journal article·2025-05Open access

Corrosion behavior of additively manufactured AlCrFeNi in lead-bismuth eutectic: dendritic oxides layer facilitate resistance to corrosion spalling

Zihan Zhu, Ning Li, Dapeng Yan, Chenyang Lu, Shaoqiang Guo, Dichen Li, Qingyu Li, Sheng Huang

Abstract

Additive Manufacturing (AM) has promising applications in the nuclear field, offering great design and manufacturing flexibility for miniaturised reactors. 316L, the container material of lead-bismuth eutectic (LBE) coolant, faces severe corrosion resistance challenges in high-temperature and high-pressure environments. This study proposes the selection of AlCrFeNi as a candidate material for the 316L surface corrosion-resistant alloy. AlCrFeNi was prepared using directional energy deposition (DED). The corrosion resistance behaviour and the difference in the properties of the oxide layer-matrix interface between AlCrFeNi and 316L were analysed by comparing the morphology and mechanical properties. The results show that a dendritic oxide layer with non-planar growth characteristics has formed inside the AlCrFeNi alloy, and that the oxide layer penetrates deep into the matrix through the pinning mechanism, while the oxide layer of 316L exhibits characteristics of crack propagation along the grain boundaries. Nanoindentation tests show that the oxide-matrix interface of AlCrFeNi exhibits gradient transition characteristics, effectively reducing the difference in interfacial stress. However, there is a significant abrupt change at the interface of 316L, which causes the oxide layer to be more prone to interfacial spalling in LBE. Dendritic oxide layer in AlCrFeNi is based on the synergistic effect of the pinning mechanism and the gradient interface, which is the essential reason for its excellent corrosion resistance and resistance to spalling. • Using metal powder mixtures enable the effective additive manufacturing process. • Cracks occur in 316L after corrosion, while AlCrFeNi does not. • The oxide-matrix interface in AlCrFeNi presents a gradient characteristic. • Oxide in AlCrFeNi matches well with the elastic-plastic properties of the matrix. • Dendritic oxide layer in AlCrFeNi facilitates resistance to corrosion spalling.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Intermetallics and Advanced Alloy Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (74)

