Microstructure and metastable phase formation of Mo-added Ti6Al4V alloys under laser micro-alloying
Source abstract
Abstract
Understanding the influence of alloying elements on the solidification stage of Ti-based alloys during additive manufacturing (AM) is crucial for subsequent microstructural control and composition optimization. In this work, a laser micro-alloying (LMA) technique is employed to retain the initial solidification microstructure of the alloys. The laser micro-alloying parameters are first optimized, after which Ti6Al4V- x Mo ( x = 0–8 wt%) samples are fabricated using a selected processing parameter (2400 W, 0.2 s) to investigate the influence of Mo content on the microstructure of Ti6Al4V. The results indicate that as the Mo content increases, the alloy's microstructure evolves from a uniform distribution to a distinctive cellular morphology, which is attributed to the enrichment of Mo in the cell interior. The transition from the β phase to the α/α′ phases is inhibited, ultimately resulting in a microstructure predominantly composed of the β phase. Importantly, the increase in Mo content induces a higher proportion of the α″ phase, which is due to the larger lattice distortion that makes atomic migration more difficult and favors the transformation of the bcc -β phase into the orthorhombic-α″ phase. Furthermore, the microhardness of the alloy exhibits a trend of initial increase followed by a decrease, with heterogeneous phases contributing to uneven hardness distribution. This work provides theoretical insights into the microstructure formation and regulation of Mo-added Ti6Al4V alloys in laser additive manufacturing.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (36)
Show source-provided references
1. Material-structure-performance integrated laser-metal additive manufacturing10.1126/science.abg1487 ↗
2. High fatigue resistance in a titanium alloy via near-void-free 3D printing10.1038/s41586-024-07048-1 ↗
3. Effect of grain boundary Widmanstätten α colony on the anisotropic tensile properties of directed energy deposited Ti-6Al-4V alloy10.1016/j.jmst.2023.09.057 ↗
4. Hierarchical anisotropic material response of directed energy deposited (DED) Ti-6Al-4V alloy10.1016/j.actamat.2024.120080 ↗
5. Control of thermally stable core-shell nano-precipitates in additively manufactured Al-Sc-Zr alloys
6. Variant selection in laser powder bed fusion of non-spherical Ti-6Al-4V powder10.1016/j.jmst.2022.10.045 ↗
7. In situ alloying based laser powder bed fusion processing of β Ti-Mo alloy to fabricate functionally graded composites10.1016/j.compositesb.2021.109059 ↗
8. Evaluating the microstructural formation in Mo added Ti6Al4V alloy fabricated by direct energy deposition using a laser-stop strategy
9. Thermophysical properties of additively manufactured Ti-5553 alloy
10. Microstructural response of β-stabilized Ti-6Al-4V manufactured by direct energy deposition10.1016/j.jallcom.2019.152021 ↗
11. Additive manufacturing of ultrafine-grained high-strength titanium alloys10.1038/s41586-019-1783-1 ↗
12. High strength Ti alloy fabricated by directed energy deposition with in-situ Cu alloying10.1016/j.jmatprotec.2022.117759 ↗
13. Fe element promotes the transformation from columnar to equiaxed grains and the formation of ultrafine microstructure of Ti-6Al-4V alloy by laser wire deposition
14. Microstructural engineering of a dual-phase Ti-Al-V-Fe alloy via in situ alloying during laser powder bed fusion
15. Study of the intrinsic mechanisms of nickel additive for grain refinement and strength enhancement of laser aided additively manufactured Ti-6Al-4V10.1088/2631-7990/ac6b61 ↗
16. Hierarchical refinement of nickel-microalloyed titanium during additive manufacturing10.1016/j.scriptamat.2021.113727 ↗
17. Ultrauniform, strong, and ductile 3D-printed titanium alloy through bifunctional alloy design10.1126/science.adj0141 ↗
18. Customizing the Young's modulus of Ti-Mo-Zr alloys by in situ additive manufacturing based on Mo spatial concentration modulation10.1016/j.jmrt.2024.03.027 ↗
19. Microstructure evolution in compositionally graded Ti(4–12wt% Mo) prepared by laser directed energy deposition10.1016/j.jmrt.2023.01.215 ↗
20. Fine-grained Ti-Cu microstructures by solid state thermal cycling
21. Understanding the solute segregation and redistribution behavior in rapidly solidified binary Ti-X alloys fabricated through non-equilibrium laser processing
22. Effects of process parameters on the microstructure and mechanical properties of a laser micro-alloying TiB/Ti-6Al-4V titanium matrix composite10.1016/j.msea.2023.144988 ↗
23. Numerical simulation of the impact of laying powder on selective laser melting single-pass formation10.1016/j.ijheatmasstransfer.2019.07.053 ↗
24. A review of in situ observations of deformation‐induced β ↔ α″ martensite transformations in metastable β Ti alloys10.1002/adem.202200281 ↗
25. Design and fabrication of a metastable beta-type titanium alloy with ultralow elastic modulus and high strength
26. In situ tailoring microstructure in additively manufactured Ti-6Al-4V for superior mechanical performance10.1016/j.actamat.2016.12.027 ↗
27. Multiphysics modeling of phase transformation and microhardness evolution in laser direct deposited Ti6Al4V10.1016/j.jmapro.2019.07.027 ↗
28. Superior high-cycle fatigue property through in-situ precipitation of α' martensite in additively repaired titanium alloy10.1016/j.jallcom.2024.174875 ↗
29. Deformation and failure mechanisms of Ti-6Al-4V as built by selective laser melting10.1016/j.msea.2019.138456 ↗
30. Effect of common alloying elements on α′ martensite start temperature in titanium alloys10.1016/j.jmrt.2023.10.159 ↗
31. Prediction of the martensite start temperature for β titanium alloys as a function of composition10.1016/j.scriptamat.2008.12.034 ↗
32. Giant thermal expansion and α-precipitation pathways in Ti-alloys10.1038/s41467-017-01578-1 ↗
33. High-strength titanium alloy with hierarchical-microstructure design via in-situ refinement-splitting strategy in additive manufacturing
34. Refinement of microstructure and improvement of mechanical properties of directed energy deposited titanium alloys by adding Fe10.1016/j.jallcom.2024.176996 ↗
35. In situ scanning and transmission electron microscopy investigation on plastic deformation in a metastable β titanium alloy10.1016/j.actamat.2017.05.018 ↗
36. High temperature rise dominated cracking mechanisms in ultra-ductile and tough titanium alloy10.1038/s41467-020-15772-1 ↗