Characteristics of oxide films on TA16 alloy after long-term exposure in simulated secondary circuit water environment of small modular reactor
Source abstract
Abstract
Currently, little is known about the characteristics of oxide films on Ti alloys exposed to the secondary circuit water environment of small modular reactors (SMRs). In this study, multiple microstructural characterization techniques were employed to meticulously characterize the oxide film characteristics of the TA16 alloy after 6000 h and 8000 h of exposure to a simulated SMR secondary circuit water environment. The results indicate that the oxide films on the 6000 h specimen are composed of a microcrystalline anatase TiO 2 interior layer and a coarse-grained anatase TiO 2 exterior layer, while the oxide film on the 8000 h specimen typically consists of a microcrystalline anatase TiO 2 inner layer, an NiFe 2 O 4 middle layer, and a coarse-grained anatase TiO 2 outer layer. As the corrosion time is extended to 8000 h, the presence of NiFe 2 O 4 oxide particles can be attributed to oxide deposition by the 316L stainless steel autoclave used in the corrosion experiments, which results in the migration of Ni and Fe ions onto the surface of the Ti alloy.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Nuclear Materials and Properties · Titanium Alloys Microstructure and Properties · Hydrogen embrittlement and corrosion behaviors in metals
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Recent advances in processing of titanium alloys and titanium aluminides for space applications: a review10.1557/s43578-021-00104-w ↗
2. Titanium alloy production technology, market prospects and industry development10.1016/j.matdes.2010.09.011 ↗
3. Small modular reactors: an overview of modeling, control, simulation, and applications10.1109/ACCESS.2024.3351220 ↗
4. Thermal hydraulics analysis of a helical coil steam generator of a small modular reactor10.1016/j.anucene.2017.06.002 ↗
5. Small modular reactors: simpler, safer, cheaper?10.1016/j.energy.2012.01.078 ↗
6. Formation of oxide films on titanium alloys under the conditions of the primary circuit of light-water nuclear reactors (a review)
7. High temperature oxidation behavior and research status of modifications on improving high temperature oxidation resistance of titanium alloys and titanium aluminides: a review10.1016/j.jallcom.2016.06.212 ↗
8. Protection of titanium alloy components against high temperature corrosion10.1016/S0921-5093(03)00150-3 ↗
9. Characterization of oxide layers on Ti–2Al–2.5Zr and Ti–4Al–2V alloys oxidized at 300 °C in a neutral water steam
10. Titanium dissolution-passivation in highly chloridic and oxygenated aqueous solutions reaction mechanism extended to supercritical water conditions10.1149/1.1787171 ↗
11. Sorption of (137)Cs and (60)Co on titanium oxide films in light water reactor primary circuit environment10.3390/ma15124261 ↗
12. Oxide formation on titanium alloys in primary water of nuclear pressurised water reactor10.1016/j.corsci.2019.01.020 ↗
13. Corrosion of titanium alloys in pressurised water at 300 °C: kinetics and modelling10.1016/j.corsci.2021.109646 ↗
14. Corrosion behavior of nickel base alloys, stainless steel and titanium alloy in supercritical water containing chloride, phosphate and oxygen10.1016/j.cherd.2015.05.003 ↗
15. The effect of molten phosphate on corrosion of 316 stainless steel, alloy 625, and titanium TA8 in supercritical water oxidation conditions10.3390/ma16010395 ↗
16. Corrosion of titanium alloys in high temperature seawater10.14773/cst.2015.14.4.195 ↗
17. Influence of high-temperature water vapor on titanium film surface10.1007/s11085-016-9630-3 ↗
18. Microstructure, texture, and hardness evolution of cold-rolled high-purity Ti sheet during annealing at 350 °C to 550 °C10.1007/s11661-022-06651-z ↗
19. Microstructural characterization and hardness variation of pure Ti surface-treated by pulsed laser10.1016/j.jallcom.2018.01.113 ↗
20. Corrosion behavior of TA16 titanium alloy during long-term exposure in simulated water environment of small modular reactor10.1016/j.jmrt.2023.11.122 ↗
21. Pourbaix diagrams for chromium, aluminum and titanium extended to high-subcritical and low-supercritical conditions10.1016/j.corsci.2012.02.002 ↗
22. Mechanistic understanding of the localized corrosion behavior of laser powder bed fused 316L stainless steel in pressurized water reactor primary water10.1016/j.scriptamat.2023.115764 ↗
23. Corrosion behavior of selected structural materials in a simulated steam-cycle high-temperature gas-cooled reactor helium environment10.13182/NT79-A19223 ↗
24. Study of corrosion kinetics and microstructure of α-phase pure titanium tube in environment 300°C and 8.6MPa water10.1016/j.corsci.2019.108217 ↗
25. Corrosion of titanium alloys in pressurised water at 350 °C and 17.5 MPa10.1016/j.corsci.2022.110268 ↗