journal article·2025-07Open access

Macro and micro structural responses of dissimilar TC4/TC17 titanium alloy joints in linear friction welding and post-welding heat treatment processes and their effects on tensile and fatigue performance

Jiatao Liu, Jinglong Li, Feng Jin, Da Zhang, Wei Guo, Jiangtao Xiong

Abstract

The heterogeneous TC4 (Ti-6Al-4V) / TC17 (Ti-5Al-2Sn-2Zr-4Mo-4Cr) joint, formed by linear friction welding (LFW) and post-weld treatment, shows significant potential for blisk manufacturing in aircraft engines. Both LFW and heat treatment involve numerous parameters that can substantially impact joint performance, including strength and fatigue. Macroscopically, welding parameters affect the interface micro voids, influencing tensile strength, while microscopically, post-weld aging can alter the interface microstructure and affect fatigue performance. However, optimizing LFW and post-weld heat treatment for dissimilar titanium alloys remains underexplored. This study investigates the macro and microstructural responses of TC4/TC17 joints during LFW and post-weld aging, focusing on tensile and fatigue properties. Welding was performed at varying pressure (30-150 MPa) and frictional speed (240-400 mm/s) to evaluate burn-off length, interface integrity, and tensile strength. Aging treatments (550-680°C, 4h) were applied to examine their effects on microstructure and fatigue. Results show that a sufficient burn-off length is crucial for joint performance, with welding parameters affecting interface quality, such as micro-voids, which influence tensile strength. The optimal welding conditions for TC4/TC17 joints were found to be 120 MPa pressure and 288-400 mm/s frictional speed, producing defect-free interfaces with joint efficiency comparable to the base material. Aging between 630°C and 680°C caused minimal changes to microstructure and fatigue life, with cracks initiating in the TC4 base material. These insights help optimize LFW for dissimilar titanium alloys in aerospace applications.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced Welding Techniques Analysis · Titanium Alloys Microstructure and Properties · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. BLISK fabrication by linear friction welding
2. Vibration response of metal plate and shell structure under multi-source excitation with welding and bolt connection10.3390/agriculture14060816 ↗
3. Linear and rotary friction welding review10.1080/09506608.2015.1109214 ↗
4. Study of microstructure and mechanical properties of Ti2AlNb/TiAl LFW joint
5. On the effect of a thermal treatment on the tensile and fatigue properties of weak zones of similar Ti17 linear friction welded joints and parent material10.1016/j.matchar.2020.110570 ↗
6. Design and experiment of low-frequency ultrasonic nozzle integrating air-assistant system and acoustic levitation mechanism
7. Study on low fatigue damage behavior of TC17 titanium alloy with basket-weave microstructure10.1016/j.ijfatigue.2024.108462 ↗
8. Microstructure and mechanical properties of friction welding joints with dissimilar titanium alloys10.3390/met6050108 ↗
9. Effect of post-weld heat treatment on microstructure and property of linear friction welded Ti17 titanium alloy joint10.1179/1362171811Y.0000000079 ↗
10. Linear friction welding of equiaxed Ti17 titanium alloy: effects of microstructure evolution on tensile and impact properties10.1007/s10853-023-08666-2 ↗
11. In-situ investigation on dislocation slip concentrated fracture mechanism of linear friction welded dissimilar Ti17 (α+ β)/Ti17 (β) titanium alloy joint10.1016/j.msea.2023.144991 ↗
12. Interfacial characteristics and cohesion mechanisms of linear friction welded dissimilar titanium alloys: Ti–5Al–2Sn–2Zr–4Mo–4Cr (Ti17) and Ti–6Al–2Sn–4Zr–2Mo (Ti6242)10.1016/j.matchar.2019.109942 ↗
13. Strength, fatigue strength and toughness of dissimilar Ti17–Ti64 linear friction welded joints: effect of soft surface contamination and depletion of α precipitates10.1016/j.msea.2020.139989 ↗
14. On the effect of a thermal treatment on the tensile and fatigue properties of weak zones of similar Ti17 linear friction welded joints and parent material10.1016/j.matchar.2020.110570 ↗
15. Effect of linear friction welding process on microstructure evolution, mechanical properties and corrosion behavior of GH4169 superalloy10.1016/j.cja.2024.03.039 ↗
16. A review on rotary and linear friction welding of Inconel alloys
17. Fatigue fracture behavior of a Ti17 joint under various heat treatment specifications prepared by linear friction welding10.1016/j.matchar.2023.113318 ↗
18. Formation and evolution of new α grain boundary and its influence on globularization of α lamellae in TC17 alloy10.1016/j.jallcom.2020.156141 ↗
19. Evolution characterization of α lamellae during isothermal compression of TC17 alloy with colony-α microstructure10.1016/j.msea.2017.12.023 ↗
20. Phase/grain boundary assisted-3D static globularization mechanism of TC17 alloy based on the microstructure reconstruction and in-situ TEM observation10.1016/j.jmst.2023.02.043 ↗
21. Effect of electrical pulse treatment on the microstructural and mechanical responses of heterogeneous linear friction welded TC17/TC4 dissimilar joint10.1016/j.jmrt.2025.01.011 ↗