Effect of rare earth La on hydrogen diffusion and hydrogen embrittlement susceptibility of 42CrMo martensitic steel
Source abstract
Abstract
The effect of rare earth (RE) La on hydrogen diffusion and hydrogen embrittlement (HE) susceptibility of 42CrMo martensitic steel was studied by electrochemical hydrogen permeation test, hydrogen microprint technique (HMT) and slow strain rate tensile (SSRT). The results show that La modifies original Al 2 O 3 and MnS inclusions and generates numerous well-dispersed RE inclusions. Individual RE inclusions with lower stress distribution exhibit a reduced propensity to promote HE and higher hydrogen trapping capacity than Al 2 O 3 and MnS. Additionally, the addition of RE refines the grain structure and increases the number of high angle grain boundaries (HAGBs), effectively suppressing the propagation of hydrogen induced cracks. Compared to non-RE steel, the hydrogen diffusion coefficient of RE steel is reduced by up to 19.1%. As La content increases from 0 wt% to 0.011 wt% and 0.015 wt%, HE susceptibility of test steel decreases initially and then increases. Consequently, the appropriate addition of La can effectively impede hydrogen diffusion, improve hydrogen trapping efficiency and reduce HE susceptibility in martensitic steel.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Welding Techniques and Residual Stresses · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (64)
Show source-provided references
1. Hydrogen degradation of a boron-bearing steel with 1050 and 1300MPa strength levels10.1016/j.scriptamat.2004.10.023 ↗
2. Alloy and composition dependence of hydrogen embrittlement susceptibility in high-strength steel fasteners
3. Hydrogen embrittlement mechanisms in advanced high strength steel10.1016/j.actamat.2021.117488 ↗
4. Hydrogen trapping and hydrogen embrittlement (HE) susceptibility of X70 grade high-strength, acid-resistant, submarine pipeline steel with Mg treatment10.1016/j.jmrt.2023.03.011 ↗
5. Improving hydrogen induced cracking resistance of high strength acid-resistant submarine pipeline steels via trace-Mg treatment10.1016/j.ijhydene.2022.12.322 ↗
6. A new perspective on hydrogen diffusion and hydrogen embrittlement in low-alloy high strength steel10.1016/j.corsci.2020.108800 ↗
7. Evaluation of hydrogen trapping in high strength steels by thermal desorption spectroscopy10.1016/j.msea.2012.04.078 ↗
8. Analysis of key factors of hydrogen environmental assisted cracking evaluation by small punch test on medium and high strength steels10.1016/j.msea.2017.03.006 ↗
9. Role of Ca treatment in hydrogen induced cracking of hot rolled API pipeline steel in acid sour media10.1007/s12540-013-1008-3 ↗
10. Effect of microstructure and inclusions on hydrogen induced cracking susceptibility and hydrogen trapping efficiency of X120 pipeline steel10.1016/j.msea.2010.07.022 ↗
11. Structures of hydrogen-induced cracks under different hydrogen concentrations for a high strength steel10.1016/j.engfailanal.2021.105587 ↗
12. Effect of hydrogen charging on the mechanical properties of advanced high strength steels10.1016/j.ijhydene.2013.12.190 ↗
13. A micromechanics approach to the study of hydrogen transport and embrittlement10.1016/S0013-7944(00)00126-0 ↗
14. Effect of Ce addition on inclusions and grain structure in gear steel 20CrNiMo10.1002/srin.202000394 ↗
15. Effect of Ce-La on inclusion evolution in Al-killed high strength steel10.1051/metal/2020076 ↗
16. Effect of inclusions modified by rare earth elements (Ce, La) on localized marine corrosion in Q460NH weathering steel10.1016/j.corsci.2017.10.001 ↗
17. Effect of solid-solution rare earth in steel on transformation of super-cooled austenite
18. Study of application of rare earth elements in advanced low alloy steels10.1016/j.jallcom.2007.04.234 ↗
19. Effects of rare earth elements on inclusions and impact toughness of high-carbon chromium bearing steel10.1016/j.jmst.2019.01.015 ↗
20. Effect of vanadium and rare earth microalloying on the hydrogen embrittlement susceptibility of a Fe-18Mn-0.6C TWIP steel studied using the linearly increasing stress test10.1016/j.corsci.2021.109440 ↗
21. Role of rare-earth yttrium in the hydrogen embrittlement of AISI 321 austenitic stainless steel10.1016/j.ijhydene.2022.08.267 ↗
22. Effect of Ce content on the hydrogen induced cracking of X80 pipeline steel10.1016/j.ijhydene.2022.12.331 ↗
23. Influence of surface roughness on consecutively hydrogen absorption cycles in Ti-6Al-4V alloy10.1016/j.ijhydene.2010.07.163 ↗
24. Modelling of roughness effect on hydrogen permeation in a low carbon steel
25. The influence of surface roughness on the hydrogen permeation of type API 5L-X52 steel
26. The mechanism of hydrogen evolution on iron in acid solutions by determination of permeation rates10.1149/1.2426195 ↗
27. Hydrogen transport through annealed and deformed armco iron10.1007/BF02644334 ↗
