journal article·2024-03Open access

Enhanced high-temperature mechanical properties of the Cu–1.16Ni–0.36Cr alloy owing to interactions between metastable precipitates and dislocations

Shaolin Li, Wenming Sun, Kexing Song, Qiangsong Wang, Yingying Zhu

Abstract

Herein, an alloy Cu–1.16Ni–0.36Cr with outstanding high-temperature mechanical properties was obtained, and the underlying mechanism was discussed. The properties were compared with those of commercial Cu–Fe–P alloys. The alloy exhibited a high-temperature softening temperature of 674.7 °C. Tensile tests conducted at high temperatures revealed that at 700 °C, the alloy maintained a tensile strength of 131.3 MPa, whereas Cu–Fe–P alloys only exhibited a tensile strength of 58.7 MPa. Microstructural analysis revealed the formation of nanoscale Ni3Cr7 precipitates near fractures at high temperatures, with the average size being approximately 10 nm. These nanoscale precipitates hindered the coarsening of Cr particles and dislocation slips, forming dislocation rings and substantially enhancing the high-temperature mechanical properties of the alloy. Furthermore, the nanoscale precipitates considerably impeded the growth and expansion of recrystallized grains. After a high-temperature treatment at 700 °C, a portion of the microstructure in the alloy remained stretched, with the small-angle grain boundaries being high (68.2%) and the recrystallization degree being only 50.4%.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Microstructure and mechanical properties · Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Breedis · 2016
2. Evolution of microstructure and residual stress for a lead-frame Cu-2.13 Fe-0.026 P (wt.%) alloy10.1016/j.jallcom.2023.171383 ↗
3. Effect of Si additions on mechanical properties and softening resistance of Cu–Ni-Sn-P alloy10.1016/j.mtcomm.2023.105394 ↗
4. 4H-SiC integrated circuits for high-temperature applications
5. Effect of annealing temperature on dual-structure coexisting precipitates in Cu–2.18 Fe–0.03 P alloy and softening mechanism at high temperature10.1007/s10853-022-07910-5 ↗
6. Microstructure, residual stress, and mechanical properties evolution of a Cu–Fe–P alloy under different conditions10.1016/j.jmrt.2023.05.015 ↗
7. Microstructure and properties of Cu–2.3 Fe–0.03 P alloy during thermomechanical treatments10.1016/S1003-6326(15)63757-8 ↗
8. Effect of Fe particle on the surface peeling in Cu− Fe− P lead frame10.1007/BF02840870 ↗
9. Study of the coarsening and hardening behaviors of coherent g-Fe particles in Cu-2.1 Fe alloy
10. Effect of annealing temperature on microstructure, properties and residual stress of C19400 alloy
11. Calculation of the nickel-chromium-copper phase diagram from binary data10.1016/0001-6160(57)90099-8 ↗
12. Microstructural behavior and mechanical hardening in a Cu-Ni-Cr alloy10.1007/BF00541804 ↗
13. Hernandez-Santiago · 2010 · vol. 654 · 2346
14. The effect of heat treatment on precipitate in the Cu-Ni-Al alloy Hiduron® 13010.1016/j.msea.2017.03.069 ↗
15. Microstructure and properties of a novel Cu-Cr-Yb alloy with high strength, high electrical conductivity and good softening resistance
16. Effects of Y addition on the microstructure, properties and softening resistance of Cu-Cr alloy10.1016/j.jallcom.2022.163816 ↗
17. Precipitate evolution in Cux [Ni3Cr1] spinodal alloys under mismatch control10.1016/j.matchemphys.2018.11.035 ↗
18. Stability of binary precipitates in Cu-Ni-Si-Cr alloys investigated through active learning10.1016/j.matchemphys.2023.128053 ↗
19. Precipitate of an intermetallic phase with Pt 2 Mo-type structure in alloy 62510.1007/s11661-999-0194-6 ↗
20. An experimental study on the ordered alloy Ni_2Cr10.2320/matertrans1960.10.365 ↗
21. Deformation twinning versus slip in Ni-based alloys, containing Pt2Mo-structured, Ni2Cr-typed precipitates10.1016/j.matdes.2021.109820 ↗
22. Role of Fe in long-range ordered Ni2Cr precipitates in Ni-Cr-Fe model alloys during isothermal aging
23. Significantly enhanced high-temperature mechanical properties of Cu-Cr-Zn-Zr-Si alloy with stable second phases and grain boundaries10.1016/j.matdes.2023.112292 ↗
24. Effect of Ni and Mn contents on the microstructure and properties of Cu-Ni-Mn-P alloy10.1016/j.jallcom.2022.163636 ↗
25. Strengthening mechanism and effect of Al2O3 particle on high-temperature tensile properties and microstructure evolution of W–Al2O3 alloys
26. Significant enhancement in high-temperature tensile strength of trace nano-Y2O3-reinforced TiAl alloy prepared by selective electron beam melting
27. Effects of temperature and strain rate on tensile properties of Cu-Cr-Zr-Ti Alloy10.1016/j.msea.2016.05.035 ↗
28. Effects of cold rolling reduction rate on the microstructure and properties of Cu-1.16 Ni-0.36 Cr alloy after thermo-mechanical treatment10.3390/ma16196508 ↗
29. Strengthening and high-temperature softening resistance of low Si-added Cu–Cr–Zr alloy for fusion reactor application
30. Cr-based second phases in a high conductivity Cu-Cr-Nb alloy with high high-temperature strength10.1016/j.matdes.2022.110784 ↗