journal article·2025-07Open access

Study on the influence of microstructural defects of API 5L-B, X52, and X52QS pipeline steels on fracture toughness degradation under in-situ hydrogen environment

Qian Zhao, Yunying Xing, Xiaohu Huang, Qiuxin Liu, Zhu Wang, Yanxia Du, Lei Zhang

Abstract

This paper systematically studies the hydrogen permeation behavior and hydrogen-induced cracking sensitivity of three typical pipe materials for medium and low pressure pipe networks, namely API 5L-B (banded structure), X52 and sulfur-resistant steel X52QS. In-situ gas-phase hydrogen permeation testing under 4 MPa H 2 and fracture toughness evaluation were conducted to systematically analyze the influence of microstructure on hydrogen-induced damage behavior. Results show that API 5L-B exhibits the highest hydrogen trap density, the lowest fracture toughness, and the most pronounced brittle fracture characteristics, indicating the greatest susceptibility to hydrogen embrittlement. X52 shows moderate sensitivity, while X52QS demonstrates the lowest trap density and the best resistance to hydrogen-induced cracking. Further analysis reveals that the increased susceptibility of API 5L-B is primarily attributed to the segregation of its ferrite/pearlite banded structure, higher pearlite content, high dislocation density, and the presence of Al 2 O 3 /MnS inclusions.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Material Properties and Failure Mechanisms · Mechanical Failure Analysis and Simulation

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (75)

