Exploring the 5Cr steel as supercritical CO2 geothermal extraction pipeline from corrosion point of view: Effects of phase environment, temperature and Cl−
Source abstract
Abstract
The corrosion performance of 5Cr steel as injection/production pipeline material for Supercritical CO 2 (S–CO 2 ) geothermal extraction has been systematically investigated in both S–CO 2 and H 2 O phases at 23 MPa. The results show that H 2 O phase induces more severe corrosion damage on 5Cr steel than S–CO 2 phase. Increasing temperature from 150 to 300 °C and the introduction of 2000 ppm Cl − intensify corrosion. Despite environmental variation, 5Cr steel consistently forms a dual-layer structure comprising an outer FeCO 3 /Fe–O layer and an inner FeCr 2 O 4 spinel layer, and the latter plays an important role in improving the corrosion resistance. 5Cr steel is suitable for S–CO 2 environments below 200 °C.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Hydrogen embrittlement and corrosion behaviors in metals · Calcium Carbonate Crystallization and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (48)
Show source-provided references
1. The potential of coupled carbon storage and geothermal extraction in a CO2-enhanced geothermal system: a review10.1186/s40517-020-00173-w ↗
2. A comparison of electric power output of CO2 plume geothermal (CPG) and brine geothermal systems for varying reservoir conditions10.1016/j.apenergy.2014.11.043 ↗
3. Power generation with renewable energy and advanced supercritical CO2 thermodynamic power cycles: a review10.3390/en16237781 ↗
4. A literature review of using supercritical CO2 for geothermal energy extraction: potential, methods, challenges, and perspectives10.1016/j.ref.2024.100637 ↗
5. Corrosion and corrosion fatigue of AISI 420C (X46Cr13) at 60°C in CO2-saturated artificial geothermal brine10.1016/j.corsci.2012.11.005 ↗
6. Applications of density functional theory to corrosion and corrosion prevention of metals: a review10.1002/mgea.83 ↗
7. High-throughput experimental techniques for corrosion research: a review10.1002/mgea.20 ↗
8. Enhanced microbiologically influenced corrosion resistance of 5Cr pipeline steel in the presence of Shewanella oneidensis MR-110.1016/j.colcom.2025.100841 ↗
9. Investigation of corrosion behavior of 5Cr steel in CO2-silty sand environment: effects of hydrodynamic impact angles10.1016/j.ijpvp.2024.105369 ↗
10. Study on corrosion resistance mechanism of Cr-containing steel in simulated oilfield produced fluid10.1016/j.ijoes.2023.100154 ↗
11. Corrosion behavior and durability of low-alloy steel rebars in marine environment10.1007/s11665-016-2342-7 ↗
12. Cracking of 5Cr steel tee-pipe during start-up operation in heavy oil upgrade refinery10.1016/j.engfailanal.2017.06.052 ↗
13. Effect of double quenching and tempering heat treatment on the microstructure and mechanical properties of a novel 5Cr steel processed by electro-slag casting10.1016/j.msea.2014.09.063 ↗
14. Effect of Cr content on the electrochemical behavior of low-chromium X65 steel in CO2 environment10.20964/2016.10.58 ↗
15. Comparison of corrosion behavior of X52 steel in liquid and supercritical CO2 transport environments with multiple impurities10.1016/j.corcom.2024.01.006 ↗
16. Effects of chloride content on CO2 corrosion of carbon steel in simulated oil and gas well environments10.1016/j.corsci.2014.03.025 ↗
17. Long-term corrosion and stress corrosion cracking of X65 steel in H2O-saturated supercritical CO2 with SO2 and O2 impurities10.1016/j.conbuildmat.2022.129746 ↗
18. 2003
19. Effects of alternating current on microbiologically synergistic corrosion of pipeline steel X80 applied by elastic stress10.1016/j.corcom.2023.08.001 ↗
20. Corrosion behavior of AlCrVTi light-weight high-entropy alloy coating in different corrosion environments10.1007/s44251-023-00020-7 ↗
21. In situ monitoring of stress corrosion at the alloy 625|NaCl interface10.1007/s44251-024-00034-9 ↗
