journal article·2023-11Open access

Surface self-nanocrystallization and -lubricating dependent wear resistance of austenitic steels at same initial hardness level

Ting Zhao, Chen Chen, Zhiqing Lin, Zekui Wang, Xu Dong, Yuefeng Wang, Zhinan Yang, Bo Lv, Fucheng Zhang

Abstract

In the present paper, two austenitic wear-resistant steels, namely 110Mn13 and 0Cr17Ni10Mn5Mo2 steels, were cold-rolled to a same hardness level of ∼270HV. Mechanical properties and wear resistance under various applied loads were tested. The deformed microstructure, worn surface morphologies and wear debris were discussed to analyze the wear resistance. Results showed that a higher density of deformation twins and dislocations were generated in the 0Cr17Ni10Mn5Mo2 steel to reach a same hardness level with the 110Mn13 steel. Consequently, the 0Cr17Ni10Mn5Mo2 steel obtained higher yield strength (736 MPa) but lower ultimate strength (896 MPa), elongation (30.5%) and strain hardening rate than the 110Mn13 steel when the impact absorption energies were at a similar level of ∼170 J. The weight loss of the 0Cr17Ni10Mn5Mo2 steel reduced by over 40% compared to that of the 110Mn13 steel under the selected wear conditions. With the cold-rolled microstructure, the worn surface of both the test steels produced nanocrystalline layers. The nanocrystalline layer thickness of the 0Cr17Ni10Mn5Mo2 steel was over 5 μm, far larger than that of the 110Mn13 steel. Meanwhile, with the wear debris containing Cr-oxide adhering to the worn surface, which could facilitate the self-lubricating effect, the 0Cr17Ni10Mn5Mo2 steel presented better wear resistance than the 110Mn13 steel.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Metal Alloys Wear and Properties · Surface Treatment and Residual Stress

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Effect of N + Cr alloying on the microstructures and tensile properties of Hadfield steel10.1016/j.msea.2016.09.106 ↗
2. Review on research progress of steel and iron wear-resistant materials
3. Research and application of high Mn steel lining plate
4. High speed pounding: a novel technique for the preparation of a thick surface layer with a hardness gradient distribution on Hadfield steel10.1016/j.scriptamat.2010.11.043 ↗
5. Explosion hardening of Hadfield steel crossing10.1179/174328408X363263 ↗
6. Effect of explosion hardening on impact abrasive wear behavior of Hadfield steel
7. Deformation, fracture, and wear behaviours of C + N enhancing alloying austenitic steels10.1016/j.msea.2012.08.063 ↗
8. Impact–abrasive–corrosion wear of Fe-based alloys: influence of microstructure and chemical composition upon wear resistance10.1016/j.wear.2013.06.006 ↗
9. Wear behavior and the corresponding work hardening characteristics of Hadfield steel10.1016/j.triboint.2018.01.044 ↗
10. Wear resistance improvement of austenitic 316L steel by laser alloying with boron10.1016/j.surfcoat.2016.02.058 ↗
11. Effect of pack-boriding on the tribological behavior of hardox 450 and HiTuf steels10.1515/rams-2020-0030 ↗
12. Dry sliding wear behavior of boron-doped AISI 1020 steels10.12693/APhysPolA.132.455 ↗
13. Dry sliding wear behavior of boron-doped 205 manganese steels10.1007/s11665-020-04796-9 ↗
14. On the comparison of the abrasive wear behavior of aluminum alloyed and standard Hadfield steels10.1016/j.wear.2009.07.010 ↗
15. Effect of Mo alloying on wear behavior of Hadfield steel10.3901/JME.2020.14.081 ↗
16. On the comparison of microstructural characteristics and mechanical properties of high-vanadium austenitic manganese steels with the Hadfield steel10.1016/j.msea.2011.10.089 ↗
17. Strain hardening and nanocrystallization behaviors in Hadfield steel subjected to surface severe plastic deformation10.1016/j.msea.2018.05.059 ↗
18. The effect of contact area on velocity weakening of the friction coefficient and friction instability: a case study on brake friction materials10.1016/j.triboint.2019.02.034 ↗
19. Microstructure and wear behaviors of laser clad NiCr/Cr3C2–WS2 high temperature self-lubricating wear-resistant composite coating10.1016/j.apsusc.2011.12.021 ↗
20. Nanocrystalline advanced high strength steel produced by cold rolling and annealing10.1007/s11661-016-3394-x ↗
21. Wear behaviour of nanocrystallised Hadfield steel10.1016/j.wear.2012.11.038 ↗
22. Corrosion behaviour of nanocrystalline 304 stainless steel prepared by equal channel angular pressing10.1016/j.corsci.2011.08.049 ↗
23. Preparation of nanocrystalline 430L stainless steel by HEBM and SPS10.1016/S1006-706X(08)60147-8 ↗
24. Microstructural evolution and mechanical properties of nanocrystalline Fe–Mn–Al–C steel processed by high-pressure torsion10.1016/j.msea.2021.142073 ↗
25. Surface nanocrystallization of metallic alloys with different stacking fault energy induced by laser shock processing10.1016/j.matdes.2016.05.028 ↗
26. Simulation for surface self-nanocrystallization under shot peening10.1007/BF02487679 ↗
27. Laser shock peening induced surface nanocrystallization and martensite transformation in austenitic stainless steel10.1016/j.jallcom.2015.06.268 ↗
28. The significance of near surface microstructure in the wear process10.1016/0043-1648(78)90125-4 ↗
29. Recent progress on wear-resistant materials: designs, properties, and applications10.1002/advs.202003739 ↗
30. Design of TiZrNbTa multi-principal element alloys with outstanding mechanical properties and wear resistance10.1016/j.msea.2022.143203 ↗
31. Influence of oxides on the formation of self-lubricating layer and anti-wear performance during sliding10.1016/j.triboint.2022.108188 ↗
32. Tribological studies of chromium oxide films for magnetic recording applications10.1016/S0040-6090(97)00453-7 ↗