journal article·2025-07Open access

Study on the salt-corrosion and oxidation role mechanism of Ni-based single crystal superalloy in the long-term hot corrosion environment

Y.Q. Yang, L. Yang, Y.C. Zhao, H.Q. Pei, Z.X. Wen, Y.C. Zhou

Abstract

Hot corrosion is one of the key factors affecting the long-term service of Ni-based single crystal superalloys. In this paper, the long-term hot corrosion test of a second-generation Ni-based single crystal superalloy was carried out in a high-temperature furnace. Then, the microstructure morphology and composition of the alloy were analyzed by a series of characterization methods, which clarified the evolution process of the corrosion/oxidation layer and the attack of the corrosive salt. Meanwhile, EBSD analysis revealed that recrystallization was formed on the γ′-depleted layer, accelerating the cross-section evolution of the alloy. Finally, the effects of Al element content and salt amount on the hot corrosion behavior were investigated separately by the ingenious design of two groups of control tests, and the long-term hot corrosion behavior of Ni-based single crystal superalloys is investigated by decomposition into salt-corrosion damage and alloy-oxidation protection behavior for the first time. Further, the salt corrosion-oxidation role mechanism of Ni-based single crystal superalloy in the long-term hot corrosion environment was revealed.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · High Temperature Alloys and Creep · Metallurgical Processes and Thermodynamics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (49)

