On the impact toughness of amorphous/crystalline metallic laminates
Source abstract
Abstract
The creation of amorphous/crystalline (A/C) laminated structures offers a promising approach towards the production of damage-tolerant A/C metallic materials. However, constraints in fabrication techniques have resulted in limited explorations into the toughening behavior of bulk A/C laminates. This study scrutinizes the impact toughness of macroscale A/C Ni-P/Ni laminates through instrumented Charpy impact testing. The findings reveal that the thickness of the amorphous Ni-P layer significantly influences the impact toughness of A/C Ni-P/Ni laminates. A/C Ni-P/Ni laminates possessing thin Ni-P layers (1 or 4 μm) demonstrated high impact energy, which was comparable to the monolithic coarse-grained (CG) structure; however, the impact energy decreased with the increasing Ni-P layers thickness. Microstructural characterization of the crack-path profile disclosed that the desired impact toughness in the A/C Ni-P/Ni laminate with a thin Ni-P layer is primarily due to intrinsic toughening induced by plastic deformation ahead of the crack tip, and extrinsic toughening afforded by interface delamination. As the Ni-P layer thickens, brittle interface delamination emerges as the dominant extrinsic toughening source to resist fracture, thereby rendering the A/C Ni-P/Ni laminate vulnerable to impact loading. This work not only elucidates the dependence of toughening mechanism on the Ni-P layer thickness in A/C Ni-P/Ni laminates but also proposes an effective strategy for designing damage-tolerant metallic materials subject to impact loading by incorporating thin, brittle amorphous and thick, ductile crystalline materials to create laminated structures.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metallic Glasses and Amorphous Alloys · Laser Material Processing Techniques · Shape Memory Alloy Transformations
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (62)
Show source-provided references
1. Amorphous alloys
2. Mechanical behavior of amorphous alloys10.1016/j.actamat.2007.01.052 ↗
3. Research status and prospect of impact toughness of bulk metallic glasses
4. Effect of carbon nanotubes on the interface evolution and dielectric properties of polylactic acid/ethylene–vinyl acetate copolymer nanocomposites10.1007/s42114-022-00489-0 ↗
5. Direct ink printing reduced graphene oxide/KCu7S4 electrodes for high-performance supercapacitors10.1007/s42114-022-00488-1 ↗
6. A novel nacre-like metal/metal structure by lithography and electrodeposition10.1016/j.jallcom.2021.158853 ↗
7. Impact-resistant nacre-like transparent materials10.1126/science.aaw8988 ↗
8. Bioinspired nacre-like alumina with a bulk-metallic glass-forming alloy as a compliant phase10.1038/s41467-019-08753-6 ↗
9. Reinforcement learning design framework for nacre-like structures optimized for pre-existing crack resistance10.1016/j.jmrt.2023.03.230 ↗
10. Mechanical properties and optimal grain size distribution profile of gradient grained nickel10.1016/j.actamat.2018.04.065 ↗
11. Revealing extraordinary intrinsic tensile plasticity in gradient nano-grained copper10.1126/science.1200177 ↗
12. On the impact toughness of gradient-structured metals10.1016/j.actamat.2020.04.027 ↗
13. A grain-size-dependent structure evolution in gradient-structured (GS) Ni under tension10.1016/j.nanoms.2019.12.004 ↗
14. Dual-gradient structure leads to optimized combination of high fracture resistance and strength-ductility synergy with minimized final catastrophic failure10.1016/j.jmrt.2021.08.102 ↗
15. Effect of amorphous layer thickness on the tensile behavior of bulk-sized amorphous Ni-P/crystalline Ni laminates10.1016/j.matlet.2018.01.164 ↗
16. Interface affected zone for optimal strength and ductility in heterogeneous laminate10.1016/j.mattod.2018.03.006 ↗
17. Role of layered structure in ductility improvement of layered Ti-Al metal composite10.1016/j.actamat.2018.05.005 ↗
18. Heterostructured copper-brass laminates with gradient transition layer10.1016/j.jmrt.2023.02.161 ↗
19. Deformation behavior and bonding properties of Cu/Al laminated composite plate by corrugated cold roll bonding10.1016/j.jmrt.2022.12.135 ↗
20. Synthesis of amorphous/crystalline laminated metals via accumulative roll bonding10.1007/s11837-018-3269-2 ↗
21. Intrinsic and extrinsic size effects in the deformation of amorphous CuZr/nanocrystalline Cu nanolaminates10.1016/j.actamat.2014.07.027 ↗
