Competitive and collaborative relationship between Al–3P and TiB2 nanoparticles in the microstructure manipulation of eutectic Al–Si alloys
Source abstract
Abstract
In this work, the synergistic effects of the modifier Al–3P master alloy and nano-TiB 2 ceramic particles on the microstructure and mechanical performance of cast eutectic Al–Si alloys were investigated. Results showed that AlP and nano-TiB 2 particles served as efficient heterogeneous nucleation sites of Si and α-Al, respectively. Incorporated TiB 2 and Al–3P performed the best manipulating potency on the solidification microstructure of Al–Si alloys than separately added, primary Si was significantly refined and the transition of Al–Si eutectic was promoted. Room-temperature and high-temperature tensile strength were also markedly enhanced, the yield strength, ultimate tensile strength and fracture strain of eutectic Al–Si alloys manipulated by Al–3P + nano-TiB 2 particles were increased by 36.4%, 31.7% and 32.1% at 250 °C and 60.0%, 42.0% and 50.9% at 300 °C, respectively, in comparison to the unmodified alloys. The enhanced high-temperature strength was attributed to the refinement of primary Si and α-Al, which was achieved through the synergistic effects of nano-TiB 2 particles and Al–3P. Then the grain boundary density increased, with finer eutectic Si and nanoparticles being effectively pinned at the grain boundaries, thereby boosting the mechanical performance. This study provides theoretical research and experimental basis for the development and application of heat-resistant aluminum alloys.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (68)
Show source-provided references
1. In situ nanocrystals manipulate solidification behavior and microstructures of hypereutectic Al-Si alloys by Zr-based amorphous alloys10.1016/j.jmrt.2020.02.091 ↗
2. Effectively refining Al-10Si alloy via Al-Ti-Nb-B refiner with Nb2O510.1016/j.jmst.2023.08.029 ↗
3. Microstructure, tensile properties and creep behavior of Al-12Si-3.5Cu-2Ni-0.8Mg alloy produced by different casting technologies10.1016/j.jmst.2017.06.011 ↗
4. Highly ductile hypereutectic Al-Si alloys fabricated by selective laser melting10.1016/j.jmst.2021.07.050 ↗
5. Influence of high pressure and manganese addition on Fe-rich phases and mechanical properties of hypereutectic Al−Si alloy with rheo-squeeze casting10.1016/S1003-6326(19)64934-4 ↗
6. Development and applications of aluminum alloys for aerospace industry10.1016/j.jmrt.2023.09.274 ↗
7. Effect of Ni content on the wear behavior of Al-Si-Cu-Mg-Ni/SiC particles composites10.1007/s12613-023-2701-y ↗
8. Additive manufacturing of magnesium and its alloys: process-formability-microstructure-performance relationship and underlying mechanism10.1088/2631-7990/acf254 ↗
9. Additive manufacturing of heat-resistant aluminum alloys: a review10.1088/2631-7990/ad7f2e ↗
10. Hot deformation behavior and microstructure evolution of Be/2024Al composites10.1007/s12613-023-2662-1 ↗
11. An Al-Al interpenetrating-phase composite by 3D printing and hot extrusion10.1007/s12613-022-2543-z ↗
12. Drawing–upsetting–extrusion–clinching of high-strength steel and aluminum alloy10.1007/s42243-023-00917-5 ↗
13. Effect of V on high-temperature mechanical properties of Al–5Cu–1.5Ni alloy10.1007/s42243-023-01115-z ↗
14. Effects of prior ECAP process on the dynamic impact behaviors of hypereutectic Al-Si alloy10.1016/j.msea.2020.139902 ↗
15. Comparison of in situ nanocrystals, Sr and nanocrystals + Sr manipulating microstructures and mechanical properties of eutectic Al–Si13.0–Cu5.0–(Ni2.0)–Mg0.6 alloy10.1016/j.jmrt.2020.05.061 ↗
16. Solidification microstructure manipulation mechanism of hypoeutectic and hypereutectic Al–Si alloys controlled by trace in-situ nano-Fe2B and nano-Fe3Si10.1016/j.jmrt.2022.10.142 ↗
