technique10.1007/s12540-020-00889-1 ↗
43. Processing, microstructure and mechanical characterization of a new magnesium based multicomponent alloy10.1016/j.matpr.2019.12.349 ↗
44. Achieving high strength in commercial Mg cast alloys through large strain rolling10.1016/j.matlet.2005.04.061 ↗
45. The effects of second phase on microstructure and properties of degradable as-cast Mg-Zn-Ca alloy for intrauterine device (IUD) applications10.20964/2022.08.39 ↗
46. Effects of extrusion and heat treatment on the mechanical properties and biocorrosion behaviors of a Mg–Nd–Zn–Zr alloy10.1016/j.jmbbm.2011.05.026 ↗
47. Investigation of Mg–x Li–Zn alloys for potential application of biodegradable bone implant materials10.1007/s10856-021-06516-8 ↗
48. Development and biomaterial characterization of Mg-Li-Zn-Ca alloys
49. In vitro and in vivo assessment of squeeze-cast Mg-Zn-Ca-Mn alloys for biomedical applications10.1016/j.actbio.2022.07.040 ↗
50. Modeling the precipitation processes and strengthening mechanisms in a Mg-Al-(Zn) AZ91 alloy10.1007/s11661-005-0330-x ↗
51. Influence of grain size and texture on Hall-Petch relationship for a magnesium alloy10.1016/j.scriptamat.2011.08.028 ↗
52. Influence of Zn on the microstructure and mechanical properties of Mg-Gd-Zr alloy10.1016/j.msea.2022.143136 ↗
53. Interactions between basal dislocations and β1′ precipitates in Mg-4Zn alloy: mechanisms and strengthening10.1016/j.actamat.2020.01.028 ↗
54. Influence of initial microstructure on the strengthening effect of extruded Mg–8Sn–4Zn–2Al alloys10.1007/s40195-017-0673-5 ↗
55. Effect of Sn content on strain hardening behavior of as-extruded Mg-Sn alloys10.1016/j.msea.2017.12.074 ↗
56. Strain hardening of as-extruded Mg-xZn (x= 1, 2, 3 and 4 wt%) alloys10.1016/j.jmst.2018.09.015 ↗
57. Microstructural evolution and strengthening of AM90 magnesium alloy processed by ECAP10.1007/s13369-017-2574-3 ↗
58. Solid solution and precipitation strengthening effects in basal slip, extension twinning and pyramidal slip in Mg-Zn alloys10.1016/j.actamat.2021.117374 ↗