The synergy effect of elements on the oxidation resistance of a high-purity directionally solidification nickel-based superalloy
Source abstract
Abstract
A study on the film characteristics of a Cr2O3-forming nickel-based superalloy is conducted. A triplex structure is observed, in which Ta-Ti layer is developed between the external Cr2O3 and inner Al2O3 layer. When the exposure time increased, Ti atoms are divorced from the Ta-Ti layer, filling the voids inside the Cr2O3 layer, which improve the density of the external Cr2O3 layer and retard the inward penetration of the nitrogen. As a result, the degree of internal nitrides is reduced. Consequently, the synergy effect of Ta and Ti in the Cr2O3 forming alloy is beneficial to improve the oxidation resistance.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: High-Temperature Coating Behaviors · High Temperature Alloys and Creep · Metallurgical Processes and Thermodynamics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (34)
Show source-provided references
1. Reed · 2008
2. Donachie · 2002 · 287
3. Effect of specimen thickness on the creep response of a Ni-based single-crystal superalloy10.1016/j.actamat.2012.06.043 ↗
4. Environmentally-assisted grain boundary attack as a mechanism of embrittlement in a nickel-based superalloy10.1016/j.actamat.2016.12.039 ↗
5. Effect of alloying elements and microstructure on the cyclic oxidation performance of three nickel-based superalloys
6. Oxidation behavior of a single-crystal Ni-base superalloy in Air-ii: at 1000, 1100 and 1150 oC in air10.1023/A:1024629716452 ↗
7. Oxidation behavior of a single-crystal Ni-base superalloy in air at 900, 1000 and 1100 oC10.1007/s11085-006-9016-z ↗
8. Long-term oxidation behavior and mechanism of DD6 Ni-based single crystal superalloy at 1050 °C and 1100 °C in air10.1016/j.jallcom.2017.02.031 ↗
9. Oxidation behavior of a single-crystal Ni-base superalloy between 900 and 1000 oC in air10.1016/j.jallcom.2009.10.261 ↗
10. Oxidation behavior of GTD111 Ni-based superalloy at 900 ◦C in air10.1016/j.corsci.2015.07.031 ↗
11. Chromia layer growth on a Ni-based superalloy: sub-parabolic kinetics and the role of titanium10.1016/j.corsci.2013.05.016 ↗
12. The oxidation characteristics of the nickel-based superalloy, RR1000, at temperatures of 700∼900 oC10.3184/096034012X13341417107382 ↗
13. Short-term isothermal oxidation of hot extruded GH3536 Ni-based superalloy in solid and semi-solid temperature ranges
14. High temperature oxidation behavior of Ni-based superalloy GH20210.1016/j.matchar.2016.05.013 ↗
15. The oxidation of metals at high temperatures
16. Film evolution and growth mechanism of a Ni-based superalloy in the two models at the different temperatures
17. The influence of CrTaO4 layer on the oxidation behavior of a directionally-solidified nickel-based superalloy at 850-900 oC10.1016/j.jallcom.2017.07.066 ↗
18. Ta effect on oxidation of a nickel-based single-crystal superalloy and its sputtered nanocrystalline coating at 900-1100 oC10.1016/j.apsusc.2015.03.157 ↗
19. A study on the multiple stages of oxidation kinetics in a single crystal nickel-based superalloy10.1016/j.corsci.2021.109512 ↗
20. The high temperature oxidation behavior of a superalloy prepared by vacuum induction melting and electron beam smelting: a comparative study
21. Interaction of Ta and Cr on Type-I hot corrosion resistance of single crystal Ni-base superalloys10.1016/j.corsci.2017.01.011 ↗
22. Effect of Ti and Ta on the oxidation of a complex superalloy10.1007/BF00603531 ↗
23. Oxidation of nickel-based single-crystal superalloys for industrial gas turbine applications10.1016/j.actamat.2010.09.027 ↗
24. Knacke · 1991
25. Theoretical analysis of the diffusion processes determining the oxidation rate of alloys
26. Two typical oxidation models on nickel-based superalloys under different initial surface roughness10.1016/j.corsci.2020.108942 ↗
27. Spallation resistance of oxide scales on alloy 617 enhanced by boron addition10.1016/j.corsci.2018.06.002 ↗
28. A comparison of the growth kinetics and scale morphology for three superalloys at 930 °C in air and low PO2 environment10.1023/A:1004658814608 ↗
29. Metallic interconnectors for solid oxide fuel cells-a review
30. Influence of Ta content on hot corrosion behaviour of a directionally solidified nickel base superalloy10.1016/j.jallcom.2014.08.259 ↗
31. Selective oxidation and internal nitridation during high-temperature exposure of single-crystal nickel based superalloys
32. Residential mobility and household energy-saving appliances purchasing behavior in urban areas:Evidence from China
33. QC and MD modelling for predicting the electrochemical stability window of electrolytes: new estimating algorithm10.3390/batteries8120292 ↗
34. Unreported resistance in charge transport limits the photoconversion efficiency of aqueous dye-sensitised solar cells: an electrochemical impedance spectroscopy study