Microstructure and mechanical properties of titanium matrix composites with alternating layers α '/β formed by selective laser melting
Source abstract
Abstract
Mo 2 C/Ti6Al4V composites were fabricated via selective laser melting (SLM) with varying Mo 2 C conditions, and the microstructure evolution and mechanical properties were systematically examined. The results reveal that most Mo 2 C particles undergo in-situ reactions with the titanium matrix during SLM processing, resulting in the formation of nanoscale whisker-like TiC. The segregation of Mo promotes β -Ti phase formation, yielding a characteristic microstructure where α′-Ti domains in Mo-poor regions alternate with β -Ti bands in Mo-rich zones. Furthermore, increasing Mo 2 C content facilitates the refinement of both α′ -Ti and primary β -Ti columnar grains. Compared with Ti6Al4V, the titanium matrix composites exhibited 27.2% and 34.3% enhancements in tensile strength and microhardness, respectively. To maintain optimal strength-ductility balance, the optimal Mo 2 C addition should not exceed 2 wt%. The improved mechanical performance is attributed to the synergistic effects of grain refinement strengthening and dispersion strengthening mechanisms, arising from the unique combination of α′ / β microstructures, nano-scale TiC precipitates, and residual Mo 2 C. These findings provide critical guidance for selecting reinforcement materials in additive manufacturing to develop high-performance composite systems.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Laser and Thermal Forming Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (61)
Show source-provided references
1. Selective laser melting to manufacture “In Situ” metal matrix composites: a review10.1002/adem.201801244 ↗
2. Microstructure evolution and mechanical properties in ultra fi ne grained Al/TiC composite fabricated by accumulative roll bonding10.1016/j.compositesb.2015.03.009 ↗
3. Additive manufacturing of metallic components by selective electron beam melting — a review additive manufacturing of metallic components by selective electron beam melting
4. Laser and electron-beam powder-bed additive manufacturing of metallic implants : a review on processes
5. Barriobero-vila P, Gussone J, Haubrich J, Sandlöbes S, Cesar J, Silva D, et al. Inducing stable α+β microstructures during selective laser melting of Ti-6Al-4V using intensified intrinsic heat treatments n.d.:1–14. https://doi.org/10.3390/ma10030268.10.3390/ma10030268 ↗
6. The role of lattice defects, element partitioning and intrinsic heat effects on the microstructure in selective laser melted Ti-6Al-4V10.1016/j.actamat.2019.01.039 ↗
7. Heat treatment possibilities for an in situ β Ti-TiC composite made by laser powder bed fusion
8. Achieving high strength and high ductility in WC-reinforced iron-based composites by laser additive manufacturing
9. Yu · 2019 · 104 · 330
10. International journal of machine tools and manufacture recent developments and opportunities in additive manufacturing of titanium-based matrix composites : a review10.1016/j.ijmachtools.2018.06.003 ↗
11. Gong
12. Selective laser melting of TiC/Ti bulk nanocomposites : influence of nanoscale reinforcement10.1016/j.scriptamat.2012.04.013 ↗
13. Selective laser melting of in-situ TiC/Ti5Si3 composites with novel reinforcement architecture and elevated performance10.1016/j.surfcoat.2010.11.051 ↗
14. Selective laser melting additive manufacturing of Ti-based nanocomposites: the role of nanopowder10.1007/s11661-013-1968-4 ↗
15. Microstructure and tensile properties of laser melting deposited TiC/TA15 titanium matrix composites10.1016/j.jallcom.2009.05.112 ↗
16. Scanning velocity influence on microstructure, microhardness and wear resistance performance of laser deposited Ti6Al4V/TiC composite10.1016/j.matdes.2013.03.049 ↗
17. Interfacial structures and strengthening mechanisms of in situ synthesized TiC reinforced Ti6Al4V composites by selective laser melting10.1016/j.ceramint.2021.08.323 ↗
18. Nano-SiC whisker-reinforced Ti6Al4V matrix composites manufactured by selective laser melting : fine equiaxed grain formation mechanism and mechanical properties10.1016/j.jmatprotec.2023.117981 ↗
19. Corrosion behavior of SiC/Ti6Al4V titanium matrix composites fabricated by SLM10.1016/j.jmrt.2024.06.093 ↗
20. Microstructure evolution and strengthening mechanism of TiC/Ti6Al4 V composites fabricated by selective laser melting during isothermal deformation10.1080/17452759.2024.2374466 ↗
21. Comparative study of microstructures and mechanical properties of in situ Ti-TiB composites produced by selective laser melting, powder metallurgy, and casting technologies10.1557/jmr.2014.122 ↗
22. Selective laser melting of in situ titanium-titanium boride composites: processing, microstructure and mechanical properties10.1016/j.actamat.2014.05.022 ↗
