Rolling contact fatigue property of gradient rare earth addition M50 bearing steel with surface nano-grains and its inhibited martensite decay
Source abstract
Abstract
A gradient nanostructured surface layer of ∼600 μm in thickness was prepared on M50 steel with rare earth additions by a surface mechanical rolling treatment. The initial microstructure was refined into nanosized grains (∼29 nm in diameter) in the top surface layer, causing a significant increase of surface hardness. Meanwhile, the grain size increases, and the microhardness decreases gradually to the matrix values with increasing depth. Rolling contact fatigue tests showed that the fatigue lives are significantly increased by the gradient nanostructured surface layer. Analysis of failure mechanism revealed that both softening in the near surface layer and hardening in the subsurface occur under rolling contact testing. And surface spalling is the predominant failure mode, of which the cracks initiate from primary carbides in the top surface layer owing to surface softening. In gradient nanostructured samples, the nano-grains inhibit carbon migration by impeding dislocation movement in the near surface layer, so that martensite decay is suppressed. Consequently, the crack initiation is inhibited, and the fatigue property is enhanced.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metal Alloys Wear and Properties · Surface Treatment and Residual Stress · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (52)
Show source-provided references
1. Steels for bearings10.1016/j.pmatsci.2011.06.002 ↗
2. The effect of ion implantation on the fatigue life and corrosion resistance of M50 steel bearings10.1016/0257-8972(95)08349-9 ↗
3. Failure analysis of an inter-shaft bearing of an aero gas turbine engine10.1007/s11668-015-9933-8 ↗
4. Failure analysis of bearings of aero-engine10.1007/s11668-019-00746-3 ↗
5. Damage evolution around primary carbides under rolling contact fatigue in VIM–VAR M5010.1016/j.ijfatigue.2016.05.026 ↗
6. Understanding the factors controlling rolling contact fatigue damage in VIM-VAR M50 steel10.1016/j.ijfatigue.2017.10.018 ↗
7. Rolling contact fatigue behaviour of M50 bearing steel with rare earth addition10.1016/j.ijfatigue.2023.107940 ↗
8. Comprehensive analysis of nitriding behavior and synergistic strengthening mechanism on quenched M50 steel10.1016/j.surfcoat.2022.128307 ↗
9. Dual-strengthening of steel surface and bulk via synergistic effect of plasma nitriding: a case study of M50 steel10.1016/j.surfcoat.2021.126910 ↗
10. The microstructure and tribological properties of M50 steel surface after titanium ion implantation10.1016/j.apsusc.2021.150349 ↗
11. The microstructure of Ta alloying layer on M50 steel after surface alloying treatment induced by high current pulsed electron beam10.1016/j.vacuum.2016.11.036 ↗
12. Tribological performance of a novel wide-temperature applicable a-C/(WC/a-C) film against M50 steel10.1016/j.triboint.2020.106189 ↗
13. Improving the tribological properties of AISI M50 steel using Sns/Zno solid lubricants10.1016/j.jallcom.2019.153494 ↗
14. Microstructure and tribological performances of M50 bearing steel processed by ultrasonic surface rolling10.1016/j.triboint.2022.107818 ↗
15. A continuum damage mechanics based approach to damage evolution of M50 bearing steel considering residual stress induced by shot peening10.1016/j.triboint.2018.05.023 ↗
16. Understanding the nanostructure evolution and the mechanical strengthening of the M50 bearing steel during ultrasonic shot peening10.1016/j.msea.2022.142721 ↗
17. Ultrastrong gradient M50 bearing steel with lath-shape nano-martensite by ultrasonic shot peening and its enhanced wear resistance at elevated temperature10.1016/j.matdes.2024.112786 ↗
18. Fatigue behaviors of AISI 316L stainless steel with a gradient nanostructured surface layer10.1016/j.actamat.2014.12.057 ↗
19. Revealing extraordinary intrinsic tensile plasticity in gradient nano-grained copper10.1126/science.1200177 ↗
20. Simultaneous enhancement of stress- and strain-controlled fatigue properties in 316L stainless steel with gradient nanostructure10.1016/j.actamat.2019.02.008 ↗
21. Strain-induced formation of a gradient nanostructured surface layer on an ultrahigh strength bearing steel10.1016/j.jmst.2017.12.012 ↗
22. Enhanced fatigue property by suppressing surface cracking in a gradient nanostructured bearing steel10.1080/21663831.2016.1253625 ↗
23. Residual stress. Part 1 – measurement techniques10.1179/026708301101509980 ↗
24. Enhanced rolling contact fatigue property of a rare earth addition bearing steel with a gradient nanostructured surface layer10.1016/j.jmst.2024.06.005 ↗
