Interfacial texture-driven failure behaviors of Gd/Yb co-doped YSZ thermal barrier coatings under thermal cyclic loading: Design and optimization
Source abstract
Abstract
Double ceramic layer (DCL) thermal barrier coatings (TBCs) with excellent thermal shock resistance have been developed but are weakest at the inter-ceramic interface. It is desirable to improve the interfacial bonding between the ceramic layers to further enhance service reliability. In this study, an interfacial texture deposition strategy was proposed to strengthen the inter-ceramic interface of the self-developed DCL TBCs. Specifically, eight interfacial textures were deposited at the interfaces between YSZ and RYSZ (where R represents two rare-earth oxides, Gd 2 O 3 and Yb 2 O 3 , R = 6.5 wt%) layers, followed by thermal cycling tests to explore their critical roles in the failure behaviors of DCL TBCs. Microstructural evolutions, phase compositions, and stress variations were investigated in detail. The relationship between texture and interfacial separation was identified. A denser texture spacing led to a smaller flaking area. Ultimately, the coating performance reached its optimum when the interfacial texture had a diameter of 2.5 mm, a spacing of 1.5 mm, and a height of 200 μm. After 230 thermal cycles at 1150 °C, the flaking area was only 23 % of that observed in untextured TBCs, and the layer RYSZ did not undergo phase transformation. This study provides theoretical support for interfacial texture and lanthanide-doped YSZ design of TBCs.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Nuclear Materials and Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (54)
Show source-provided references
1. New generation aero combustor
2. Thermal barrier coatings for gas-turbine engine applications
3. Present status and future prospects of plasma sprayed multilayered thermal barrier coating systems10.1016/j.jeurceramsoc.2020.03.016 ↗
4. Mechanisms controlling the durability of thermal barrier coatings10.1016/S0079-6425(00)00020-7 ↗
5. Microstructural characterization of GZ/CYSZ thermal barrier coatings after thermal shock and CMAS+ hot corrosion test10.1016/j.jeurceramsoc.2017.02.004 ↗
6. Mechanics-based scaling laws for the durability of thermal barrier coatings10.1016/S0079-6425(00)00007-4 ↗
7. Advanced structural ceramics in aerospace propulsion10.1038/nmat4687 ↗
8. Oxidation and degradation of a plasma-sprayed thermal barrier coating system10.1016/S0257-8972(96)02985-4 ↗
9. Effect of temperature on rumpling and thermally grown oxide stress in an EB-PVD thermal barrier coating10.1016/j.surfcoat.2006.07.212 ↗
10. Characterization of a cyclic displacement instability for a thermally grown oxide in a thermal barrier system10.1016/S1359-6454(01)00071-4 ↗
11. A numerical assessment of the durability of thermal barrier systems that fail by ratcheting of the thermally grown oxide10.1016/S1359-6454(03)00194-0 ↗
12. Enhancement of strain tolerance of functionally graded LaTi2Al9O19 thermal barrier coating through ultra-short pulse based laser texturing10.1016/j.surfcoat.2016.07.018 ↗
13. Improved the durability of thermal barrier coatings with interface modified by three-dimensional mesh patterns10.1111/jace.14360 ↗
14. Thermal barrier coatings with interface modified by 3D mesh patterns: failure analysis and design optimization10.1111/jace.15386 ↗
15. Crack propagation modeling on the interfaces of thermal barrier coating system with different thickness of the oxide layer and different interface morphologies10.1016/j.matdes.2011.05.039 ↗
16. Laser surface patterning to enhance adhesion of plasma sprayed coatings10.1016/j.surfcoat.2015.07.022 ↗
17. The behavior of plasma sprayed thermal barrier coating with laser microtextured bond coat under high temperature testing10.1016/j.surfcoat.2022.129095 ↗
18. Bioinspired multiscale wet adhesive surfaces: structures and controlled adhesion
19. High temperature durability of a bond-coatless plasma-sprayed thermal barrier coating system with laser textured Ni-based single crystal substrate10.1016/j.surfcoat.2018.01.006 ↗
20. Improvement of strain tolerance of functionally graded TBCs through laser surface micro-texturing10.1007/s10853-016-0363-0 ↗
21. Laser surface texturing (LST) treatment before thermal spraying: a new process to improve the substrate-coating adherence10.1016/j.surfcoat.2010.07.044 ↗
22. Laser-induced concave/convex micro-textures array for enhancing performance of surface coatings: bond coating in thermal barrier coating system10.1016/j.jmapro.2024.03.027 ↗
23. Laser texturing at interface for improved strain tolerance and thermal insulation performance of thermal barrier coatings10.1016/j.surfcoat.2023.129385 ↗
