Towards sustainable additive manufacturing: Enhanced productivity via numerical-experimental melt pool engineering in laser powder bed fusion of Ti-alloy
Source abstract
Abstract
Laser Powder Bed Fusion (LPBF) offers a promising approach for creating metallic components with tailored properties. However, low production speed and high manufacturing costs remain challenges. Enhancing the building rate improves economic efficiency and reduces energy consumption, contributing to a greener environment. This study proposes a numerical-experimental approach to increase the LPBF build rate for Ti-5553 while maintaining part quality and performance. High-speed scanning parameters that produce parts with high density, low surface roughness, and sufficiently large melt pools were chosen from the optimized process parameters. A time-efficient and cost-effective simulation, developed by the authors, was used to predict the effects of process parameters on melt pool geometry and the possibility of lack-of-fusion defect formation due to increased hatch distance and layer thickness. This predictive analysis led to the selection of two parameter sets for fast and dense sample printing. The results indicate that increasing the hatch distance and the layer thickness enhances productivity by approximately 54 % and 104 %, respectively, compared to the original optimized parameters. The printed samples with fast-print parameters exhibit an excellent density (>99.98 %) and a favorable surface roughness (<17 μm). While these samples demonstrate a slightly finer grain size than the reference, their tensile strength, elongation, and hardness differ by less than 4 %, confirming negligible mechanical impact. These findings demonstrate a viable strategy for significantly improving LPBF efficiency while maintaining part quality.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · High Entropy Alloys Studies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (65)
Show source-provided references
1. Toyserkani · 2021
2. Microstructural control in metal laser powder bed fusion additive manufacturing using laser beam shaping strategy10.1016/j.actamat.2019.11.053 ↗
3. Microstructural porosity in additive manufacturing: the formation and detection of pores in metal parts fabricated by powder bed fusion
4. Additively manufactured materials and structures: a state-of-the-art review on their mechanical characteristics and energy absorption10.1016/j.ijmecsci.2023.108102 ↗
5. Energy consumption in additive manufacturing of metal parts
6. Assessing the sustainability of laser powder bed fusion and traditional manufacturing processes using a parametric environmental impact model10.1016/j.resconrec.2023.107138 ↗
7. Additive manufacturing for sustainability and circular economy: needs, challenges, and opportunities for 3D printing of recycled polymeric waste
8. Note on the rate and energy efficiency limits for additive manufacturing10.1111/jiec.12664 ↗
9. Sustainable additive manufacturing: an overview on life cycle impacts and cost efficiency of laser powder bed fusion
10. Life cycle assessment of selective-laser-melting-produced hydraulic valve body with integrated design and manufacturing optimization: a cradle-to-gate study
11. Energy efficiency of Gaussian and ring profiles for LPBF of nickel alloy 71810.1007/s00170-024-13511-0 ↗
12. A LifeCycle analysis and economic cost analysis of corrugated cardboard box reuse and recycling in the United States10.3390/resources12020022 ↗
13. Productivity improvement opportunities for metal powder bed fusion technologies: a systematic literature review10.1108/RPJ-09-2023-0333 ↗
14. Topology optimization of multi-material active structures to reduce energy consumption and carbon footprint
15. Ferreira · 2022 · 22
16. Innovative and best practices in sustainable strategies for waste reduction in additive manufacturing10.1016/j.hybadv.2025.100527 ↗
17. HYbrid titanium alloys produced by laser powder bed fusion using Ti-5553 and Ti–42Nb powder recycling10.1016/j.jmrt.2023.11.208 ↗
18. Mechanical properties of hastelloy X produced by laser powder bed fusion and affected by spatter redeposition10.1016/j.jmrt.2024.02.150 ↗
19. Optimization of hatch spacing for improved build rate and high density preservation in laser powder bed fusion of pure titanium10.1016/j.jmrt.2024.11.265 ↗
20. Increasing productivity for laser powder bed fusion of Ti–6Al–4V parts through increased layer thickness10.1007/s40964-025-01079-4 ↗
21. Increasing productivity of laser powder bed fusion manufactured hastelloy X through modification of process parameters10.1016/j.jmapro.2022.04.013 ↗
22. Quality and productivity trade-off in powder-bed additive manufacturing10.1007/s40964-020-00122-w ↗
23. Laser powder bed fusion of metallic components: latest progress in productivity, quality, and cost perspectives10.1016/j.jmrt.2023.11.049 ↗
24. Increasing the productivity of laser powder bed fusion: influence of the hull-bulk strategy on part quality, microstructure and mechanical performance of Ti-6Al-4V