Show source-provided references
1. The material basis of the global economy: Worldwide patterns of natural resource extraction and their implications for sustainable resource use policies10.1016/j.ecolecon.2007.02.034 ↗
2. The effect of hydrogen on the mechanical properties of high purity iron III. The dependence of softening in specimen size and charging current density10.1016/0025-5416(79)90193-9 ↗
3. Effects of multiple welding thermal cycles on hydrogen permeation parameters of X80 steel10.1016/j.corsci.2021.109797 ↗
4. San Marchi · 2011
5. Characterization of inclusions of X80 pipeline steel and its correlation with hydrogen-induced cracking10.1016/j.corsci.2010.12.011 ↗
6. Recommendations on X80 steel for the design of hydrogen gas transmission pipelines10.1016/j.ijhydene.2012.02.009 ↗
7. Effect of manganese content and microstructure on the susceptibility of X70 pipeline steel to hydrogen cracking10.1016/j.msea.2012.04.076 ↗
8. Sour corrosion performance and sensitivity to hydrogen induced cracking in the X70 pipeline steel: effect of microstructural variation and pearlite percentage10.1016/j.ijpvp.2022.104759 ↗
9. Sensitivity to hydrogen induced cracking, and corrosion performance of an API X65 pipeline steel in H2S containing environment: influence of heat treatment and its subsequent microstructural changes10.1016/j.jmrt.2021.07.118 ↗
10. Effect of calcareous deposits on hydrogen permeation in X80 steel under cathodic protection10.1016/j.matchemphys.2017.12.015 ↗
11. Effect of inclusions on the hydrogen embrittlement of martensitic medium-Mn steel10.1016/j.jmrt.2023.08.090 ↗
12. Effect of 2-mercaptobenzothiazole concentration on sour-corrosion behavior of API X60 pipeline steel: electrochemical parameters and adsorption mechanism10.1007/s12613-020-2156-3 ↗
13. The effect of temperature, CO2, H2S gases and the resultant iron carbonate and iron sulfide compounds on the sour corrosion behaviour of ASTM A-106 steel for pipeline transportation10.1016/j.ijpvp.2019.02.019 ↗
14. The effect of natural inhibitor concentration of Fumaria officinalis and temperature on corrosion protection mechanism in API X80 pipeline steel in 1 M H2SO4 solution10.1016/j.ijpvp.2020.104241 ↗
15. Study on hydrogen embrittlement behaviour of X52 welded joints in hydrogen transport environments
16. The regulation of dislocation and precipitated phase improving hydrogen embrittlement resistance of pipeline steel in high pressure hydrogen environment10.1016/j.ijfatigue.2024.108657 ↗
17. Influence of phase morphology on hydrogen embrittlement of type 2205 duplex stainless steel10.1016/j.msea.2025.148335 ↗
18. Comparative study on hydrogen induced cracking sensitivity of two commercial API 5L X80 steels10.1016/j.ijpvp.2022.104620 ↗
19. Effect of microstructure on hydrogen embrittlement and hydrogen-induced cracking behaviour of a high-strength pipeline steel weldment10.1016/j.corsci.2023.111764 ↗
20. The influence of chemical composition and microstructure of API linepipe steels on hydrogen induced cracking and sulfide stress corrosion cracking10.1016/S0921-5093(03)00217-X ↗
21. Effects of defect on the hydrogen embrittlement behavior of X80 pipeline steel in hydrogen-blended natural gas environments10.1016/j.ijhydene.2024.01.107 ↗
22. Inhibiting effect of carbon monoxide on gaseous hydrogen embrittlement of pipelines transporting hydrogen10.1016/j.corsci.2023.111789 ↗
23. Influence of hydrogen fugacity on the fracture toughness and fracture mechanism of a X65 natural gas transmission pipeline steel10.1016/j.ijhydene.2024.09.035 ↗
24. Effects of hydrogen on the fracture toughness of X80 steel base metal and girth weld under strong cathodic current with in-situ hydrogen charging10.1016/j.engfailanal.2022.106143 ↗
25. Investigating the influence mechanism of hydrogen partial pressure on fracture toughness and fatigue life by in-situ hydrogen permeation10.1016/j.ijhydene.2021.03.183 ↗
26. Assessing the effects of loading rate on fracture toughness of AISI 1020 and API 5L X80 steels with hydrogen charging: experimental and numeric simulation study10.1016/j.engfracmech.2024.110771 ↗
27. Different effects of pure hydrogen vs. hydrogen/natural gas mixture on fracture toughness degradation of two carbon steels10.1016/j.matlet.2021.129924 ↗
28. Hydrogen embrittlement of structural steels: effect of the displacement rate on the fracture toughness of high-pressure hydrogen pre-charged samples10.1016/j.ijhydene.2019.03.279 ↗
29. 2017
30. Hydrogen permeation and embrittlement susceptibility of X80 welded joint under high-pressure coal gas environment10.1016/j.corsci.2016.04.029 ↗
31. 2021
32. Determination of the critical plastic strain-induced stress of X80 steel through an electrochemical hydrogen permeation method10.1016/j.electacta.2016.08.026 ↗
33. Interaction between dislocations, precipitates and hydrogen atoms in a 2000 MPa grade hot-stamped steel10.1016/j.jmrt.2022.04.094 ↗
34. A comprehensive review on hydrogen permeation barrier in the hydrogen transportation pipeline: mechanism, application, preparation, and recent advances10.1016/j.ijhydene.2024.12.379 ↗
35. Effect of surface calcareous deposits on hydrogen uptake of X80 steel under strong cathodic current10.1016/j.ijhydene.2020.10.264 ↗
36. Investigations of temperature effects on hydrogen diffusion and hydrogen embrittlement of X80 pipeline steel under electrochemical hydrogen charging environment10.1016/j.corsci.2023.111460 ↗