Show source-provided references
1. A review on molten sulfate salts induced hot corrosion10.1016/j.jmst.2021.03.013 ↗
2. Pontika · 2023 · 23
3. Hot corrosion failure in the first stage nozzle of a gas turbine engine10.1016/j.engfailanal.2015.11.057 ↗
4. influence of two different salt mixture combinations of Na2SO4-NaCl-NaVO3 on hot corrosion behavior of Ni-base superalloy Nimonic263 at 800 °C10.1007/s11665-019-3866-4 ↗
5. Study on the hot corrosion-creep failure mechanism of Ni-based single crystal superalloy considering the stress dependence10.1016/j.msea.2024.146350 ↗
6. An investigation of oxidation/hot corrosion-creep interaction at 800°C in a Ni-base superalloy coated with salt mixture deposits of Na2SO4-NaCl-NaVO310.1016/j.corsci.2018.11.029 ↗
7. Interaction of hot corrosion fatigue and load dwell periods on a nickel-base single crystal superalloy10.1016/j.ijfatigue.2018.07.029 ↗
8. Fatigue durability of a single-crystal nickel-based superalloy with prior corrosion
9. Influence of hot corrosion on thermal fatigue behavior of Ni-based single crystal superalloy: invisible and accelerated crack10.1016/j.ijfatigue.2024.108162 ↗
10. Hot corrosion-creep interaction in IN718 under simulated marine environment: introducing strain-associated-time (SAT) plots for comprehensive understanding10.1016/j.corsci.2021.109667 ↗
11. Low-temperature hot corrosion effects on the low-cycle fatigue lifetime and cracking behaviors of a powder metallurgy Ni-based superalloy10.1016/j.ijfatigue.2018.06.035 ↗
12. Fatigue behaviors of a nickel-based superalloy after hot-corrosion: experiments and peridynamic simulations10.1016/j.ijfatigue.2023.108070 ↗
13. Failure analysis of a first stage IN738 gas turbine blade tip cracking in a thermal power plant10.1016/j.csefa.2016.11.002 ↗
14. Corrosion failures in gas turbine hot components10.1007/s11668-012-9571-3 ↗
15. Hot corrosion failure in the first stage nozzle ofa gas turbine engine10.1016/j.engfailanal.2015.11.057 ↗
16. Hot corrosion of shipboard gas turbine blades10.1007/s11085-020-09990-7 ↗
17. A review of composition evolution in Ni-based single crystal superalloys10.1016/j.jmst.2020.01.026 ↗
18. Investigation on the hot corrosion behavior of a single crystal Ni-based superalloy in molten Na2SO4+K2SO4 salts improved by different preoxidation treatments10.1016/j.corsci.2023.111377 ↗
19. Effect of surface treatment and crystal orientation on hot corrosion of a Ni-based single-crystal superalloy10.1016/j.corsci.2020.108472 ↗
20. High-temperature oxidation and hot corrosion of Ni-based single crystal superalloy in the incubation stage10.1016/j.corsci.2023.111026 ↗
21. Hot corrosion mechanism of laser metal deposited Ni-based single crystal superalloy under fuel gas atmosphere10.1016/j.surfcoat.2023.130057 ↗
22. Influence of Cr content on hot corrosion and a special tube sealing test of single crystal nickel base superalloy10.1016/j.corsci.2019.05.001 ↗
23. Role of tantalum in the hot corrosion of a Ni-base single crystal superalloy10.1016/j.corsci.2015.05.066 ↗
24. Long-term hot corrosion behavior of boiler tube alloys in waste-to-energy plants10.1007/s11085-016-9627-y ↗
25. Long-term corrosion behavior of FeCr(Al, Ni) alloys in O2 + H2O with KCl (s) at 600°C: microstructural evolution after breakaway oxidation10.1016/j.corsci.2023.111654 ↗
26. Hot corrosion of Fe and Ni-based alloys in Wase-to-energy environment at 850°C10.1016/j.engfailanal.2021.105964 ↗
27. High temperature oxidation and hot corrosion behaviors of Ti2AlNb alloy at 923 K and 1023 K10.1016/j.corsci.2021.109336 ↗
28. The long-term corrosion behavior of FeCrAl(Si) alloys after breakaway oxidation at 600°C10.1016/j.corsci.2023.111155 ↗
29. High temperature hot corrosion of single crystal superalloy DD6 Subject to varying amounts of sodium salt deposited
30. Effect of pre-hot salt corrosion on hot salt corrosion fatigue behavior of the TC11 titanium alloy at 500 °C10.1016/j.ijfatigue.2022.107055 ↗
31. Synergistic effect of multiple molten salts on hot corrosion behaviour of Ni-based single crystal superalloy10.1016/j.corsci.2022.110381 ↗
32. Effect of Al content on the high-temperature oxidation of Co-20Cr-(5, 10) Al oxide dispersion strengthened superalloys10.1016/j.corsci.2017.01.015 ↗
33. Effect of rare earth Y on oxidation behavior of NiAl-Al2O310.1016/S1003-6326(11)61607-5 ↗
34. Effect of θ-alumina formation on the growth kinetics of alumina-forming superalloys10.1007/BF01048641 ↗
35. Long-term oxidation behavior and mechanism of DD6 Ni-based single crystal superalloy at 1050 °C and 1100 °C in air10.1016/j.jallcom.2017.02.031 ↗
36. AlxCoCrFeNi high entropy alloys with superior hot corrosion resistance to Na2SO4 + 25% NaCl at 900°C10.1016/j.corsci.2021.109479 ↗
37. Thermodynamics of gas phase chromium species: the chromium chlorides, oxychlorides, fluorides, oxyfluorides, hydroxides, oxyhydroxides, mixed oxyfluorochlorohydroxides, and volatility calculations in waste incineration processes10.1016/0010-2180(94)00215-E ↗
38. Hot corrosion behavior of NiCoCrAlYSi laser cladding coating modified using high-current pulsed electron beam in different corrosive salt environments10.1016/j.matchar.2023.113565 ↗
39. In-situ XRD investigations of FeAl intermetallic phase-based alloy oxidation
40. The effect of tensile stress on oxidation behavior of nickel-base single crystal superalloy10.1016/j.corsci.2021.109737 ↗
41. Microstructural evolution and mechanical properties of NiCrAlYSi+NiAl/cBN abrasive coating coated superalloy during cyclic oxidation10.1016/j.jmst.2020.08.043 ↗
42. Oxidation behaviors and compressive strength evolution of DD6 Ni-based single-crystal superalloy at 1100°C10.1016/j.corsci.2022.110684 ↗
43. Microstructural evolution of the interface between NiCrAlY coating and superalloy during isothermal oxidation10.1016/j.matdes.2015.05.014 ↗
44. Environmental effect on mechanical properties of a gamma-prime strengthened nickel-based alloy: effect of the surface oxidation and formation of gamma-prime free zones10.1016/j.msea.2019.03.013 ↗
45. Low cycle fatigue of a single crystal CoNi-base superalloy10.1016/j.msea.2021.142007 ↗
46. Localized recrystallization during creep in nickel-based superalloys GTD444 and René N510.1016/j.actamat.2014.03.052 ↗
47. Kinetics of creep damage accumulation induced by a room-temperature plastic deformation introduced during processing of AM1 Ni-based single crystal superalloy10.1016/j.msea.2020.139571 ↗
48. Oxidation of nickel-based single-crystal superalloys for industrial gas turbine applications10.1016/j.actamat.2010.09.027 ↗
49. Oxidation behaviour and microstructure degeneration of cast Ni-based superalloy M951 at 900°C10.1016/j.apsusc.2019.02.150 ↗