28. A new analysis of diffusion of hydrogen in iron and ferritic steels
29. Effects of hydrogen-charging on the susceptibility of X100 pipeline steel to hydrogen-induced cracking10.1016/j.ijhydene.2009.09.090 ↗
30. Sequential kinetic analysis of the influences of non-metallic inclusions on hydrogen diffusion and trapping in high-strength pipeline steel with Al-Ti deoxidisation and Mg treatment10.1016/j.corsci.2021.110006 ↗
31. Key factors affecting hydrogen trapping at the inclusions in steels: a combined study using microprint technique and theoretical modeling10.1016/j.corsci.2022.110239 ↗
32. Visualization of diffusive hydrogen in low alloy steel by means of hydrogen microprint technique at elevated temperatures10.2320/matertrans.MRA2008325 ↗
33. Correlation between the microstructure and hydrogen embrittlement resistance in a precipitation-hardened martensitic stainless steel10.1016/j.corsci.2021.109260 ↗
34. Hydrogen diffusion and trapping in A 42CrMo4 quenched and tempered steel: influence of tempering temperature10.1016/j.ijhydene.2020.08.134 ↗
35. Hydrogen trapping on non metallic inclusions in Cr-Mo low alloy steels10.1016/S0010-938X(98)00008-0 ↗
36. Effects of sulfide inclusion on hydrogen transport in steels10.1016/0167-577X(95)00068-2 ↗
37. Effect of MnS inclusions on hydrogen diffusion in steel
38. Effect of submicron-scale MnS inclusions on hydrogen trapping and HIC susceptibility of X70 pipeline steels10.1002/srin.201700566 ↗
39. Effect of retained austenite stability and morphology on the hydrogen embrittlement susceptibility in quenching and partitioning treated steels10.1016/j.msea.2016.02.026 ↗
40. Hydrogen-induced fast fracture in notched 1500 and 1700 MPa class automotive martensitic advanced high-strength steel10.1016/j.corsci.2021.109550 ↗
41. The role of hydrogen in hydrogen embrittlement fracture of lath martensitic steel10.1016/j.actamat.2012.06.040 ↗
42. Effect of cerium on the behavior of inclusions in H13 steel10.1002/srin.201800371 ↗
43. Evolution mechanisms of MgO•Al2O3 inclusions by cerium in spring steel used in fasteners of high-speed railway10.2355/isijinternational.55.970 ↗
44. Evolution mechanism of inclusions in H13 steel with rare earth magnesium alloy addition10.2355/isijinternational.ISIJINT-2019-094 ↗
45. Effect of rare earth-magnesium alloy on inclusion evolution in industrial production of die steel10.1002/srin.201900103 ↗
46. The synergistic action and interplay of hydrogen embrittlement mechanisms in steels and iron: localized plasticity and decohesion10.1016/j.engfracmech.2019.106528 ↗
47. Hydrogen permeation and hydrogen-induced cracking10.1016/B978-0-323-52472-8.00007-1 ↗
48. In-situ characterization of initial marine corrosion induced by rare-earth elements modified inclusions in Zr-Ti deoxidized low-alloy steels10.1016/j.jmrt.2019.11.080 ↗
49. Numerical study of the effect of inclusions on the residual stress distribution in high-strength martensitic steels during cooling10.3390/app9030455 ↗
50. Effect of different microstructural parameters on hydrogen induced cracking in an API X70 pipeline steel10.1007/s12540-017-6691-z ↗
51. Influence of inclusions on initiation of pitting corrosion and stress corrosion cracking of X70 steel in near-neutral pH environment10.1016/j.corsci.2018.11.007 ↗
52. Solution and precipitation hardening in (Ca, Mn) sulfides and selenides10.1007/BF02643479 ↗
53. Juvonen · 2004
54. Structural, phonon, mechanical, optical, and thermodynamic properties of stable β-La2S3 from first-principles calculations10.1016/S1002-0721(17)60910-4 ↗
55. A study on infrared transmission of lanthanum sulfide and oxysulfide in the 2.5-14 μm region10.1016/S0167-577X(97)00163-8 ↗
56. First La2O2S infrared transparent ceramics10.1016/j.jeurceramsoc.2022.12.002 ↗
57. Crystal-lattice parameters and thermal linear-expansion coefficients of ceramics based on doped oxysulfides of rare-earth elements
58. An extensive study of hydrogen-induced cracking susceptibility in an API X60 sour service pipeline steel10.1016/j.ijhydene.2016.01.031 ↗
59. A comparative fracture analysis on as-received and electrochemically hydrogen charged API X60 and API X60SS pipeline steels subjected to tensile testing10.1016/j.engfailanal.2021.105721 ↗
60. In-situ EBSD study of the degradation behavior in a type 316 Austenitic Stainless Steel during plastic deformation10.1177/0309324720984930 ↗
61. Enumeration of the hydrogen-enhanced localized plasticity mechanism for hydrogen embrittlement in structural materials10.1016/j.actamat.2018.12.014 ↗
62. Hydrogen-enhanced localized plasticity - a mechanisem for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
63. The effect of non-metallic inclusion morphology on the hydrogen induced cracking (HIC) resistance of L80 steel10.1016/j.jmrt.2023.03.008 ↗
64. Effect of grain refinement on the hydrogen embrittlement of 304 austenitic stainless steel10.1016/j.jmst.2019.03.043 ↗