22. Effects of long-term annealing on pitting corrosion behavior of type 304 borated stainless steels10.1016/j.corcom.2024.08.001 ↗
23. Comparative study of A106 steel corrosion in fresh and dirty MEA solutions during the CO2 capture process: effect of NO3−10.1016/j.corsci.2020.108521 ↗
24. The formation mechanism of corrosion scale and electrochemical characteristic of low alloy steel in carbon dioxide-saturated solution10.1016/j.corsci.2011.12.025 ↗
25. Effect of chloride ion content on pitting corrosion of dispersion-strengthened-high-strength steel10.1016/j.corcom.2022.03.005 ↗
26. Simultaneous optimization of corrosion resistance and mechanical properties of LMD-processed 316L austenitic stainless steel by adding Ti nanoparticles in a simulated environment for proton exchange membrane fuel cells10.1016/j.vacuum.2025.114205 ↗
27. Optimization of corrosion resistance of LMD-processed 316L austenitic stainless steel by adding CeO2 nanoparticles in a simulated environment for PEMFCs
28. Condensed phase corrosion of P91 and DSS 2205 steels at advanced oxygen-fired pressurized fluidized bed combustion plants10.1002/maco.202011882 ↗
29. Thermodynamics of Cr2O3, FeCr2O4, ZnCr2O4, and CoCr2O410.1016/j.jct.2007.03.001 ↗
30. Influence of a small velocity variation on the evolution of the corrosion products and corrosion behaviour of super 13Cr SS in a geothermal CO2 containing environment10.1016/j.corsci.2020.108983 ↗
31. Pourbaix diagram for HP-13Cr stainless steel in the aggressive oilfield environment characterized by high temperature, high CO2 partial pressure and high salinity10.1016/j.electacta.2018.08.156 ↗
32. Oxidation processes and involved chemical reactions of corrosion-resistant alloys in supercritical water10.1021/acs.iecr.0c01394 ↗
33. A thermodynamic and kinetic study of the formation and evolution of corrosion product scales on 13Cr stainless steel in a geothermal environment10.1016/j.corsci.2020.108640 ↗
34. Corrosion behavior of carbon steel in supercritical CO2-Water environments
35. Water effect on steel under supercritical CO2 condition
36. Corrosion behaviors of steels under supercritical CO2 conditions10.1515/corrrev-2014-0067 ↗
37. Microstructural stability and high temperature isothermal oxidation behavior studies of high entropy alloy Al0.5CoCrFeNi10.1016/j.corcom.2024.07.005 ↗
38. Observation of the formation of CuAl2O4 by the direct consumption of Al2O3 in an NAB alloy at elevated temperature10.1016/j.corsci.2024.112026 ↗
39. Flow line corrosion failure as a function of operating temperature and CO2 partial pressure using real time field data10.1016/j.engfailanal.2019.04.037 ↗
40. Corrosion of heat exchanger materials in co-combustion thermal power plants10.1016/j.rser.2022.112328 ↗
41. Revealing the temperature effects on the corrosion behaviour of 2205 duplex stainless steel from passivation to activation in a CO2-containing geothermal environment10.1016/j.corsci.2021.109495 ↗
42. The evolution and characterisation of the corrosion scales formed on 3Cr steel in CO2-containing conditions relevant to geothermal energy production10.1016/j.corsci.2021.109342 ↗
43. Haynes · 2016
44. L21-strengthened face-centered cubic high-entropy alloy with well pitting resistance10.1016/j.corsci.2023.111043 ↗
45. Combating marine corrosion on engineered oxide surface by repelling, blocking and capturing cl−: a mini review10.1016/j.corcom.2021.09.001 ↗
46. The role of Cl- in the formation of the corrosion products and localised corrosion of 15Cr martensite stainless steel under an CO2-containing extreme oilfield condition10.1016/j.corsci.2021.109935 ↗
47. A study on the interaction between chloride ions and CO2 towards carbon steel corrosion10.1016/j.corsci.2020.108531 ↗
48. Corrosion testing of materials in simulated superheated geothermal environment10.1016/j.corsci.2020.108584 ↗