23. Effect of powder particle shape on the properties of in situ Ti-TiB composite materials produced by selective laser melting10.1016/j.jmst.2015.08.007 ↗
24. Graded layered titanium composite structures with TiB2 inclusions fabricated by selective laser melting10.1016/j.compstruct.2016.11.013 ↗
25. Microstructure and mechanical properties of (TiB+TiC)/Ti composites fabricated in situ via selective laser melting of Ti and B 4 C powders
26. Wu · 2024 · vol. 43 · 2805
27. Progress in materials science electromagnetic treatment enhancing performance of metal materials
28. ScienceDirect ScienceDirect ScienceDirect effect of hot isostatic pressure treatment on the electron-beam melted specimens costing models for optimization gary capacity between used capacity and operational efficiency10.1016/j.promfg.2018.02.102 ↗
29. Laser-assisted synthesis of Ti–Mo alloys for biomedical applications10.1016/j.msec.2012.03.007 ↗
30. Heat treatment of Ti6Al4V produced by selective laser melting : microstructure and mechanical properties10.1016/j.jallcom.2012.07.022 ↗
31. ScienceDirect microstructure and mechanical properties of a novel b titanium metallic composite by selective laser melting10.1016/j.actamat.2014.01.018 ↗
32. Laser powder bed fusion of Mo2C/Ti-6Al-4V composites with alternately laminated α′/β phases for enhanced mechanical properties
33. Journal of materials science & technology In-situ formation of Ti-Mo biomaterials by selective laser melting of Ti/Mo and Ti/Mo2C powder mixtures : a comparative study on microstructure , mechanical and wear performance , and thermal mechanisms10.1016/j.jmst.2021.09.017 ↗
34. Materials science & engineering A In-situ modulating laminated microstructure of α+β+TiC in titanium composites by laser powder bed fusion of Mo2C/Ti powder mixture towards biomedical applications10.1016/j.msea.2022.144101 ↗
35. Structure and properties of cast binary Ti-Mo
36. Monshi A, Foroughi MR. Modified scherrer equation to estimate more accurately nano-crystallite size using XRD 2014. https://doi.org/10.4236/wjnse.2012.23020.10.4236/wjnse.2012.23020 ↗
37. Resistivity study and computer modelling of the isothermal transformation kinetics of Ti–6Al–4V and Ti–6Al–2Sn–4Zr–2Mo–010.1016/S0925-8388(00)01227-5 ↗
38. Malinov · 2002 · vol. 48 · 279
39. Geng · 2022 · vol. 15 · 280
40. In situ transformations during SLM of an ultra-strong TiC reinforced Ti composite
41. In fl uence of trace boron addition on microstructure , tensile properties and their anisotropy of Ti6Al4V fabricated by laser directed energy deposition10.1016/j.matdes.2019.107943 ↗
42. Zhang
43. The clarification of a 00 phase precipitate from b phase in Ti-15Mn alloy by mismatch theory10.1016/j.matlet.2017.05.032 ↗
44. Observation and characterization of isothermal α″ in a new β-type titanium alloy10.1080/09500839.2016.1157635 ↗
45. Li · 2008 · vol. 185 · 49
46. G rowth morphologies and mechanism of TiC in the laser surface alloyed coating on the substrate of TiAl
47. Song · 2009 · 311 · 378
48. Growth morphologies and mechanisms of TiC grains during selective laser melting of Ti–Al–C composite powder10.1016/j.matlet.2009.08.043 ↗
49. Xiong · 20151958
50. Yan · 2021 · 174
51. Selective laser melting of low modulus Ti-Mo alloy : a/b heterogeneous conchoidal structure10.1016/j.matlet.2020.127544 ↗
52. Materials science & engineering A evolution of the microstructure and optimization of the tensile properties of the Ti–6Al–4V alloy by selective laser melting and heat treatment10.1016/j.msea.2020.140673 ↗
53. Vilaro T, Colin C, Bartout JD. As-Fabricated and heat-treated microstructures of the Ti-6Al-4V alloy processed by selective laser melting n.d. https://doi.org/10.1007/s11661-011-0731-y.10.1007/s11661-011-0731-y ↗
54. Ceramic reinforced high modulus steel composites: processing, microstructure and properties10.1179/1879139514Y.0000000135 ↗
55. Wegst · 2015 · vol. 14 · 23
56. Refined grain formation behavior and strengthening mechanism of α-titanium with nitrogen fabricated by selective laser melting
57. Reinforcement size dependence of mechanical properties and strengthening mechanisms in diamond reinforced titanium metal matrix composites10.1016/j.compositesb.2018.12.014 ↗
58. ScienceDirect influence of length-scales on spatial distribution and interfacial characteristics of B4C in a nanostructured Al matrix10.1016/j.actamat.2015.01.062 ↗
59. Strength and strain hardening of aluminum matrix composites with randomly dispersed nanometer-length fragmented carbon nanotubes10.1016/j.scriptamat.2013.01.013 ↗
60. Orowan strengthening and forest hardening superposition examined by dislocation dynamics simulations10.1016/j.actamat.2010.06.028 ↗
61. Microstructure evolution and mechanical properties of in-situ Ti6Al4V–TiB composites manufactured by selective laser melting10.1016/j.compositesb.2020.108567 ↗