journal article·2026-01Open access

Cryogenic rolling synergistically enhances mechanical properties and electrical conductivity of an Al-0.7Mg-0.4Si-0.1Fe alloy

Yan Wang, Xiaoli Cui, Wanli Jiao, Yang Fu, Hongwei Cui, Yongxiao Wang, Hui Li

Abstract

Balancing strength and electrical conductivity (EC) is key to broadening the applications of conductive aluminum alloys. This study systematically investigates how cold deformation regulates this balance in an Al-0.7Mg-0.4Si-0.1Fe alloy. Results show that with increasing deformation, the yield strength markedly improves from 43.5 MPa to 199.9 MPa, albeit with an expected decline in ductility. While the electrical conductivity is further increased to 57.9% IACS (from 55.2% IACS) by 70% deformation. So, a 70% deformation provides the optimal balance between EC and mechanical properties. Mechanism analysis indicates that dislocation strengthening induced by cold deformation is the dominant factor for the increase in YS. Collectively, these three mechanisms-dislocation strengthening, precipitation strengthening, texture strengthening from <1 0 1> and <1 1 1> oriented grains-contribute predominantly to the yield strength increment, accounting for 78.7% of the total increase. Meanwhile, The rolling process triggers Mg/Si precipitation and drives the development of elongated fibrous grain boundaries, while also inducing the preferential alignment of β-Al 5 FeSi and Mg 2 Si phases. These factors reduce the probability of electron scattering and improve EC. In summary, this study provides a process reference and theoretical basis for preparing medium-strength, high-conductivity Al-Mg-Si-Fe alloys.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (48)

