Effects of GTAW process and post-welding heat treatment on the microstructure evolution, cracking behavior and hardness of Inconel 939 superalloy using Inconel 617 filler metal
Source abstract
Abstract
This study investigates repair welding of service-aged Inconel 939 superalloy (100,000 operational hours) using gas tungsten arc welding (GTAW) with Inconel 617 filler metal. The research focuses on three key challenges: (1) irregularities in pre-existing MC carbides, (2) heat-affected zone (HAZ) liquation cracking, and (3) post-weld heat treatment (PWHT) effects on microstructure evolution and hardness distribution. Initial welding revealed a 91 μm HAZ crack, identified as liquation cracking caused by localized melting of service-induced lamellar carbides along grain boundaries. PWHT yielded microstructural improvements and hardness homogenization across the weld pool, partial melting zone (PMZ), and HAZ. However, the heat treatment also promoted crack growth to 386 μm, characterized as strain-aging cracking due to its formation and propagation during PWHT.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: High Temperature Alloys and Creep · Additive Manufacturing Materials and Processes · Aluminum Alloy Microstructure Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (42)
Show source-provided references
1. Crack types, mechanisms, and suppression methods during high-energy beam additive manufacturing of nickel-based superalloys: a review
2. Donachie · 2002
3. Reed · 2008
4. MacKenzie · 2005
5. Processing of nickel‐base superalloys for turbine engine disc applications10.1002/1527-2648(200012)2:12<777::AID-ADEM777>3.0.CO;2-R ↗
6. The growth of γ′ precipitates in nickel-base superalloys10.1016/0001-6160(83)90062-7 ↗
7. Microstructural investigation of IN 939 superalloy10.1016/0042-207X(92)90115-D ↗
8. Evaluation of the in 939 alloy for large aircraft engine structures
9. Investigation of microstructure evolution of Inconel 939 joint diffusion brazed using an amorphous liquated Ni-Cr-Fe-Si-B interlayer
10. Comparison of microstructural stability of IN939 superalloy with two different manufacturing routes during long-time aging10.1016/S1003-6326(14)63245-3 ↗
11. The effect of heat treatment sequence on microstructure and mechanical properties of diffusion brazed IN-939 superalloy10.1016/j.jmatprotec.2018.11.020 ↗
12. Effect of welding parameters on the liquation cracking behavior of high-chromium Ni-based superalloy10.1007/s11665-020-05292-w ↗
13. Effects of long-term thermal exposure on the microstructure and properties of a cast Ni-base superalloy10.1007/s11661-007-9381-5 ↗
14. Heat-affected zone crack healing in IN939 repaired joints using hot isostatic pressing10.1007/s40194-018-0579-5 ↗
15. González · 2012 · 1372
16. Relationship of isothermal solidification completion and precipitate formation with mechanical properties of Inconel 939 joints vacuum TLP bonded by an amorphous Ni–Cr–Fe–Si–B filler alloy10.1016/j.jmrt.2022.04.139 ↗
17. Effects of residual stresses induced by repair welding on the fracture toughness of Ni-based IN939 alloy10.1016/j.tafmec.2020.102614 ↗
18. Advanced weld repair of gas turbine hot section components
19. Study on incipient melting in cast Ni base IN939 superalloy during solution annealing and its effect on hot workability10.1179/1743284712Y.0000000090 ↗
20. Lippold · 2011
21. Evaluations of residual stresses in repair welding of Ni-based IN939 superalloy10.1080/01495739.2020.1751759 ↗
22. A review on TIG welding technology variants and its effect on weld geometry10.1016/j.matpr.2021.07.308 ↗
23. Effects of heat input on metallurgical behavior in HAZ of multi-pass and multi-layer welded IN-939 superalloy10.1016/j.jmrt.2021.08.113 ↗
24. Investigating the effects of repair welding on microstructure, mechanical properties, and corrosion behavior of IN-939 superalloy10.1007/s11665-022-07596-5 ↗
25. Microstructural response to heat affected zone cracking of prewelding heat-treated Inconel 939 superalloy10.1016/j.matchar.2011.09.006 ↗
26. Effects of pre-and post-weld heat treatment cycles on the liquation and strain-age cracking of IN939 superalloy10.1088/2631-8695/ab4d6c ↗
27. Effects of pre-weld heat treatment and heat input on metallurgical and mechanical behaviour in HAZ of multi-pass welded IN-939 superalloy10.3390/met10111453 ↗
28. Effect of preweld heat treatment on the microstructure of heat-affected zone (HAZ) and weldability of Inconel 939 superalloy10.1007/s11665-013-0704-y ↗
29. Liquation cracking in the heat-affected zone of IN939 superalloy tungsten inert gas weldments10.1007/s12613-019-1954-y ↗
30. Effects of filler metals on heat-affected zone cracking in IN-939 superalloy gas-tungsten-arc welds10.1007/s11665-020-04617-z ↗
31. A study on microstructure and phase transformation in the weld fusion zone of TIG-welded IN939 with IN625 and IN718 as filler metal10.1007/s11661-020-05690-8 ↗
32. Heat-induced effects and cracking susceptibility in gas tungsten arc welding of Inconel 939 superalloy using Inconel 625 filler metal
33. On the development of a new pre-weld thermal treatment procedure for preventing heat-affected zone (HAZ) liquation cracking in nickel-base IN 738 superalloy10.1080/14786435.2014.956838 ↗
34. Rejuvenation of the microstructure and mechanical properties of a service-exposed IN939 superalloy by heat treatments10.1080/09603409.2018.1448529 ↗
35. Revisiting the diffusion of niobium in an as-cast nickel-based superalloy during annealing at elevated temperatures10.1007/s12540-019-00342-y ↗
36. Investigation of solidification and segregation characteristics of cast Ni-base superalloy K417G10.1016/j.jmst.2016.11.009 ↗
37. The effect of pre-heating and pre-cold treatment on the formation of liquation and solidification cracks of nickel-based superalloy welded by laser beam10.1016/j.jmrt.2020.07.053 ↗
38. Microstructural analysis of laser-beam-welded directionally solidified INCONEL 73810.1007/s11661-006-9063-8 ↗
39. Liquation cracking behavior and control in the heat affected zone of GH909 alloy during Nd: YAG laser welding10.1016/j.jmatprotec.2017.01.018 ↗
40. Mechanism of post-weld heat treatment cracking in Rene 80 nickel based superalloy10.1179/026708302225001633 ↗
41. Post-weld heat treatment cracking in autogenous GTA welded cast Inconel 738LC superalloy10.1179/174328406X131055 ↗
42. The effect of lattice misfit on the dislocation motion in superalloys during high-temperature low-stress creep10.1016/j.actamat.2005.06.013 ↗