Microstructure and mechanical properties of Ti65 titanium alloy T-joints welded by dual-beam laser
Source abstract
Abstract
This study systematically characterized the microstructure, phase transformation, and mechanical properties of Ti65 titanium alloy T-joints welded using dual-beam laser with Ti65 welding wire as filler. The welded joint exhibits distinct zones: the base material retains a fine duplex α-phase microstructure; the heat-affected zone (HAZ) shows grain coarsening and phase transformation; and the fusion zone (FZ) forms needle-like α′ martensite due to rapid cooling-induced β-phase transformation. Elemental analysis confirms uniform alloy distribution with no segregation. X-ray diffraction (XRD) reveals that the fusion zone comprises predominantly α′ martensite (76.79%) with a minor β phase. Electron backscatter diffraction (EBSD) demonstrates grain refinement and a high proportion of high-angle grain boundaries in the fusion zone, enhancing strength and crack resistance. Tensile testing indicates high strength (723–779 MPa) but limited ductility (1.3–1.5% elongation). Hardness decreases gradually from the fusion zone to the skin zone, with fine-grain strengthening significantly increasing fusion zone hardness. These findings demonstrate that dual-beam laser welding with Ti65 filler wire effectively refines microstructure and enhances mechanical properties, addressing critical challenges in welding high-performance titanium alloys.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Welding Techniques and Residual Stresses · Titanium Alloys Microstructure and Properties · Additive Manufacturing Materials and Processes
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Current research and development status of dissimilar materials laser welding of titanium and its alloys10.1016/j.optlastec.2020.106090 ↗
2. Microstructure and texture variations in high temperature titanium alloy Ti65 sheets with different rolling modes and heat treatments10.3390/ma13112466 ↗
3. Microstructure and mechanical properties of laser welded Ti-6Al-4V (TC4) titanium alloy joints10.1016/j.optlastec.2023.110320 ↗
4. Effect of pre-heating and post-weld local heat treatment on the microstructure and mechanical properties of low-cost β-titanium alloy welding joints, obtained by EBW10.4028/p-o8uehr ↗
5. Electron beam welding and post heat treatment of a new near-beta high-strength Ti-4Al-5Mo-5V-5Cr-1Nb alloy10.3390/met12081396 ↗
6. In-situ observation of grain growth and phase transformation in weld zone of Ti-6Al-4V titanium alloy by laser welding with filler wire10.1088/2053-1591/abfc7b ↗
7. Effects of groove clearance size on gap bridging capacity in PWLBW of Ti6Al4V alloy sheet assembled in butt joint configuration: numerical simulation and experimental assessment10.1016/j.optlastec.2022.108527 ↗
8. Study on the grain morphology and fracture performance of T-joints for Ti6Al4V alloy manufactured by dual laser beam bilateral synchronous welding10.1016/j.optlastec.2021.107153 ↗
9. Characterization of laser beam offset welding of titanium to steel with 38Zn-61Cu alloy filler10.1016/j.optlastec.2020.106195 ↗
10. Influence of filler on the microstructure, mechanical properties and residual stresses in TIG weldments of dissimilar titanium alloys10.1007/s40195-021-01236-y ↗
11. Grain refinement of Ti-15V-3Cr-3Sn-3Al metastable β titanium alloy welds using boron-modified fillers10.1016/j.jallcom.2018.03.286 ↗
12. Influences of different filler metals on electron beam welding of titanium alloy to stainless steel10.1016/S1003-6326(14)63034-X ↗
13. Experimental and simulation study on the microstructure of TA15 titanium alloy laser beam welded joints10.1016/j.optlastec.2017.03.014 ↗
14. Study of the microstructure and properties of the butt joint of laser-welded titanium alloy with flux-cored wire10.3390/met13020369 ↗