Show source-provided references
1. Effect of cold drawing on the microstructure and property of precipitation strengthening u alloy prepared by continuous casting-extrusion10.1016/j.msea.2024.147669 ↗
2. Optimizing strength and electrical conductivity of 6201 aluminum alloy wire through rotary swaging and aging processes10.1016/j.jmatprotec.2024.118497 ↗
3. Development of ultra-high-strength Al-Mg-Si conductor alloys with copper addition via scalable thermomechanical processes10.1016/j.scriptamat.2024.116462 ↗
4. Breaking the strength-conductivity paradigm in hypoeutectic Al–Si alloy via annealing-induced Si nanoprecipitation10.1016/j.msea.2024.146924 ↗
5. Enhanced strength-conductivity trade-off in Al-Mg-Si alloys with optimized Mg/Si ratio10.1016/j.jallcom.2023.172682 ↗
6. Effects of natural aging and pre-aging on the strength and electrical conductivity in Al-Mg-Si AA6201 conductor alloys10.1016/j.msea.2021.141538 ↗
7. Effects of processing paths on the microstructure, mechanical properties and electrical conductivity of dilute Al-Zr-Sc alloy conductive wires10.1016/j.jmst.2023.11.060 ↗
8. Mechanical properties and interfacial characteristics of 6061 Al alloy plates fabricated by hot-roll bonding10.1007/s12613-023-2801-8 ↗
9. Microstructural heterogeneity and bonding strength of planar interface formed in additive manufacturing of Al−Mg−Si alloy based on friction and extrusion10.1007/s12613-022-2506-4 ↗
10. Preheating-assisted solid-state friction stir repair of Al-Mg-Si alloy plate at different rotational speeds10.1007/s12613-023-2772-9 ↗
11. Efficient production of kilometer-scale ultrafine aluminum wire with superior strength and electrical conductivity10.1016/j.msea.2024.146535 ↗
12. Microstructural change due to isochronal annealing in severely plastic-deformed commercial purity aluminium10.1080/14786435.2015.1021400 ↗
13. Pre-aging combined with multi-stage rolling processing: enhancing precipitate-dislocation interaction for strengthening of Cu-Cr-Zr-Ni-Si alloy10.1016/j.matdes.2025.114365 ↗
14. The microstructure evolution and strengthening mechanism of fine-grained Al–Mn alloy with nanoscale precipitates during cryorolling10.1016/j.msea.2024.146680 ↗
15. Achieving ultrahigh strength in binary Al-10Mg alloy through heavy cryogenic rolling10.1016/j.jallcom.2022.166931 ↗
16. Microstructure, texture and mechanical properties of FRAM-6061 aluminum alloy under rolling at different temperatures10.1016/j.msea.2025.148713 ↗
17. Quantitative model for grain boundary effects on strength-electrical conductivity relation10.1016/j.actamat.2024.120390 ↗
18. Grain design in ultra-fine Al wire with remarkable combination of strength and conductivity: ultra-fine-long grains with super strong ⟨111⟩ texture10.1016/j.scriptamat.2023.115746 ↗
19. Breaking the trade-off relation of strength and electrical conductivity in pure Al wire by controlling texture and grain boundary10.1016/j.jallcom.2018.07.358 ↗
20. Enhanced formability of Al–Mg–Si–Zn alloy sheet via dislocation structure and texture during cold rolling10.1016/j.jmrt.2023.12.246 ↗
21. Effects of processing paths on microstructure evolution and properties of high-strength and high-conductivity Al-Mg-Si alloys10.1016/j.msea.2025.148606 ↗
22. Influence of dislocation structures on precipitation phenomena in rolled Al–Mg–Si alloy10.1016/j.msea.2020.139903 ↗
23. Influence of precipitates on the grain refinement in CuFe2 alloy processed by rolling with cyclic movement of rolls10.1016/j.matdes.2016.07.138 ↗
24. Evolution of Fe–rich phases in Mg melt and a novel method for separating Al and Fe from Al–Si–Fe alloys10.1016/j.matdes.2017.08.029 ↗
25. Fe-bearing phase formation, microstructure evolution, and mechanical properties of Al-Mg-Si-Fe alloy fabricated by the twin-roll casting process10.1016/j.jallcom.2021.161202 ↗
26. Systematic study of growth behavior of β-Al9Fe2Si2 in Al alloys with high iron and silicon contents10.1016/j.jmrt.2023.07.212 ↗
27. Effect of total iron and silicon contents and homogenization on the microstructure and performance of 6201 Al–Mg–Si ingots10.1007/s43452-024-00974-x ↗
28. Influence of Mg and Si content and heat treatment on electrical conductivity and hardness of AA6101 Al alloy10.1007/s10853-023-08288-8 ↗
29. The improvement of electrical conductivity of hypoeutectic Al-Si alloys achieved by composite melt treatment10.1016/j.jallcom.2019.02.242 ↗
30. Improving the combination of electrical conductivity and tensile strength of Al 1070 by rotary swaging deformation10.1016/j.rinp.2019.102236 ↗
31. Design of non-heat-treatable Al-Fe-Ni alloys with high electrical conductivity and high strength via CALPHAD approach10.1016/j.jallcom.2024.176920 ↗
32. Mechanical and electrical properties of an ultrafine grained Al–8.5wt. % RE (RE=5.4wt.% Ce, 3.1wt.% La) alloy processed by severe plastic deformation10.1016/j.matdes.2015.10.163 ↗
33. Effect of La content on microstructure, tensile properties, and electrical conductivity of cast Al-Mg-Si-xLa alloys10.1007/s41230-025-4101-6 ↗
34. The improvement mechanism of good matching between electrical conductivity and mechanical properties for Al-4Si-0.8Mg-0.6Fe alloy10.1016/j.jallcom.2022.168275 ↗
35. Mechanical and physical properties of aluminum and its alloys for electrical conductors: a review
36. Influence of AlB2 compound on elimination of incoherent precipitation in artificial aging of wires drawn from redraw rod extruded from billets cast of alloy AA-6101 by vertical direct chill casting10.1016/j.matdes.2007.06.004 ↗
37. Modification of AA-6201 alloy for manufacturing of high conductivity and extra high conductivity wires with property of high tensile stress after artificial aging heat treatment for all-aluminium alloy conductors10.1016/j.matdes.2005.06.005 ↗
38. Heterostructured materials10.1016/j.pmatsci.2022.101019 ↗
39. Recent development of advanced precipitation-strengthened Cu alloys with high strength and conductivity: a review10.1016/j.pmatsci.2023.101141 ↗
40. Study on the microstructure evolution and strengthening mechanism of Cu-Ni-Si alloy after two-stage rolling and aging10.1016/j.matdes.2025.113935 ↗
41. Hall–petch relation and boundary strengthening10.1016/j.scriptamat.2004.06.002 ↗
42. Sc/Zr ratio-dependent mechanisms of strength evolution and microstructural thermal stability of multi-scale hetero-structured Al–Mg–Sc–Zr alloys10.1016/j.jmst.2022.09.009 ↗
43. Study about heat treatment on microstructure, electrical conductivity and mechanical properties of Al-1Si-0.6Mg-0.2Fe alloy10.1016/j.matchar.2024.113700 ↗
44. Strength-conductivity synergy in hypoeutectic Al-Si conductors via ultrafine-grained embedded Si nanoprecipitates10.1016/j.msea.2025.148124 ↗
45. Developing age-hardenable Al-Zr alloy by ultra-severe plastic deformation: significance of supersaturation, segregation and precipitation on hardening and electrical conductivity10.1016/j.actamat.2020.116503 ↗
46. Asymmetric cold rolling of AA7075 alloy: the evolution of microstructure, crystallographic texture, and mechanical properties10.1016/j.msea.2021.141801 ↗
47. Achieving excellent mechanical and electrical properties in Al-Si alloy via heterogeneous lamella structure with high-density nanoprecipitates10.1016/j.msea.2024.147778 ↗
48. Optimization of electrical conductivity and strength combination by structure design at the nanoscale in Al–Mg–Si alloys10.1016/j.actamat.2015.07.039 ↗