Achieving fully-equiaxed fine β-grains in laser-additive-manufactured Sn-free high-temperature titanium alloy designed by cluster formula
Source abstract
Abstract
Conventional high-temperature titanium alloys contain Sn as their essential alloying element. Upon additive manufacturing, these alloys exhibit insufficient mechanical properties due to the presence of coarse β-columnar grains. In this work, Sn-free high-temperature Ti-5.5Al-11.2Zr-4.8Ta-1.6W-0.5Si alloy with fully-equiaxed fine β grains was designed targeted for additive manufacturing on the basis of the composition formula of Ti65 alloy. This alloy shows good additive manufacturability and tensile strengths. Its composition formula satisfy α-{[Al-Ti 12 ](AlTi 2 )} 12 +β-{[(Al-Ti 10.5 Zr 3.5 ](Ta 0.75 W 0.25 Ti 1.5 Si 0.5 )} 5 , featuring equiaxed β grains via Ta replacing Mo/Nb and enhanced additive-manufacturability via Zr replacing Sn. In the as-deposited state, this alloy shows complete equiaxed fine β grains and inner with bimodal basket-weave microstructure, as well as excellent tensile properties (ultimate tensile strength (UTS) of 1312 MPa, yield strength (YS) of 1258 MPa, and elongation of 1.8%). Its 600 °C UTS of 703 MPa, YS of 551 MPa, and elongation of 18%, being comparable to those wrought conventional high-temperature Ti alloys.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Effect of thermal exposure on microstructure and mechanical properties of Ti65 high-temperature titanium alloy deposited by laser direct energy deposition10.1016/j.msea.2024.146757 ↗
2. Effect of heat treatments on tribology property of Ti6Al4V alloy under dry friction
3. Optimization of shape and performance for wire and arc additive manufacturing with in-situ rolling of Ti-6Al-4V ELI alloy10.1016/j.jmrt.2025.02.068 ↗
4. Microstructure and mechanical properties of 2319 aluminum alloy deposited by laser and cold metal transfer hybrid additive manufacturing10.1016/j.jmrt.2023.08.312 ↗
5. Simulation of residual stress and distortion evolution in dual-robot collaborative wire-arc additive manufactured Al-Cu alloys10.1080/17452759.2024.2409390 ↗
6. Influence of thermomechanical processing and heat treatment on microstructure, tensile properties and fracture toughness of Ti-1100-0.1B alloy10.1016/j.jallcom.2013.11.014 ↗
7. Quantitative characterization of lamellar α precipitation behavior of IMI834 Ti-alloy in isothermal and non-isothermal heat treatments10.1016/S1003-6326(21)65785-0 ↗
8. Effect of processing parameters on hot deformation behavior and microstructural evolution during hot compression of as-cast Ti60 titanium alloy10.1016/j.msea.2013.07.086 ↗
9. Precipitates and alloying elements distribution in near α titanium alloy Ti6510.1016/j.jmst.2019.03.018 ↗
10. Effects of W alloying and heating on microstructure and mechanical properties of a PM Ti-6Al-2Sn-4Zr-2Mo-0.1Si alloy for high temperature applications10.1016/j.jallcom.2023.168966 ↗
11. Influences of thermal exposure on the microstructural evolution and subsequent mechanical properties of a near-α high temperature titanium alloy10.1016/j.msea.2020.138934 ↗
12. Metal 3D printing as a disruptive technology for superalloys10.1038/s41467-020-16188-7 ↗
13. Structure and mechanical properties of Ti-6Al-4V alloy after zirconium addition10.1016/j.msea.2012.05.043 ↗
14. A novel magnetic field assisted powder arc additive manufacturing for Ti60 titanium alloy: method, microstructure and mechanical properties
15. Deciphering the transformation pathway in laser powder-bed fusion additive manufacturing of Ti-6Al-4V alloy
