journal article·2025-05Open access

Mechanism study of brittle-to-ductile transition temperature in W-0.2 wt% Al2O3 alloy

Ziwen Zhao, Tielong Sun, Changji Wang, Hua Yu, Liya Cui, Caihong Dou, Yunchao Zhao, Cheng Zhang, Di Dong, Kunming Pan

Abstract

W-0.2 wt% Al 2 O 3 alloy plates were fabricated using composite powders prepared by the wet chemical method, followed by cold isostatic pressing, vacuum sintering, and hot-rolling. The addition of Al 2 O 3 particles significantly refines the grain of tungsten matrix compared to pure tungsten, reducing the average grain size from 1 μm to 0.73 μm. The bending strength of the W-0.2 wt% Al 2 O 3 alloy reaches 1379 MPa at room temperature, with a maximum bending strength of 5090 MPa at 300 °C, representing increases of 64 % and 45.8 % over pure tungsten, respectively. The mechanical properties of tungsten alloys were significantly enhanced by the introduction of Al 2 O 3 particles. The W-0.2 wt% Al 2 O 3 alloy exhibited a ductile at 200 °C, with its ductile-to-brittle transition temperature reduced by 100 °C compared to pure tungsten. The improvement in performance is attributed to the refinement of the grain of tungsten and the high proportion of low-angle grain boundaries improves the dislocation transfer path, thereby enhancing the toughness of the material. The synergistic effect of grain refinement and low-angle grain boundaries contributes to the increase in bending strength and the decrease in ductile-to-brittle transition temperature.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced materials and composites · Metallurgical Processes and Thermodynamics · Fusion materials and technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. An investigation of the microstructure and properties of rolled W-Al2O3 alloy10.1016/j.jallcom.2024.176223 ↗
2. Effect of Al2O3content and swaging on microstructure and mechanical properties of Al2O3/W alloys10.1016/j.ijrmhm.2019.105082 ↗
3. Effects of vanadium concentration on the densification, microstructures and mechanical properties of tungsten vanadium alloys10.1016/j.jnucmat.2014.04.019 ↗
4. The microstructure and radiation resistance of fine-grained W-0.3 wt% Y2O3 prepared by nano in-situ composite exposed to low-energy and high-flux helium plasma10.1016/j.jallcom.2022.163927 ↗
5. Effect of ZrO2content on microstructure and mechanical properties of W alloys fabricated by spark plasma sintering10.1016/j.ijrmhm.2018.11.006 ↗
6. Ductilisation of tungsten (W): on the shift of the brittle-to-ductile transition (BDT) to lower temperatures through cold rolling10.1016/j.ijrmhm.2015.09.001 ↗
7. Ductility enhancement of tungsten after plastic deformation10.1016/j.jallcom.2019.02.097 ↗
8. Characterization of ODS-tungsten microwave-sintered from sol-gel prepared nano-powders10.1016/j.jnucmat.2013.05.049 ↗
9. Sintering and characterization of W-Y and W-Y2O3 materials10.1016/j.fusengdes.2008.12.001 ↗
10. Fabrication of W-Y2O3 composites by ultrasonic spray pyrolysis and spark plasma sintering10.1016/j.ijrmhm.2021.105606 ↗
11. Fabrication and mechanical properties of tungsten alloys reinforced with c-ZrO2 particles10.1016/j.jallcom.2018.07.342 ↗
12. Preparation, microstructure, and constitutive equation of W-0.25 wt% Al2O3 alloy10.1016/j.msea.2018.12.001 ↗
13. Microstructure and preparation of an ultra-fine-grained W-Al2O3 composite via hydrothermal synthesis and spark plasma sintering10.1016/j.ijrmhm.2017.12.022 ↗
14. Effect of hot rolling on the microstructure and fracture behavior of a bulk fine-grained W-Y2O3 alloy10.1016/j.msea.2015.08.045 ↗