25. YB/T 5345-2014. Metallic materials-Rolling contact fatigue test.
26. In situ investigation of the fracture of primary carbides and its mechanism in M50 steel10.1016/j.matchar.2022.111822 ↗
27. A statistical distribution function of wide applicability10.1115/1.4010337 ↗
28. The progression of surface rolling contact fatigue damage of rolling bearings with artificial dents10.1080/10402004.2014.983251 ↗
29. Atom probe tomography analysis of the white etching layer in a rail track surface10.1016/j.actamat.2010.02.030 ↗
30. Development of white etching layers on rails: simulations and experiments10.1016/j.wear.2016.03.028 ↗
31. Microstructural evolution of white and brown etching layers in pearlitic rail steels10.1016/j.actamat.2019.04.012 ↗
32. Plasticity of lath martensite by sliding of substructure boundaries10.1016/j.scriptamat.2016.04.006 ↗
33. Lath martensite plasticity enabled by apparent sliding of substructure boundaries10.1016/j.matdes.2019.107646 ↗
34. Enhanced mechanical properties and corrosion resistance of 316L stainless steel by pre-forming a gradient nanostructured surface layer and annealing10.1016/j.actamat.2021.116773 ↗
35. Stabilizing nanostructures in metals using grain and twin boundary architectures10.1038/natrevmats.2016.19 ↗
36. Low-oxygen rare earth steels10.1038/s41563-022-01352-9 ↗
37. Enhanced thermal stability of nanograined metals below a critical grain size10.1126/science.aar6941 ↗
38. Johnson · 1985
39. Thermodynamics and kinetics of phase transformation in rare earth–magnesium alloys: a critical review10.1016/j.jmst.2020.01.022 ↗
40. Notch sensitivity in fatigue limit of high strength steel10.2355/tetsutohagane.TETSU-2015-045 ↗
41. The role of carbon in the white etching crack phenomenon in bearing steels10.1016/j.actamat.2020.11.022 ↗
42. Strain-induced martensite decay in bearing steels under rolling contact fatigue: modelling and atomic-scale characterisation10.1016/j.actamat.2017.08.005 ↗
43. A unified theory for microstructural alterations in bearing steels under rolling contact fatigue10.1016/j.actamat.2018.05.056 ↗
44. Modelling and characterisation of stress-induced carbide precipitation in bearing steels under rolling contact fatigue10.1016/j.actamat.2017.02.006 ↗
45. Effect of block size on the strength of lath martensite in low carbon steels10.1016/j.msea.2005.12.048 ↗
46. Martensite in steel: strength and structure10.1016/S0921-5093(99)00288-9 ↗
47. Block and sub-block boundary strengthening in lath martensite10.1016/j.scriptamat.2016.01.043 ↗
48. Effect of martensitic morphology on mechanical properties of an as-quenched and tempered 25CrMo48V steel10.1016/j.msea.2011.11.078 ↗
49. Combined strengthening from nanotwins and nanoprecipitates in an iron-based superalloy10.1016/j.actamat.2018.04.001 ↗
50. Atomistic tensile deformation mechanisms of Fe with gradient nano-grained structure10.1063/1.4928448 ↗
51. Molecular dynamics simulation study of the effect of grain size on the deformation behavior of nanocrystalline body-centered cubic iron10.1016/j.scriptamat.2010.11.019 ↗
52. Influence of residual stresses on the crack initiation and short crack propagation in a martensitic spring steel10.3390/met12071085 ↗