37. Analysis of electrochemical hydrogen permeation through X-65 pipeline steel and its implications on pipeline stress corrosion cracking10.1016/j.ijhydene.2006.07.018 ↗
38. The adsorption and diffusion of electrolytic hydrogen in palladium
39. A comparison of vintage and modern X65 pipeline steel using hollow specimen technique for in-situ hydrogen testing10.1016/j.engfailanal.2024.108530 ↗
40. Hydrogen permeation in a submerged arc weldment of TMCP steel10.1016/S0254-0584(02)00100-1 ↗
41. Specimen thickness effect on the property of hydrogen embrittlement in single edge notch tension testing of high strength pipeline steel10.1016/j.ijhydene.2018.06.118 ↗
42. Influence of hydrogen on the microstructure and fracture toughness of friction stir welded plates of API 5L X80 pipeline steel10.1016/j.ijhydene.2019.06.210 ↗
43. Hydrogen enhanced fatigue crack growth rates in a ferritic Fe-3 wt%Si alloy and a X70 pipeline steel10.1016/j.engfracmech.2019.106641 ↗
44. Dual roles of pearlite microstructure to interfere/facilitate gaseous hydrogen-assisted fatigue crack growth in plain carbon steels10.1016/j.ijfatigue.2021.106561 ↗
45. Effect of the cathodic current density on the sub-surface concentration of hydrogen in X80 pipeline steels under cathodic protection10.1016/j.ijhydene.2016.09.214 ↗
46. Hydrogen-induced cracking assessment in pipeline steels through permeation and crystallographic texture measurements10.1007/s11665-016-2021-8 ↗
47. Effect of tempering temperature and inclusions on hydrogen-assisted fracture behaviors of a low alloy steel10.1016/j.msea.2016.11.064 ↗
48. Influence factors on hydrogen embrittlement of high strength low alloy steels
49. Post weld heat treatment of hypereutectoid hadfield steel: characterization and control of microstructure, phase equilibrium, mechanical properties and fracture mode of welding joint10.1016/j.jmapro.2018.06.009 ↗
50. Microstructural features and hydrogen diffusion in bcc FeCr alloys: a comparison between the Kelvin probe- and nanohardness based-methods10.1016/j.ijhydene.2024.12.433 ↗
51. Small crack formation in a low carbon steel with banded ferrite-pearlite structure10.1016/j.msea.2004.09.058 ↗
52. Material selection for hydrogen long-distance transmission pipelines
53. Hayden · 2009
54. Hydrogen embrittlement behavior of high strength bainitic rail steel: effect of tempering treatment10.1016/j.engfailanal.2018.07.005 ↗
55. Effect of nickel on hydrogen permeation in ferritic/pearlitic low alloy steels10.1016/j.ijhydene.2017.12.174 ↗
56. Hydrogen embrittlement of hardened low-carbon sheet steel10.2355/isijinternational.50.294 ↗
57. Effect of grain size on the resistance to hydrogen embrittlement of API 2W Grade 60 steels using in situ slow-strain-rate testing10.1016/j.corsci.2017.08.032 ↗
58. The impact of misorientation on the grain boundary energy in bi-crystal copper: an atomistic simulation study10.1007/s00894-022-05037-7 ↗
59. Structures and transitions in bcc tungsten grain boundaries and their role in the absorption of point defects10.1016/j.actamat.2018.07.051 ↗
60. Effect of environmental and metallurgical factors on hydrogen induced cracking of HSLA steels10.1016/j.corsci.2008.09.030 ↗
61. Effect of microstructure and inclusions on hydrogen induced cracking susceptibility and hydrogen trapping efficiency of X120 pipeline steel10.1016/j.msea.2010.07.022 ↗
62. Effect of non-metallic inclusions on hydrogen-induced cracking of API5L X100 steel10.1016/j.ijhydene.2010.05.089 ↗
63. Effect of stress triaxiality on the hydrogen embrittlement micromechanisms in a pipeline steel evaluated by fractographic analysis10.1016/j.msea.2023.145689 ↗
64. Investigation of hydrogen embrittlement behavior in X65 pipeline steel under different hydrogen charging conditions10.1016/j.msea.2022.144262 ↗
65. The effect of hydrogen on the fracture toughness of friction-stir welded API 5L X70 pipeline steels10.1111/ffe.13799 ↗
66. In situ observation of pearlite phase transition in high-carbon steel under different holding temperatures and cooling rates using confocal laser scanning microscope10.1016/j.jmrt.2023.02.216 ↗
67. Role of ferrite/pearlite banded structure and segregation on mechanical properties of microalloyed hot rolled steel10.1179/026708399101505121 ↗
68. Hydrogen adsorption and diffusion on the surface of alloyed steel: first-principles studies10.1016/j.ijhydene.2023.12.046 ↗
69. Hydrogen embrittlement in bearing steels10.1080/02670836.2016.1156810 ↗
70. A general model for hydrogen trapping at the inclusion-matrix interface and its relation to crack initiation10.1080/14786435.2017.1378451 ↗
71. Effect of Cr-rich carbide precipitates on austenite stability and consequent corrosion behavior of ultrafine-grained 304 stainless steel produced by cryogenic rolling and annealing treatment10.1016/j.matchar.2022.112553 ↗
72. Effects of Si on the stress rupture life and microstructure of a novel austenitic stainless steel10.1016/j.jmrt.2023.06.131 ↗
73. Nanoscale precipitation, mechanical properties, and deformation behavior of NiAl-strengthened high-strength steels: effects of Ni and Al contents and ratios10.1016/j.matdes.2023.112341 ↗
74. Effects of grain size on hydrogen environment embrittlement of high strength low alloy steel in 45 MPa gaseous hydrogen10.2320/matertrans.M2009241 ↗
75. A review of influence of hydrogen on fracture toughness and mechanical properties of gas transmission pipeline steels10.1016/j.ijhydene.2025.01.018 ↗