15. Application of powder metallurgy and hot rolling processes for manufacturing aluminum/alumina composite strips10.1016/j.msea.2012.09.103 ↗
16. Preparation and characterization of Mo/Al2O3 composites10.1016/j.ijrmhm.2015.07.033 ↗
17. Microstructure and mechanical properties of W-Al2O3 alloy plates prepared by a wet chemical method and rolling process10.3390/ma15227910 ↗
18. Deformation-induced ω phase transition in polycrystalline tungsten under extreme shock loading10.1016/j.scriptamat.2024.116432 ↗
19. Influence of crystallographic orientations and nanovoid on the plastic mechanism and damage behavior of single-crystal tungsten under shock10.1016/j.jmrt.2025.01.040 ↗
20. Evaluation of phase relationship in W-Fe-C ternary system through symmetry principles and first-principles calculation10.1016/j.matdes.2022.111376 ↗
21. Recent progress in R&D on tungsten alloys for divertor structural and plasma facing materials10.1016/j.jnucmat.2013.02.074 ↗
22. The nature behind the preferentially embrittling effect of impurities on the ductility of tungsten10.1016/j.commatsci.2014.06.036 ↗
23. Effect of initial grain size on microstructure, texture and magnetic properties of non-oriented electrical steel10.1016/j.jmrt.2024.06.193 ↗
24. Effect of grain size on the shear banding behavior of Ti-6Al-4V alloy under quasi-static compression10.1007/s11661-020-05695-3 ↗
25. Dislocations with edge components in nanocrystalline bcc Mo10.1557/jmr.2012.403 ↗
26. Competing processes in reactions between an edge dislocation and dislocation loops in a body-centred cubic metal10.1016/j.scriptamat.2010.01.034 ↗
27. Effects of temperature on structure and mobility of the ⟨1 0 0⟩ edge dislocation in body-centred cubic iron10.1016/j.actamat.2009.12.033 ↗
28. The effect of tungsten content on the rolling texture and microstructure of Ta-W alloys10.1016/j.matchar.2019.110067 ↗
29. Fracture toughness and microstructural characterization of polycrystalline rolled tungsten10.1016/j.ijrmhm.2010.05.006 ↗
30. Microstructure study of hot rolling nanosized in-situ Al2O3 particle reinforced A356 matrix composites10.1016/j.jallcom.2020.157107 ↗
31. Effect of hot-working process on interface structure and ductile-to-brittle transition temperature of tungsten alloy reinforced by Al2O3 particles10.1016/j.ijrmhm.2022.105945 ↗
32. Processing of fine-grained W materials without detrimental phases and their mechanical properties at 200–432K10.1016/j.msea.2007.03.079 ↗
33. An investigation of the microstructure and ductility of annealed cold-rolled tungsten10.1016/j.actamat.2018.10.002 ↗
34. Nanostructured high-strength molybdenum alloys with unprecedented tensile ductility10.1038/nmat3544 ↗
35. Strengthening mechanism and effect of Al2O3 particle on high-temperature tensile properties and microstructure evolution of W-Al2O3alloys10.1016/j.msea.2022.142678 ↗
36. Small-scale analysis of brittle-to-ductile transition behavior in pure tungsten10.1016/j.jmst.2021.07.024 ↗
37. Ductilisation of tungsten (W) through cold-rolling: R-curve behaviour10.1016/j.ijrmhm.2016.03.006 ↗
38. Dislocation-mediated strain hardening in tungsten: thermo-mechanical plasticity theory and experimental validation10.1016/j.jmps.2015.08.015 ↗
39. Hierarchical microstructures enabled excellent low-temperature strength-ductility synergy in bulk pure tungsten10.1016/j.actamat.2022.117765 ↗
40. Grain refinement in titanium prevents low temperature oxygen embrittlement10.1038/s41467-023-36030-0 ↗
41. The mechanism of plastic deformation of crystals, Part I