Microstructure and high-temperature mechanical properties of TP310HCbN welded joint
Source abstract
Abstract
The microstructure of TP310HCbN welded joints and its effect on the tensile and low-cycle fatigue properties were investigated in the temperature range 20–700 °C, particularly in the operating range of 500–700 °C. The results showed that the welded joint was fully austenitic; however, a significantly different microstructure was formed in each welding zone, inducing material inhomogeneity. The material inhomogeneity was most pronounced in the weld metal, wherein an austenitic columnar grain structure composed of dendrite cores and interdendritic regions was developed. A combined analysis of the nanoindentation, failure mechanism, and kernel average misorientation using electron backscatter diffraction revealed that the dendrite core was the softest region in the welded joint and the deformation was localized here, thereby serving as a crack nucleation site and propagation path. This promoted premature failure of the welded joint, resulting in a reduction in the tensile strength, ductility, and the fatigue resistance, in comparison to the base metal. As both the welded joint and base metal showed significant cyclic hardening behavior (more than two-fold increase in the tensile peak stress) during fatigue deformation, the plastic strain energy density was found to be a suitable fatigue parameter, which was invariant throughout the fatigue life. An energy-based unified fatigue life prediction model using material toughness was developed, and its validity was demonstrated by successfully predicting the temperature dependence of the fatigue life as well as the fatigue life reduction of the welded joint.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: High Temperature Alloys and Creep · Fatigue and fracture mechanics · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Microstructure and mechanical properties of HR3C austenitic steel after service10.5604/01.3001.0009.7100 ↗
2. Microstructure evolution and mechanical properties of HR3C steel during long-term aging at high temperature10.1016/S1006-706X(14)60139-4 ↗
3. Microstructure evolution in HR3C austenitic steel during long-term creep at 650 oC10.1016/j.msea.2016.10.077 ↗
4. Investigation the effect of precipitating characteristics on the creep behavior of HR3C austenitic steel at 650 oC10.1016/j.msea.2018.10.124 ↗
5. Welding and weldability of candidate ferritic alloys for future advanced ultrasupercritical fossil power plants10.1179/1362171813Y.0000000152 ↗
6. A process-structure-property model for welding of 9Cr power plant components: the influence of welding process temperatures on in-service cyclic plasticity response10.1016/j.ijpvp.2019.04.015 ↗
7. Assessing corrosion fatigue characteristics of dissimilar material weld between Alloy617 and 12Cr steel using buttering welding technique
8. Digital image correlation study on tensile properties of high strength quenched and tempered steel weld joints prepared by K-TIG and GMAW10.1016/j.msea.2021.142033 ↗
9. Charanterization of heterogenous creep deformation in vanadium-modified 2.25Cr1Mo steel weldments by digital image correlation10.1016/j.msea.2021.141350 ↗
10. Maddox · 1991
11. On the fatigue performance of laser hybrid welded high Zn 7000 alloys for next generation railway components10.1016/j.ijfatigue.2016.05.017 ↗
12. Fatigue design rules for welded structures
13. Microstructure and creep fracture behavior in HR3C/T92 dissimilar steel welds10.1016/j.msea.2020.140128 ↗
14. Tensile and fatigue properties of Super304H welded joint at elevated temperatures10.1016/j.ijfatigue.2020.105989 ↗
15. 2005
16. 2015
17. 2009
18. 2009
19. 2005
20. Effect of Cr content on the corrosion resistance of Ni-Cr-P coatings for PEMFC metallic bipolar plates10.1007/s40243-019-0158-8 ↗
21. Solid state crack repair by friction stir processing in 304L stainless steel10.1016/j.jmst.2017.10.023 ↗
22. Influence of post welding heat treatments on sensitization of AISI 347 stainless steel welded joint10.1016/j.jmrt.2019.11.031 ↗
23. Mutual mechanical effects of ferrite and martensite in a low alloy ferrite-martensite dual phase steel10.1016/j.jallcom.2017.02.287 ↗
24. Evaluation of the thermal aging of ferrite in austenitic stainless steel weld by electrochemical analysis
25. Study of the martensite structure at the weld interface and the fracture toughness of dissimilar metal joint
26. Microstructrual characteristics of fusion zone in continuous wave fiber laser welded Nb-modified δ–TRIP steel10.1016/j.jmrt.2021.09.116 ↗
27. Effect of aging treatment on the microstructures and mechanical properties evolution of 25Cr-20Ni austenitic stainless steel weldments with different Nb Contents10.1016/j.jmst.2018.10.017 ↗
28. Prediction of austenitic weld metal microstructure and properties
29. Coexistence of two distinct fatigue failure mechanisms in Super304H welded joint at elevated temperatures10.1016/j.msea.2021.141465 ↗
30. 2015
31. 2015
32. Temperature effect on the low-cycle fatigue behavior of type 316L stainless steel: cyclci non-stabilization and an invariable fatigue parameter10.1016/j.msea.2006.12.035 ↗
33. BS 7270 · 1990
34. Orientation gradients and geometrically necessary dislocations in ultrafine grained dual-phase steels studied by 2D and 3D EBSD10.1016/j.msea.2010.01.004 ↗
35. Fatigue damage assessment of SUS316L using EBSD and PALS measurements10.1016/j.matchar.2019.05.038 ↗
36. A study of the effects of cyclic thermal stresses on a ductile metal
37. The exponential law of endurance tests
38. Cyclic plastic strain energy and fatigue of metals
39. A new energy-based fatigue damage parameter in life prediction of high-temperature structural material10.1016/j.msea.2008.07.035 ↗