16. A high-temperature Ti-6.8Al-6.8Zr-2.3V-2.1Mo-0.7Nb alloy suitable for laser-additive manufacturing10.1016/j.msea.2023.145519 ↗
17. Solidification behavior and grain morphology of laser additive manufacturing titanium alloys10.1016/j.jallcom.2018.11.055 ↗
18. Achieving fully-equiaxed fine β-grains in titanium alloy produced by additive manufacturing10.1080/21663831.2022.2115323 ↗
19. Review of structural models for the compositional interpretation of metallic glasses10.1080/09506608.2019.1638581 ↗
20. Composition formulas of Ti alloys derived by interpreting Ti-6Al-4V10.1007/s11431-020-1812-9 ↗
21. Design of ultra-strong as-cast titanium alloy at 600 °C by using cluster formula10.1007/s40195-024-01778-x ↗
22. A novel soft-magnetic B2-based multiprincipal-element alloy with a uniform distribution of soherent body-centered-cubic nanoprecipitates10.1002/adma.202006723 ↗
23. Developing novel low-density high-entropy superalloys with high strength and superior creep resistance guided by automated machine learning10.1016/j.actamat.2024.120656 ↗
24. Composition design procedures of Ti-based bulk metallic glasses using the cluster-plus-glue-atom model10.1016/j.actamat.2016.03.072 ↗
25. Classification of bulk metallic glasses by atomic size difference, heat of mixing and period of constituent elements and its application to characterization of the main alloying element10.2320/matertrans.46.2817 ↗
26. Gradient nanostructure evolution and phase transformation of α phase in Ti-6Al-4V alloy induced by ultrasonic surface rolling process10.1016/j.msea.2018.10.098 ↗
27. Microstructure and mechanical properties of laser-deposited Ti65 near-alpha titanium alloy10.1007/s00339-022-05955-6 ↗
28. Effect of heat treatment on microstructure and mechanical properties of laser deposited Ti60A alloy10.1016/j.jallcom.2013.09.149 ↗
29. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
30. Microstructure and mechanical properties of hybrid fabricated Ti-6.5Al-3.5Mo-1.5Zr-0.3Si titanium alloy by laser additive manufacturing10.1016/j.msea.2014.04.019 ↗
31. The anisotropy of laser melting deposition additive manufacturing Ti-6.5Al-3.5Mo-1.5Zr-0.3Si titanium alloy10.1016/j.matdes.2014.11.001 ↗
32. Microstructure and anisotropic tensile behavior of laser additive manufactured TC21 titanium alloy10.1016/j.msea.2016.07.040 ↗
33. Creep deformation behavior of three high-temperature near α-Ti alloys: IMI 834, IMI 829, and IMI 68510.1007/s11661-001-0260-1 ↗
34. Microstructure and mechanical properties of TA15 alloy after thermo-mechanical processing10.1016/j.msea.2018.03.109 ↗
35. Precipitation behavior and strengthening-toughening mechanism of hot rolled sheet of Ti65 titanium alloy during aging process10.1016/j.jallcom.2020.154786 ↗
36. Orientation dependent behavior of tensile-creep deformation of hot rolled Ti65 titanium alloy sheet10.1016/j.jmst.2020.10.021 ↗
37. A novel near α-Ti alloy prepared by hot isostatic pressing: microstructure evolution mechanism and high temperature tensile properties10.1016/j.matdes.2016.05.092 ↗
38. The interdependence theory: the relationship between grain formation and nucleant selection10.1016/j.actamat.2011.04.035 ↗
39. Beryllium as a grain refiner in titanium alloys10.1016/j.jallcom.2009.03.016 ↗
40. The sintering densification, microstructure and mechanical properties of Ti-48Al-2Cr-2Nb by a small addition of SnAl powder10.1016/j.jmrt.2021.11.096 ↗
41. High-strength titanium alloys for aerospace engineering applications: a review on melting-forging process10.1016/j.msea.2022.143260 ↗
42. High temperature hardness and oxidation behavior of TiAl alloy fabricated by electron beam selective melting additive