Show source-provided references
1. Research progress on LBE corrosion-resistant coatings: a review10.1016/j.pnucene.2024.105358 ↗
2. Review of the studies on fundamental issues in LBE corrosion10.1016/j.jnucmat.2007.06.019 ↗
3. Comparison investigation on corrosion of SIMP and t91 steels exposed to liquid LBE at 450 °C: the role of Si on reducing oxidation rate10.1016/j.corsci.2023.111553 ↗
4. Local mechanical properties of corrosion layers formed on t91 and SS316l steels after exposure to static liquid LBE at 500 °c for 1000 h obtained by nano-indentation10.1016/j.net.2024.03.005 ↗
5. Microstructural evolution of pre-oxidized t91 steel during LBE dissolution corrosion. High Temperature Corrosion of
6. Multi-physical effects induced by spatiotemporal corrosion of t91 cladding in oxygen-controlled LBE environment10.1016/j.corsci.2024.112075 ↗
7. Corrosion kinetics and mechanisms of 15–15ti steel in flowing liquid lead-bismuth eutectic at 500°c10.1016/j.jnucmat.2024.155344 ↗
8. Creep failure of a solution-annealed 15-15ti steel exposed to stagnant lead-bismuth eutectic at 550 and 600 °c10.1016/j.msea.2020.140230 ↗
9. Microstructure and corrosion property evolution of a surface-nanostructured 15–15ti austenitic steel during immersion in liquid LBE at 550 °c10.1016/j.jnucmat.2024.155475 ↗
10. A study on the fretting corrosion of 316l in static lead-bismuth eutectic (LBE): the role of slip amplitude and normal force on damage mechanism at 350 °c
11. Corrosion behavior of AISI 316l steel in static lead melt at 450 °с and 650 °c10.1016/j.prostr.2024.04.031 ↗
12. Early stages of liquid-metal corrosion on pre-oxidized surfaces of austenitic stainless steel 316l exposed to static pb-bi eutectic at 400 °c10.1016/j.corsci.2023.111680 ↗
13. Corrosion and irradiation behavior of Fe-based amorphous coating in lead-bismuth eutectic liquids10.1007/s11431-021-1938-0 ↗
14. Flow accelerated corrosion of stainless steel 316l by a rotating disk in lead-bismuth eutectic melt10.1007/s11837-021-04953-y ↗
15. Growth and exfoliation behavior of the oxide scale on 316l and t91 in flowing liquid lead–bismuth eutectic at 480 °c10.1007/s11085-019-09953-7 ↗
16. Corrosion behavior and failure mechanism of amorphous al2o3 coating at high-temperature LBE10.1016/j.vacuum.2023.112251 ↗
17. Effect of LBE corrosion on microstructure of amorphous al2o3 coating by magnetron sputtering10.1016/j.surfcoat.2022.128598 ↗
18. Study on LBE corrosion failure of FeAl/al2o3 coatings after ion irradiation10.1016/j.matdes.2024.113019 ↗
19. Three composite coatings al + al2o3, Fe–Al and Fe–Al + Al2O3 as a barrier against LBE alloys on f/m steel by multi-arc ion plating10.1007/s11661-023-07192-9 ↗
20. Effect of y2o3 addition on the microstructure and liquid LBE cavitation erosion behaviors of fe-cr-al-ti-c-xy2o3 laser clade coatings10.1016/j.jnucmat.2022.154030 ↗
21. A comprehensive evaluation of y2o3-doped alumina coatings for lead-cooled fast reactors10.1016/j.surfcoat.2024.131207 ↗
22. Lead-bismuth eutectic (LBE) corrosion behavior of AlTiN coatings at 550 and 600゜c10.1016/j.jnucmat.2020.152280 ↗
23. Irradiation-decelerated corrosion behavior of CrN/TiSiN multilayer coating in liquid pb–bi eutectic alloy10.1016/j.ceramint.2024.05.120 ↗
24. Lead-bismuth eutectic (LBE) corrosion mechanism of nano-amorphous composite TiSiN coatings synthesized by cathodic arc ion plating10.1016/j.corsci.2021.109264 ↗
25. Synergism of al and si occurs on corrosion of ti3al1−xSixC2 MAX in the static pb-bi eutectic at 550 °c10.1016/j.corsci.2024.112068 ↗
26. Long-term corrosion tests of ti3SiC2 and ti2AlC in oxygen containing LBE at temperatures up to 700 °c10.1016/j.jnucmat.2016.10.007 ↗
27. Effect of temperature on liquid metal embrittlement susceptibility of an fe10cr4al ferritic alloy in contact with stagnant lead-bismuth eutectic10.1016/j.jnucmat.2020.152196 ↗
28. Evaluation of the optimal y content for the FeCrAl coating with excellent LBE corrosion resistance10.1016/j.jnucmat.2024.155316 ↗
29. Insights into corrosion mechanism of FeCrAlY coating in oxygen-poor static and flowing LBE10.1016/j.corsci.2024.112546 ↗
30. Screening of the FeCrAl LBE corrosion-resistant coatings: the effect of cr and al contents10.1016/j.surfcoat.2023.129477 ↗
31. Enhancing LBE corrosion resistance through inhibition diffusion approach for AlTixCrFe HEA coating10.1016/j.apsusc.2024.160535 ↗
32. Improved lead-bismuth eutectic corrosion resistance and mechanical properties of reactive gas pulse sputtered AlCrFeMoTi/(AlCrFeMoTi)n composite multilayered high-entropy alloy coatings10.1016/j.jnucmat.2022.154093 ↗
33. Influence of si addition on the microstructure, mechanical and lead-bismuth eutectic corrosion properties of an amorphous AlCrFeMoTiSix high-entropy alloy coating10.1016/j.intermet.2022.107649 ↗
34. Effect of al content on the microstructure, mechanical property and lead-bismuth eutectic corrosion resistance of refractory AlxTiNbZrMoV coatings produced by magnetron sputtering
35. Microstructure, mechanical properties and lead-bismuth eutectic corrosion behavior of FeCrAlTiNb high-entropy alloy coatings10.1016/j.corsci.2023.111407 ↗
36. Corrosion behavior of AlCrFeTiNb and AlCrFeTiNb/(AlCrFeTiNb)n coatings in flowing lead–bismuth eutectic alloy with saturated oxygen concentration at 550 °C
37. Corrosion behavior of magnetron sputtering fe31cr20al17ti16nb16 high entropy coating in liquid lead-bismuth eutectic with different oxygen concentration at 500 °c10.1016/j.surfcoat.2024.130579 ↗
