Effect of microalloying on hydrogen embrittlement resistance of 125ksi grade petroleum pipe
Source abstract
Abstract
In this study, the influence of incorporating equimolar proportions of vanadium, titanium, and niobium microalloying elements into C110 steel on the hydrogen embrittlement susceptibility of oil casing steel was investigated at a strength level of 125 ksi. Experimental analyses including microstructural assessment and hydrogen permeation testing were performed to examine the impact of vanadium, titanium, and niobium microalloying elements on the stress-sustained rupture testing (SSRT) hydrogen embrittlement fracture behavior of the steel. It was demonstrated that the incorporation of vanadium microalloying elements at equimolar proportions predominantly enhances the presence of irreversible hydrogen trapping sites, enhances the resistance to tempering softening, and ultimately augments the hydrogen embrittlement resistance of the material.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Welding Techniques and Residual Stresses · Material Properties and Failure Mechanisms
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (64)
Show source-provided references
1. Hydrogen sulfide cracking of carbon and alloy steels10.5006/0010-9312-22.8.238 ↗
2. Stress corrosion of ferritic and martensitic stainless steels in saline solutions10.5006/0010-9312-29.7.268 ↗
3. The improvement of sulfide stress cracking resistance of 12% chromium stainless steels through heat treatment10.5006/0010-9312-33.7.231 ↗
4. Comparative assessment of electrochemical hydrogen absorption by pipeline steels with different strength10.1016/j.corsci.2010.02.011 ↗
5. Review of recent progress in the study of corrosion products of steels in a hydrogen sulphide environment10.1016/j.corsci.2018.05.002 ↗
6. Investigation of structure and properties of low-carbon low-alloyed Cr-Mo pipe steel intended for operating in sour environment10.1063/1.5132158 ↗
7. Microstructural effects on the stress corrosion cracking behavior of medium and high strength steels10.1007/BF02668549 ↗
8. Environmentally assisted cracking and hydrogen diffusion in traditional and high-strength pipeline steels10.1515/corrrev-2015-0051 ↗
9. Roles of composition and microstructure in sulfide cracking of steel10.5006/0010-9312-24.9.261 ↗
10. Effect of crystallographic orientations on the hydrogen-induced cracking resistance improvement of API 5L X70 pipeline steel under various thermomechanical processing10.1016/j.corsci.2016.05.003 ↗
11. An extensive study of hydrogen-induced cracking susceptibility in an API X60 sour service pipeline steel10.1016/j.ijhydene.2016.01.031 ↗
12. Effect of microstructure and crystallography on sulfide stress cracking in API-5CT-C110 casing steel10.1016/j.msea.2016.06.034 ↗
13. Effect of microstructure on the hydrogen trapping efficiency and hydrogen induced cracking of linepipe steel10.1016/j.corsci.2008.03.007 ↗
14. Hydrogen induced cracking susceptibility in different layers of a hot rolled X70 pipeline steel10.1016/j.ijhydene.2013.08.046 ↗
15. Observations of intergranular stress corrosion cracking in a grain-mapped polycrystal10.1126/science.1156211 ↗
16. Role of crystallographic texture on the improvement of hydrogen-induced crack resistance in API 5L X70 pipeline steel10.1016/j.ijhydene.2016.10.124 ↗
17. Role of microstructure on sulfide stress cracking of oil and gas pipeline steels10.1007/s11661-003-0128-7 ↗
18. Effects of alloying elements and microstructure on the susceptibility of the welded HSLA steel to hydrogen-induced cracking and sulfide stress cracking10.1016/j.msea.2008.11.064 ↗
19. Evaluation of the effect of V4C3 precipitates on the hydrogen induced mechanical degradation in Fe-C-V alloys10.1016/j.msea.2016.08.053 ↗
20. The effect of TiC on the hydrogen induced ductility loss and trapping behavior of Fe-C-Ti alloys10.1016/j.corsci.2016.07.013 ↗
21. Effect of Ti, Mo and Cr based precipitates on the hydrogen trapping and embrittlement of Fe–C–X Q&T alloys10.1016/j.ijhydene.2015.06.157 ↗
22. The effect of nanosized (Ti,Mo)C precipitates on hydrogen embrittlement of tempered lath martensitic steel10.1016/j.actamat.2014.04.051 ↗
23. Stress corrosion mechanism and susceptibility of X80 steel under a disbonded coating in an acidic soil solution10.1016/j.jmrt.2021.06.092 ↗
24. Effect of alternating current on the electrochemical behavior and stress corrosion cracking of TA2 in simulated marine environment10.1016/j.jmrt.2023.10.323 ↗
25. Influence of AC/DC on stress corrosion cracking of Ti-6Al-3Nb-2Zr-1Mo alloy in simulated marine solution10.1016/j.ijhydene.2023.11.120 ↗
26. Mechanism and evaluation method of stress corrosion susceptibility of 904L stainless steel with optimized structure in seawater10.1016/j.corsci.2024.111865 ↗