17. Effect and its mechanism of fixed-ratio and incremented 3Be-Sb complex modifier on microstructures and properties of hypereutectic Al-Si-Mg alloy10.1016/j.jallcom.2022.167478 ↗
18. Al2O3 nanoparticles induced simultaneous refinement and modification of primary and eutectic Si particles in hypereutectic Al–20Si alloy10.1016/j.msea.2012.01.131 ↗
19. Influence of rheo-diecasting processing parameters on microstructure and mechanical properties of hypereutectic Al–30%Si alloy10.1016/S1003-6326(17)60147-X ↗
20. Improved mechanical and frictional properties of hypereutectic Al-Si alloy by modifying Si phase with La addition
21. Investigation on the elevated-temperature tribological behaviors and mechanism of Al-Cu-Mg composites reinforced by in-situ size-tunable TiB2-TiC particles10.1016/j.triboint.2022.107943 ↗
22. Effect of Al–P–Ti–TiC–Nd2O3 modifier on the microstructure and mechanical properties of hypereutectic Al–20wt.%Si alloy10.1016/j.msea.2006.10.114 ↗
23. Significantly enhanced fatigue resistance and mechanisms of hypoeutectic Al-Si composite calibrated using trace in-situ nanocrystals10.1016/j.compositesb.2023.111138 ↗
24. Review of Sc microalloying effects in Al-Cu alloys10.1007/s12613-024-2841-8 ↗
25. Cluster formation at the Si/liquid interface in Sr and Na modified Al–Si alloys10.1016/j.scriptamat.2016.02.018 ↗
26. Combining Sr and Na additions in hypoeutectic Al–Si foundry alloys10.1016/j.msea.2005.03.091 ↗
27. Effect of Sr modification on microstructure and thermal conductivity of hypoeutectic Al−Si alloys10.1016/S1003-6326(20)65428-0 ↗
28. Microstructure, mechanical properties and corrosion behavior of Al–Si–Cu–Zn–X (X=Bi, Sb, Sr) die cast alloy10.1016/S1003-6326(16)64085-2 ↗
29. Comparing the roles of Sb and Bi on microstructures and application properties of the Al-15% Si alloy10.1016/j.jallcom.2021.160343 ↗
30. Effects of cerium and phosphorus on microstructures and properties of hypereutectic Al-21%Si alloy10.1016/S1002-0721(12)60313-5 ↗
31. Impact of P and Sr on solidification sequence and morphology of hypoeutectic Al–Si alloys: combined thermodynamic computation and phase-field simulation10.1016/j.actamat.2015.06.056 ↗
32. Morphologically templated nucleation of primary Si on AlP in hypereutectic Al-Si alloys10.1016/j.jmst.2021.06.009 ↗
33. The modification of electroless deposited Ni–P master alloy for hypereutectic Al–Si alloy10.1016/j.jallcom.2010.02.012 ↗
34. Effect of P and Sr complex modification on Si phase in hypereutectic Al–30Si alloys10.1016/j.matdes.2012.12.054 ↗
35. Insight into solidification microstructure control by trace TiCN–TiB2 particles for yielding fine-tuned nanoprecipitates in a hypoeutectic Al–Si–Mg alloy10.1016/j.msea.2021.142093 ↗
36. Experimental characterization and 3D sharp-interface model simulation of grain refinement during solidification of nano-TiCN/Al–7Si composites10.1016/j.msea.2024.146662 ↗
37. Microstructural characterizations and mechanical properties of NbB2 and VB particulate-reinforced eutectic Al-12.6 wt% Si composites via powder metallurgy method10.1016/j.apt.2018.05.013 ↗
38. Simultaneous refinement of α-Al and modification of Si in Al–Si alloy achieved via the addition of Y and Zr10.1016/j.jmrt.2024.03.219 ↗
39. Insight into Si poisoning on grain refinement of Al-Si/Al-5Ti-B system10.1016/j.actamat.2020.01.039 ↗
40. A mechanism for the poisoning effect of silicon on the grain refinement of Al–Si alloys10.1016/j.actamat.2006.09.046 ↗
41. An anti Si/Zr-poisoning strategy of Al grain refinement by the evolving effect of doped complex10.1016/j.actamat.2023.118812 ↗
42. Enhancing strength-ductility synergy and mechanisms of Al-based composites by size-tunable in-situ TiB2 particles with specific spatial distribution10.1016/j.compositesb.2021.108912 ↗