22. Ductile crystalline–amorphous nanolaminates10.1073/pnas.0702344104 ↗
23. Mechanical behaviour of laminated metal composites10.1179/imr.1996.41.5.169 ↗
24. Plastic deformation mechanisms and size effect of Cu50Zr50/Cu amorphous/crystalline nanolaminate: a molecular dynamics study10.1016/j.commatsci.2016.12.003 ↗
25. Bypassing shear band nucleation and ductilization of an amorphous–crystalline nanolaminate in tension10.1016/j.intermet.2008.06.018 ↗
26. Shear-induced mixing governs codeformation of crystalline-amorphous nanolaminates10.1103/PhysRevLett.113.035501 ↗
27. Amorphous-crystalline Al-based laminates with enhanced plasticity produced by high pressure torsion10.1016/j.matlet.2022.132155 ↗
28. Bulk mechanical alloying of Cu–Ag and Cu/Zr two-phase microstructures by accumulative roll-bonding process10.1016/j.actamat.2006.12.027 ↗
29. 2020
30. 2015 · 1
31. 2005 · 1
32. Fracture toughness and R-curve behavior of laminated brittle-matrix composites10.1007/s11661-998-0220-0 ↗
33. The effect of substrate on the microstructure and tensile properties of electrodeposited nanocrystalline nickel10.1016/S1044-5803(02)00305-4 ↗
34. Microstructural development of an electrodeposited Ni layer10.1016/j.tsf.2010.03.016 ↗
35. Effect of delamination and grain refinement on fracture energy of ultrafine-grained steel determined using an instrumented Charpy impact test10.3390/ma15030867 ↗
36. Fracture of metal/ceramic laminates—II. Crack growth resistance and toughness10.1016/S1359-6454(98)00358-9 ↗
37. Dramatically enhanced impact toughness of two-scale laminate-network structured composites10.1016/j.matdes.2017.11.067 ↗
38. Effect of crystallinity on the impact toughness of a La-based bulk metallic glass10.1016/S1359-6454(00)00052-5 ↗
39. Cryogenic Charpy impact testing of metallic glass matrix composites10.1016/j.scriptamat.2011.11.011 ↗
40. Embrittlement of a bulk metallic glass due to sub-Tg annealing10.1016/j.actamat.2004.11.040 ↗
41. Ductile to brittle transition in the Zr41. 2Ti13. 75Cu12. 5Ni10Be22. 5 bulk metallic glass10.1016/j.intermet.2006.01.032 ↗
42. On factors influencing the ductile-to-brittle transition in a bulk metallic glass10.1016/j.actamat.2009.03.047 ↗
43. Deformation and fracture behavior of a natural shell ceramic: coupled effects of shell shape and microstructure10.1016/j.msec.2018.05.002 ↗
44. Conch shell structure and its effect on mechanical behaviors10.1016/S0142-9612(03)00555-6 ↗
45. Damage-tolerance strategies for nacre tablets10.1016/j.jsb.2016.02.017 ↗
46. Processing and mechanical properties of hydroxyapatite–polysulfone laminated composites10.1016/j.jeurceramsoc.2013.11.002 ↗
47. On the exceptional damage-tolerance of gradient metallic materials10.1016/j.mattod.2019.09.023 ↗
48. On the fracture toughness of advanced materials10.1002/adma.200803322 ↗
49. Co-existence of homogeneous flow and localized plastic deformation in tension of amorphous Ni-P films on ductile substrate10.1016/j.actamat.2016.01.001 ↗
50. Mechanical properties and optimum layer thickness in an amorphous Ni–P/coarse-grained Ni bi-layered structure10.1016/j.msea.2019.05.105 ↗
51. Influence of the alumina thickness at the interfaces on the fracture mechanisms of aluminium multilayer composites10.1016/j.msea.2008.05.015 ↗
52. The conflicts between strength and toughness10.1038/nmat3115 ↗
53. Interlaminar fracture toughness and toughening of laminated composite materials: a review10.1016/0010-4361(89)90211-5 ↗
54. On the mechanistic origins of toughness in bone10.1146/annurev-matsci-070909-104427 ↗
55. Meyers · 2009
56. Mechanisms of fatigue-crack propagation in ductile and brittle solids10.1023/A:1018655917051 ↗
57. On the adhesion performance of gradient-structured Ni–P metallic coatings10.1016/j.msea.2022.143170 ↗
58. Effect of film gradient profile on adhesion strength, residual stress and effective hardness of functionally graded diamond-like carbon films10.1016/j.apsusc.2014.05.161 ↗
59. A novel approach to developing biomimetic (“Nacre-Like”) metal-compliant-phase (Nickel–Alumina) ceramics through coextrusion10.1002/adma.201602471 ↗
60. Merger of structure and material in nacre and bone–Perspectives on de novo biomimetic materials10.1016/j.pmatsci.2009.05.001 ↗
61. Tough, bio-inspired hybrid materials10.1126/science.1164865 ↗
62. A review of impact resistant biological and bioinspired materials and structures10.1016/j.jmrt.2020.10.062 ↗