27. Probing into the fundamental effect of Cr on the failure mechanisms of rebars within carbonation and stress environments
28. Micromechanical behavior of a fine-grained China low activation martensitic (CLAM) steel10.1016/j.jmst.2019.05.005 ↗
29. Correlation between vanadium carbide size and hydrogen trapping in ferritic steel10.1016/j.scriptamat.2018.04.013 ↗
30. Observation of hydrogen trapping at dislocations, grain boundaries, and precipitates10.1126/science.aaz0122 ↗
31. Effect of V/Mo ratio on the evolution of carbide precipitates and hydrogen embrittlement of tempered martensitic steel10.1016/j.corsci.2020.108929 ↗
32. The significant effect of tantalum on the hydrogen-induced cracking of pipeline steel: morphology, hydrogen permeation, and theoretical studies10.1016/j.corsci.2022.110213 ↗
33. Hydrogen trapping and hydrogen induced mechanical degradation in lab cast Fe-C-Cr alloys10.1016/j.msea.2016.05.018 ↗
34. Hydrogen trapping phenomena in martensitic steels
35. Quantitative analysis on hydrogen trapping of TiC particles in steel10.1007/s11661-006-0004-3 ↗
36. Nano-preciptates design with hydrogen trapping character in high strength steel10.1007/978-3-642-17665-4_11 ↗
37. Dual role of nanosized NbC precipitates in hydrogen embrittlement susceptibility of lath martensitic steel10.1016/j.corsci.2019.108345 ↗
38. Effect of vanadium content on hydrogen diffusion behaviors and hydrogen induced ductility loss of X80 pipeline steel10.1016/j.msea.2018.09.048 ↗
39. Atomic-scale insights on hydrogen trapping and exclusion at incoherent interfaces of nanoprecipitates in martensitic steels10.1038/s41467-022-31665-x ↗
40. On the sulfide stress cracking resistance of a 125 ksi grade high-strength low-alloyed steel for oil country tubular goods10.1016/j.corsci.2022.110781 ↗
41. Effects of chromium and tungsten on sulfide stress cracking in high strength low alloy 125 ksi grade casing steel10.1016/j.corsci.2019.108163 ↗
42. Effects of manganese and chromium on sulfide stress cracking in 125 ksi grade high-strength low-alloyed steel for oil country tubular goods10.1016/j.corsci.2025.112718 ↗
43. 2014
44. Effect of niobium on sulfide stress cracking behavior of tempered martensitic steel10.1016/j.corsci.2019.108387 ↗
45. The influence of silicon in tempered martensite: understanding the microstructure–properties relationship in 0.5–0.6wt.% C steels10.1016/j.actamat.2014.01.039 ↗
46. Predicting microstructure and strength of maraging steels: elemental optimisation10.1016/j.actamat.2016.07.020 ↗
47. Prediction of the yield strength of a secondary-hardening steel10.1016/j.actamat.2013.04.052 ↗
48. A model for the microstructure behaviour and strength evolution in lath martensite10.1016/j.actamat.2015.07.018 ↗
49. The influence of lath boundaries and carbide distribution on the yield strength of 0.4% C tempered martensitic steels10.1016/0025-5416(82)90176-8 ↗
50. Static recovery of tempered lath martensite microstructures during long-term aging in 9–12% Cr heat resistant steels10.1016/j.matlet.2009.08.024 ↗
51. Strengthening mechanisms of Nb and V microalloying high strength hot-stamped steel10.1016/j.msea.2020.140115 ↗
52. Modelling strength and ductility of ultrafine grained BCC and FCC alloys using irreversible thermodynamics10.1179/174328408X353750 ↗
53. Estimation of the system free energy of martensite phase in an Fe-Cr-C ternary alloy10.2355/isijinternational.45.1909 ↗
54. The isotropic shear modulus of multicomponent Fe-base solid solutions10.1016/S1359-6454(02)00096-4 ↗
55. Precipitation hardening in metals10.1179/026708399773002782 ↗
56. T Tabata, H K Birnbaum. Direct observations of the effect of hydrogenon the behavior of dislocationsin iron n.d.;vol. 17:4.
57. Direct observation of individual hydrogen atoms at trapping sites in a ferritic steel10.1126/science.aal2418 ↗
58. 2018
59. Hydrogen trapping by VC precipitates and structural defects in a high strength Fe–Mn–C steel studied by small-angle neutron scattering10.1016/j.msea.2011.12.080 ↗
60. Thermal desorption spectroscopy evaluation of the hydrogen-trapping capacity of NbC and NbN precipitates10.1007/s11661-013-2181-1 ↗
61. Complex precipitation mechanism of Ti-Nb-V microalloyed bainitic base high strength steel10.1007/s11595-019-2211-y ↗
62. Effect of quenching temperature on sulfide stress cracking behavior of martensitic steel10.1016/j.msea.2018.03.063 ↗
63. The dual role of coherent twin boundaries in hydrogen embrittlement10.1038/ncomms7164 ↗
64. Texture, local misorientation, grain boundary and recrystallization fraction in pipeline steels related to hydrogen induced cracking10.1016/j.msea.2014.10.009 ↗