25. High speed laser powder bed fusion of M789 tool steel with an optimized 120 μm layer thickness approach10.1016/j.procir.2022.08.141 ↗
26. Exploring spatial beam shaping in laser powder bed fusion: high-fidelity simulation and in-situ monitoring
27. Ways to increase the productivity of L-PBF processes10.1007/s43452-023-00750-3 ↗
28. Systematic investigation into laser powder bed fusion of Ti-5553 through single-track and multi-layer studies for tailored manufacturing solutions10.1016/j.jmrt.2024.10.057 ↗
29. A numerical modelling for laser Powder-bed fusion of Ti-alloy with a hybrid heat source: an investigation on solidification and microstructure formation10.1016/j.optlastec.2024.110647 ↗
30. Predictive model for porosity in powder-bed fusion additive manufacturing at high beam energy regime
31. Numerical and experimental analysis of heat distribution in the laser powder bed fusion of Ti-6Al-4V10.1080/24725854.2018.1461964 ↗
32. The influence of induction sintering on microstructure and deformation behavior of Ti-5Al-5Mo-5V-3Cr alloy10.1007/s11661-021-06179-8 ↗
33. Analysis tools for electron and X-ray diffraction. ATEX –
34. Hasanabadi · 2024
35. Effect of processing parameters on surface roughness, porosity and cracking of as-built IN738LC parts fabricated by laser powder bed fusion10.1016/j.jmatprotec.2020.116788 ↗
36. Balling phenomena in selective laser melted tungsten10.1016/j.jmatprotec.2015.02.032 ↗
37. Mitigation of lack of fusion defects in powder bed fusion additive manufacturing10.1016/j.jmapro.2018.10.028 ↗
38. Direct metal fabrication in rapid prototyping: a review10.1016/j.jmapro.2019.05.001 ↗
39. Research on track overlapping during selective laser melting of powders10.1016/j.jmatprotec.2012.05.012 ↗
40. Rapid L-PBF printing of IN718 coupled with HIP-quench: a novel approach to manufacture and heat treatment of a nickel-based alloy10.1016/j.jmrt.2024.05.128 ↗
41. Surface roughness of selective laser melted Ti-6Al-4V alloy components
42. Optimising surface roughness and density in titanium fabrication via laser powder bed fusion
43. Top surface and side roughness of inconel 625 parts processed using selective laser melting10.1108/13552540910943397 ↗
44. Influences of processing parameters on surface roughness of hastelloy X produced by selective laser melting
45. Surface roughness improvement of Ti-6Al-4V alloy overhang structures via process optimization for laser-powder bed fusion10.1016/j.jmapro.2024.01.008 ↗
46. Additive manufacturing hastelloy X with enhanced properties by optimizing strategies10.1016/j.ijmecsci.2024.109491 ↗
47. Surface roughness analysis, modelling and prediction in selective laser melting10.1016/j.jmatprotec.2012.11.011 ↗
48. Optimization of surface roughness and dimensional accuracy in LPBF additive manufacturing10.1016/j.optlastec.2021.107246 ↗
49. High-power laser powder bed fusion of cu–cr–zr alloy: a comprehensive study on statistical process optimization, microstructure, and mechanical properties10.1016/j.jmapro.2025.06.007 ↗
50. Consolidation phenomena in laser and powder-bed based layered manufacturing10.1016/j.cirp.2007.10.004 ↗
51. Crystallographic texture control of beta-type Ti–15Mo–5Zr–3Al alloy by selective laser melting for the development of novel implants with a biocompatible low Young's modulus10.1016/j.scriptamat.2016.12.038 ↗
52. Stability of crystallographic texture in laser powder bed fusion: understanding the competition of crystal growth using a single crystalline seed
53. Additive manufacturing of metallic components – process, structure and properties10.1016/j.pmatsci.2017.10.001 ↗
54. Strong morphological and crystallographic texture and resulting yield strength anisotropy in selective laser melted tantalum10.1016/j.actamat.2013.04.036 ↗
55. Messler · 2004
56. Controlling texture of NiTi alloy processed by laser powder bed fusion: smart build orientation and scanning strategy
57. Microstructural control during laser powder fusion to create graded microstructure Ni-superalloy components
58. Remelting-based microstructure engineering in laser powder bed fusion: a case study in 316L stainless steel10.1016/j.scriptamat.2024.116469 ↗
59. Effect of non-lamellar α precipitate morphology on the mechanical properties of Ti5553 parts made by laser powder-bed fusion at high laser scan speeds10.1016/j.msea.2022.143039 ↗
60. Effects of post heat treatment on microstructure and mechanical properties of Ti5553 parts made by laser powder bed fusion10.1016/j.jallcom.2022.168616 ↗
61. Microstructure and mechanical properties of the near-beta titanium alloy Ti-5553 processed by selective laser melting10.1016/j.matdes.2016.04.103 ↗
62. Controlling mechanical properties of additively manufactured hastelloy X by altering solidification pattern during laser powder-bed fusion10.1016/j.msea.2019.138081 ↗
63. Anisotropic tensile behavior of laser powder-bed fusion made Ti5553 parts10.1016/j.msea.2023.144633 ↗
64. In-situ microstructure control by laser post-exposure treatment during laser powder-bed fusion
65. Panza-Gios · 2009