15. Experimental and numerical study on microstructure and mechanical properties for laser welding-brazing of TC4 titanium alloy and 304 stainless steel with Cu-base filler metal10.1016/j.jmrt.2019.10.075 ↗
16. Microstructure and texture evolution of Ti-6Al-4V alloy T-joint fabricated by dual laser beam bilateral synchronous welding10.1016/j.msea.2021.141426 ↗
17. A new Ti-Al-Cr-Mo-Zr titanium alloy welding wire: stability, microstructure and mechanical properties10.1016/j.jmrt.2024.07.162 ↗
18. Segregation in titanium alloy ingots
19. Grain refinement of additive manufactured Ti-6.5Al-3.5Mo-1.5Zr-0.3Si titanium alloy by the addition of La2O310.1016/j.matlet.2020.128170 ↗
20. Microstructural evolution in laser melted boron alloyed Ti-6Al-4V10.1016/j.jallcom.2024.173762 ↗
21. Quantitative phase analysis of Ti-3Al-5Mo-4.5V dual phase titanium alloy by XRD whole pattern fitting method10.1016/j.matchar.2022.111854 ↗
22. A standard test method for the determination of RIR values by X-ray diffraction10.1017/S0885715600014263 ↗
23. Reduced cells10.1524/zkri.1957.109.1-6.42 ↗
24. Effect of cooling rate on α variant selection and microstructure evolution in TB17 titanium alloy10.3390/ma17205010 ↗
25. Tailoring weldability for microstructures in laser-welded near-α titanium alloy: insights on mechanical properties10.3390/met14060690 ↗
26. Martensite decomposition during rapid heating of Ti-6Al-4V studied via in situ synchrotron X-ray diffraction10.1038/s43246-024-00492-6 ↗
27. Phase transformations in a heterogeneous Ti-xNb-7Zr-0.8O alloy prepared by a field-assisted sintering technique10.1016/j.matdes.2020.109308 ↗
28. Functionally graded Ti6Al4V-Mo alloy manufactured with DED-CLAD® process
29. Influence of heat input in microwelding of titanium alloy by micro plasma arc10.1016/j.jmatprotec.2015.12.014 ↗
30. Effect of the build orientation on the mechanical properties and fracture modes of SLM Ti-6Al-4V10.1016/j.msea.2014.07.086 ↗
31. Selective laser melting of reduced graphene oxide/S136 metal matrix composites with tailored microstructures and mechanical properties10.1016/j.matdes.2019.107811 ↗
32. High ductility in a fully martensitic microstructure: a paradox in a Ti alloy produced by selective laser melting10.1080/21663831.2018.1525773 ↗
33. Room-temperature ductility of Ti–6Al–4V alloy with α′ martensite microstructure10.1016/j.msea.2010.10.070 ↗
34. Microstructure and mechanical properties of Ti-6Al-4V manufactured by selective laser melting after stress relieving, hot isostatic pressing treatment, and post-heat treatment10.1007/s11665-021-05753-w ↗
35. Crack generation and propagation mechanism of Mo–14Re alloy laser welding10.1016/j.ijrmhm.2024.106684 ↗
36. Explore the mechanism of high fatigue crack propagation rate in fine microstructure of friction stir welded aluminum alloy10.1016/j.msea.2013.05.057 ↗
37. Microstructure and texture variations in high-temperature titanium alloy Ti65 sheets with different rolling modes and heat treatments10.3390/ma13112466 ↗
38. Heat treatment of Ti-6Al-4V produced by selective laser melting: microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
39. Deformation mechanisms of Ti–6Al–4V alloy with a martensitic microstructure subjected to oligocyclic fatigue10.1016/S1359-6454(00)00152-X ↗
40. A numerical simulation method considering solid phase transformation and the experimental verification of Ti6Al4V titanium alloy sheet welding processes10.3390/ma15082882 ↗
41. Evolution on the microstructure and mechanical properties of a new multicomponent near-alpha titanium alloy after rolling and heat treatments10.3390/met13071231 ↗
42. Corrosion fatigue of high-strength titanium alloys under different stress gradients10.1007/s11837-015-1360-5 ↗