43. Synergistic optimization in solidification microstructure and mechanical performance of novel (TiCxNy − TiB2)p/Al nanocomposites: design, tuning and mechanism10.1016/j.compositesa.2022.106843 ↗
44. Interface formation and bonding control in high-volume-fraction (TiC+TiB2)/Al composites and their roles in enhancing properties10.1016/j.compositesb.2021.108605 ↗
45. Unprecedented enhancement in strength-plasticity synergy of (TiC+Al6MoTi+Mo)/Al cermet by multiple length-scale microstructure stimulated synergistic deformation10.1016/j.compositesb.2021.109265 ↗
46. Wetting of TiC by molten Al at 1123–1323K10.1016/j.actamat.2010.11.055 ↗
47. Microstructure evolution and mechanical properties of Cu-Ni-Ti transient liquid phase bonding for SiC-GH3536 joints
48. Wetting of Al2O3 by Cu-xTi alloys at 1373 K10.1016/j.jeurceramsoc.2024.01.025 ↗
49. Review on laser directed energy deposited aluminum alloys10.1088/2631-7990/ad16bb ↗
50. Ceramic particles reinforced copper matrix composites manufactured by advanced powder metallurgy: preparation, performance, and mechanisms10.1088/2631-7990/acdb0b ↗
51. Exploring the potential of FSW-ed Al–Zn–Mg–Cu-based composite reinforced by trace in-situ nanoparticles in manufacturing workpiece with customizable size and high mechanical performances10.1016/j.compositesb.2022.110425 ↗
52. Study on the oxidation mechanism of Al-SiC composite at elevated temperature10.1007/s12613-023-2778-3 ↗
53. Review on laser directed energy deposited aluminum alloys10.1088/2631-7990/ad16bb ↗
54. Comprehensive regulation of mechanical properties and thermal conductivity of Al-Si-Fe alloys through the mixed-additive (Sr and TiB2) strategy10.1016/j.jallcom.2024.175850 ↗
55. Achieving simultaneous improvement in strength and ductility in Al-Si-Mg-Ce alloy through synergistic morphology modification of eutectic (Si) and Al2Si2Ce phases by Sr addition10.1016/j.jmrt.2024.09.108 ↗
56. Processing, multiscale microstructure refinement and mechanical property enhancement of hypoeutectic Al–Si alloys via in situ bimodal-sized TiB2 particles10.1016/j.msea.2020.139081 ↗
57. Edge-to-edge matching and its applications: Part I. Application to the simple HCP/BCC system10.1016/j.actamat.2004.11.007 ↗
58. Crystallographic study of grain refinement in aluminum alloys using the edge-to-edge matching model10.1016/j.actamat.2004.11.037 ↗
59. Heterogeneous nucleating role of TiB2 or AlP/TiB2 coupled compounds on primary Mg2Si in Al–Mg–Si alloys10.1016/j.msea.2008.07.034 ↗
60. A new nucleation mechanism of primary Si by peritectic-like coupling of AlP and TiB2 in near eutectic Al–Si alloy10.1016/j.jallcom.2006.06.005 ↗
61. Absorbing formation mechanism of AlP on TiB2 substrate and their application as high-efficiency nucleating agent in Al-45Si alloy10.1016/j.jallcom.2016.09.274 ↗
62. Microstructure refinement and strengthening mechanisms of bimodal-sized and dual-phased (TiCn-Al3Tim)/Al hybrid composites assisted ultrasonic vibration10.1016/j.jallcom.2019.02.315 ↗
63. Hybrid in-situ hot rolling and wire arc additive manufacturing of Al-Si alloy: microstructure, mechanical properties and strengthening mechanism10.1016/j.jmapro.2024.07.110 ↗
64. An overview of additively manufactured metal matrix composites: preparation, performance, and challenge10.1088/2631-7990/ad54a4 ↗
65. A new approach for improving the elevated-temperature strength and ductility of Al–Cu–Mg–Si alloys with minor amounts of dual-phased submicron/nanosized TiB2–TiC particles10.1016/j.msea.2019.138266 ↗
66. Cavitation-resistant intergranular precipitates enhance creep performance of θ′-strengthened Al-Cu based alloys10.1016/j.actamat.2022.117788 ↗
67. Microstructure and mechanical properties of an in-situ TiB2/Al-Zn-Mg-Cu-Zr composite fabricated by Melt-SHS process10.1016/j.msea.2018.02.025 ↗
68. TiB2 reinforced aluminum based in situ composites fabricated by stir casting10.1016/j.msea.2014.12.033 ↗