38. Lead-bismuth eutectic corrosion behavior of NbMoVCr refractory multi-principal element alloys coating synthesized by magnetron sputtering10.1016/j.jnucmat.2024.155230 ↗
39. Corrosion behavior of refractory TiNbZrMoV high-entropy alloy coating in static lead-bismuth eutectic alloy: a novel design strategy of LBE corrosion-resistant coating? Surface and10.1016/j.surfcoat.2022.128884 ↗
40. Oxidation and dissolution behavior of FeCrNiAl based high entropy alloy and alumina-forming austenitic steel exposed to lead-bismuth eutectic (LBE)10.1016/j.corsci.2023.111693 ↗
41. Fe-14ni-14cr-2.5al steel showing excellent corrosion-resistance in flowing LBE at 550 °c and high temperature strength10.1016/j.jnucmat.2023.154703 ↗
42. Additive manufactured ODS-FeCrAl steel achieves high corrosion resistance in lead-bismuth eutectic (LBE)10.1016/j.jnucmat.2024.155516 ↗
43. Corrosion behavior of 304l stainless steel by wire arc additive manufacturing in liquid lead-bismuth eutectic at 550 °c10.1016/j.jnucmat.2024.155598 ↗
44. Effect of post-annealing on the oxidation behavior of hot rolled ODS-FeCrAl steel in liquid lead10.1016/j.corsci.2023.111815 ↗
45. Additive manufacturing of FeCrAl alloys for nuclear applications - a focused review
46. Chemical compatibility between the α-al2o3 tritium permeation barrier and li4SiO4 tritium breeder10.1016/j.surfcoat.2021.126960 ↗
47. Enhancing corrosion resistance of t91 f/m steel in liquid lead-bismuth (LBE) by slurry FeAl coating10.1016/j.jnucmat.2024.155458 ↗
48. Preliminary study of HDA coating on CLAM steel followed by high temperature oxidation10.1016/j.jnucmat.2013.03.011 ↗
49. A novel AlCrFeMoTi high-entropy alloy coating with a high corrosion-resistance in lead-bismuth eutectic alloy10.1016/j.corsci.2021.109524 ↗
50. Dissolution corrosion of 316l austenitic stainless steels in contact with static liquid lead-bismuth eutectic (LBE) at 500 °c10.1016/j.jnucmat.2017.04.004 ↗
51. The roles of ni segregation on the oxidation kinetics of austenitic stainless steel 316l exposed to oxygen-containing liquid lead-bismuth eutectic (LBE)10.1016/j.corsci.2024.112644 ↗
52. Nickel solubility limit in liquid lead–bismuth eutectic10.1016/j.jnucmat.2010.03.008 ↗
53. Dissolution corrosion of FeCrAl alloy exposed to oxygen-depleted lead-bismuth eutectic containing ni impurities at 600 °c
54. Molecular dynamics simulation on the dissolution and diffusion characteristics of FeCrAl alloy in liquid LBE10.1016/j.anucene.2023.109983 ↗
55. Experimental study on diffusion of ni in lead-bismuth eutectic (LBE)
56. Ellingham diagram: a new look at an old tool10.1016/j.corsci.2023.111113 ↗
57. A comparative study on the corrosion performance of four FeCrAl alloys with different cr contents in contact with oxygen-saturated LBE10.1016/j.jmrt.2023.02.033 ↗
58. Effect of cr and ni contents on the oxidation behavior of ferritic and austenitic model alloys in air with water vapor10.1023/B:OXID.0000032334.75463.da ↗
59. Enhancing LBE corrosion resistance through inhibition diffusion approach for AlTi x CrFe HEA coating10.1016/j.apsusc.2024.160535 ↗
60. The nature of the third-element effect in the oxidation of fe–xcr–3at.% al alloys in 1atm o2 at 1000°c10.1016/j.corsci.2007.06.019 ↗
61. Interaction between liquid lead-bismuth eutectic and aluminized inconel 625 superalloy at 600 and 850 °c10.1016/j.jnucmat.2019.02.046 ↗
62. B2-ordered NiAl content on microstructure, mechanical and oxidation properties of FeAl intermetallic compounds10.1016/j.jmrt.2021.12.128 ↗
63. Corrosion behaviors of FeCrAl alloys exposed to oxygen-saturated static lead bismuth eutectic at 550 °c10.1016/j.corsci.2022.110767 ↗
64. Fabrication and characterization of a functionally graded material from ti-6al-4v to SS316 by laser metal deposition
65. Functionally graded alloys from 316 stainless steel to Inconel 718 by powder-based laser direct energy deposition
66. Microstructure and mechanical properties of functional gradient materials of high entropy alloys prepared by direct energy deposition10.1016/j.jmrt.2023.07.276 ↗
67. The influence of y and nb addition on the corrosion resistance of fe-cr-al-ni model alloys exposed to oxygen-containing molten pb10.1016/j.corsci.2020.109152 ↗
68. Effect of ni and fe elements on microstructure and high temperature oxidation behavior of laser cladding aluminum bronze coating10.1016/j.matchemphys.2023.127383 ↗
69. Effect of graded microstructure on the modulus, hardness, and strength of hot-pressed ZrB2-b4c FGM10.1007/s10853-024-09720-3 ↗
70. A novel FeCrAlW high entropy alloy coating for enhancing lead-bismuth eutectic corrosion resistance10.1016/j.jnucmat.2023.154844 ↗
71. Influence of coating thickness on microstructure, mechanical and LBE corrosion performance of amorphous AlCrFeTiNb high-entropy alloy coatings10.1016/j.surfcoat.2022.128502 ↗
72. On the relationship between indentation hardness and modulus, and the damage resistance of biological materials10.1016/j.actbio.2017.05.034 ↗
73. Plasticity characterization of the modified layer produced by plasma nitrocarburizing of nanocrystallized 18ni maraging steel10.1016/j.vacuum.2011.04.021 ↗
74. Wear and corrosion resistance of CrN/TiN superlattice coatings deposited by a combined deep oscillation magnetron sputtering and pulsed dc magnetron sputtering10.1016/j.apsusc.2015.05.110 ↗