24. Optimization selection of the thermal conductivity of the top ceramic layer in the Double-Ceramic-Layer Thermal Barrier Coatings based on the finite element analysis of thermal insulation10.1016/j.surfcoat.2013.12.047 ↗
25. Finite element simulation of stress distribution and development in 8YSZ and double-ceramic-layer La2Zr2O7/8YSZ thermal barrier coatings during thermal shock10.1016/j.apsusc.2011.11.109 ↗
26. Behavior and mechanism of the stress buffer effect of the inside ceramic layer to the top ceramic layer in a double-ceramic-layer thermal barrier coating10.1016/j.ceramint.2013.10.021 ↗
27. Mechanisms of cracking and delamination within thick thermal barrier systems in aero-engines subject to calcium-magnesium-alumino-silicate (CMAS) penetration10.1016/j.msea.2008.01.006 ↗
28. Crack deflection at an interfaceof alumina/metal joint: a numerical analysis10.1016/j.commatsci.2006.04.006 ↗
29. Impact of interfacial texture on failure behaviour of 8YSZ thermal barrier coatings under thermal cyclic loading10.1016/j.jeurceramsoc.2024.04.059 ↗
30. Mixed-mode interfacial fracture toughness for thermal barrier coating10.1016/j.engfracmech.2006.10.021 ↗
31. Kinking of a crack out of an interface10.1115/1.3176078 ↗
32. Multiscale monitoring of interface failure of brittle coating/ductile substrate systems: a non-destructive evaluation method combined digital image correlation with acoustic emission10.1063/1.3651378 ↗
33. Interface crack between two elastic layers10.1007/BF00018123 ↗
34. Analytical modelling of oxide thickness effect on residual stresses in thermal barrier coatings10.1016/S1359-6462(99)00430-3 ↗
35. Bioinspired multiscale wet adhesive surfaces: structures and controlled adhesion
36. High temperature durability of a bond-coatless plasma-sprayed thermal barrier coating system with laser textured Ni-based single crystal substrate10.1016/j.surfcoat.2018.01.006 ↗
37. Optimization of process parameters for thermal shock resistance and thermal barrier effects of 8YSZ thermal barrier coatings through orthogonal test10.1063/5.0053054 ↗
38. Laser texturing at interface for improved strain tolerance and thermal insulation performance of thermal barrier coatings10.1016/j.surfcoat.2023.129385 ↗
39. Subtle variation in lattice parameter and thermal expansion due to heating and cooling of a high-entropy fluorite oxide (Zr0.2Ce0.2Hf0.2Y0.2Al0.2)O2-δ between 1200 and 1500 °C in air10.1016/j.ceramint.2023.08.135 ↗
40. Thermal shock testing of burner cans coated with a thick thermal barrier coating10.1361/105996398770350828 ↗
41. Crack behaviour and failure mechanisms of air plasma sprayed (Gd, Yb) doped YSZ thermal barrier coatings under oxy-acetylene flame thermal shock10.1016/j.ceramint.2024.09.417 ↗
42. The crack behavior and delamination mechanisms of air plasma sprayed thermal barrier coatings under ultrasonic plasma jet at 1600 °C10.1016/j.jeurceramsoc.2023.03.005 ↗
43. Extending interfacial toughness and thermal cycling lifetime of thermal barrier coatings via interfacial 3D pattern10.1111/jace.20254 ↗
44. Laser-induced concave/convex micro-textures array for enhancing performance of surface coatings: bond coating in thermal barrier coating system10.1016/j.jmapro.2024.03.027 ↗
45. High temperature stability and sintering resistance of Gd2O3-Yb2O3-Y2O3-ZrO2 (GYYZO) coating10.1016/j.surfcoat.2023.129405 ↗
46. Investigation of isothermal oxidation behavior of thermal barrier coatings (TBCs) consisting of YSZ and multilayered YSZ/Gd2Zr2O7 ceramic layers10.1007/s11085-016-9690-4 ↗
47. TGO growth and kinetic study of single and double layered TBC systems10.1016/j.surfcoat.2021.127135 ↗
48. Structural characteristics, oxidation performance, and failure mechanism of thermal barrier coatings fabricated by atmospheric plasma spraying and detonation gun spraying10.1016/j.engfailanal.2023.107499 ↗
49. Recent developments in additive manufacturing
50. Comparison of calcium–magnesium-alumina-silicate (CMAS) resistance behavior of produced with electron beam physical vapor deposition (EB-PVD) method YSZ and Gd2Zr2O7/YSZ thermal barrier coatings systems10.1016/j.vacuum.2021.110576 ↗
51. Thermal property and failure behaviour of Pr-doped Gd2Zr2O7 thermal barrier coatings10.1016/j.corsci.2023.111641 ↗
52. Thermal property and failure mechanism of LaDyZrO thermal barrier coatings by electron beam physical vapor deposition10.1016/j.mtphys.2022.100696 ↗
53. Evolution of cold-expanded microstructure with aging temperature and its influence on fatigue performance of hole structure at elevated temperature10.1016/j.jallcom.2023.172562 ↗
54. Effects of A-site content on the phase structure and thermal property of (La1-xGdx)2Zr2O7 ceramics10.1016/j.ceramint.2024.12.165 ↗